Abstract
High-temperature two-step chemical vapor deposition (CVD) is a promising method of preparing large-scale silica glass, in which thermal stress is generated due to uneven temperature distribution when cooling naturally to room temperature. In this paper, a numerical model of the annealing and cooling processes has been established to study the generation and evolution of thermal stress. Furthermore, the annealing parameters, including annealing temperature and annealing time, are investigated to control thermal stress. The simulation results proved that variations in annealing temperature and annealing time can significantly affect the thermal stress generated during the annealing and cooling process. The residual stress decreases with increasing annealing temperature and annealing time. To optimize the annealing process, two-step annealing, including higher and lower temperature stages, has been studied. It is found that stepwise annealing can reduce the residual stress and the stress peaks with a shorter annealing time in the high-temperature stage.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · High-Temperature Coating Behaviors · Adhesion, Friction, and Surface Interactions
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. High-throughput thermal replication of transparent fused silica glass
2. Two-photon polymerization of nanocomposites for the fabrication of transparent fused silica glass microstructures
3. Fabrication of a high-quality axicon by femtosecond laser ablation and CO(2) laser polishing for Quasi-Bessel beam generation10.1364/OE.26.023287 ↗
4. NIF Optical materials and fabrication technologies: an overview
5. Effects of injection conditions on temperature and component distributions in a CVD furnace for large-size silica glass10.1111/jace.18964 ↗
6. Chemical vapour deposition of coatings10.1016/S0079-6425(01)00009-3 ↗
7. High-performance materials for 3D printing in chemical synthesis applications10.1002/adma.201805982 ↗
8. Effects of thermal environment on dehydroxylation of porous silica preform in two-step CVD synthesis10.1111/jace.17700 ↗
9. SiO2 soot preform sintering process for the synthesis of large-size and high-purity silica glass10.1016/j.ceramint.2023.10.171 ↗
10. Investigation of stress induced by CO2 laser processing of fused silica optics for laser damage growth mitigation10.1364/OE.17.023488 ↗
11. Note: mounting ultra-high vacuum windows with low stress-induced birefringence10.1063/1.3606437 ↗
12. Residual stresses in glass after molding and its influence on optical properties10.1016/j.proeng.2011.11.132 ↗
13. A new instrument for measuring both the magnitude and angle of low level linear birefringence10.1063/1.1150000 ↗
14. Research on Precision Annealing of High Performance Silica Glass
15. Process design based on temperature field control for reducing the thermal residual stress in glass/glass laser bonding10.1016/j.optlastec.2016.12.016 ↗
16. Temperature and thermal stress simulation of window glass exposed to fire10.1016/j.proeng.2011.04.682 ↗
17. Thermal shock effect on the glass thermal stress response and crack propagation10.1016/j.proeng.2013.08.118 ↗
18. Effect of glass temperature before cooling and cooling rate on residual stresses in tempering10.1007/s40940-017-0053-6 ↗
19. Stress analysis of LCD glass substrate based on ANSYS
20. Reduction in internal friction in silica glass with high OH content10.1111/jace.16187 ↗
21. The dependence of N2 carrier gas flow rate on deposition rate and density changes of porous silica preform synthesized by eco-friendly octamethylcyclotetrasiloxane
22. Experimental study of SiO2 soot deposition using the outside vapor deposition method10.1080/02786821003671315 ↗
23. Uniaxial compression of SiO2 glass cylinders: analysis using stress-independent material coefficients10.1002/mawe.201100672 ↗
24. Uniaxial compression of SiO2 glass cylinders: analysis using stress-dependent material coefficients10.1002/mawe.201200874 ↗
25. Finite element simulation of the slumping process of a glass plate using 3D generalized viscoelastic Maxwell model10.1016/j.jnoncrysol.2014.08.018 ↗
26. Glass sagging simulation with improved calculation of radiative heat transfer by the optimized reciprocity Monte Carlo method10.1016/j.ijheatmasstransfer.2013.10.068 ↗
27. Numerical investigation of residual stresses in thin-walled additively manufactured structures from selective laser melting10.1016/j.heliyon.2023.e19385 ↗
28. Thermal expansion measurements of quartz glass by laser interferometry
29. Vlack · 1964
30. Radiation energy transfer and thermal conductivity of ceramic oxides10.1111/j.1151-2916.1960.tb13623.x ↗
31. Low temperature-elastic moduli, debye temperature and internal dilational and shear frictions of fused quartz10.1023/A:1018583918380 ↗
32. Thermal stress limitations to laser fire polishing of glasses10.1364/AO.22.002933 ↗
33. Thermal tempering simulation of glass plates: inner and edge residual stresses10.1080/01495739808956168 ↗
34. New testing and calculation method for determination viscoelasticity of optical glass10.1364/OE.28.000626 ↗
35. Investigation on the viscoelasticity of optical glass in ultraprecision lens molding process10.1016/j.jmatprotec.2008.10.030 ↗
36. Low frequency storage and loss moduli of soda-silica glasses in the transformation range10.1016/0022-3093(74)90034-9 ↗
37. Effect of glass thickness on temperature gradient and stress distribution during glass tempering10.1016/j.jnoncrysol.2016.01.008 ↗
38. Online and real-time accurate prediction of tempered glass surface stress during quenching process10.1080/01495739.2019.1590169 ↗
39. Relaxation of thermal residual stress in laser irradiated fused silica by annealing process10.4028/www.scientific.net/MSF.874.345 ↗