Sub-nano to nanometer wear and tribocorrosion of titanium oxide-metal surfaces by in situ atomic force microscopy
Source abstract
Abstract
Wear and tribocorrosion of passive oxide film covered metals have been studied at the micro and macroscopic scales. Recent advances in nanotechnology have contributed to breakthroughs in understanding of fundamental friction and wear mechanisms of atomically thin 2D materials at the nanoscale. However, for metals and materials without ultra-flat surfaces, a gap in knowledge exists at or below a few nanometers, which is too small for continuum mechanics theories and experiments including conventional atomic force microscopy (AFM) methods, due to resolution limits arising from surface roughness. Here, we report the near-atomic-scale wear of titanium in air and physiological solution from a single atomic layer to beyond the full oxide thickness using an AFM-based tribology method. Sub-nano to nanometer wear of titanium was revealed with different stages of contact pressure dependent wear regions identified as wear depth increased, featured by a transition from atomic wear (below 2.4 GPa) to elasto-plastic driven wear (above 3.6 GPa) at its oxide thickness (3.8 nm) in air. Higher stress was required to generate a similar wear penetration process in PBS compared to air. Tribocorrosion at this scale was grain orientation and voltage-dependent. Our study opens up a new method to achieve reliable angstrom-level resolution wear quantification to advance the understanding of wear and tribocorrosion of metals at the nanoscale. STATEMENT OF SIGNIFICANCE: Experimental tests of wear for metallic biomaterials at the nanoscale are difficult because engineered metal surfacesare never perfectly atomically flat, limiting the resolution of precise wear measurements to a few nanometers scale or more. To systematically address this problem, we have introduced the AFM 'image-wear-image' tribology method and obtained quantitative stress dependent measurement of the near-atomic-scale wear of titanium surfaces in air and tribocorrosion in physiological solution from a single atomic layer to beyond the full oxide film thickness. This allowedto measure sub-nano scale wear by partial removal of oxide. Nanoscale wear has been found to be grain orientation-dependent above the 'atomic scale' wear region. The nano-tribocorrosion of CP-Ti across scales and voltage effects on oxides in physiological solution was studied. Our study opens up a new method for future studies to advance the understanding of sub-nanoscale and nanoscale wear and tribocorrosion phenomenon as well as oxide growth mechanism of metallic biomaterials.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Force Microscopy Techniques and Applications · Metal and Thin Film Mechanics · Lubricants and Their Additives
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Mate · 2019
2. Contact and rubbing of flat surfaces10.1063/1.1721448 ↗
3. Rabinowicz · 1995 · 125
4. Triboelectrochemical techniques and interpretation methods in tribocorrosion: a comparative evaluation10.1016/j.triboint.2007.11.003 ↗
5. Nanotribology: friction, wear and lubrication at the atomic scale10.1038/374607a0 ↗
6. Frictional wear in metallic contacts without current
7. The breakdown of continuum models for mechanical contacts10.1038/nature03700 ↗
8. Friction laws at the nanoscale10.1038/nature07748 ↗
9. Critical length scale controls adhesive wear mechanisms10.1038/ncomms11816 ↗
10. Modeling and simulation in tribology across scales: an overview10.1016/j.triboint.2018.02.005 ↗
11. Abrasive wear on the atomic scale10.1103/PhysRevLett.88.215501 ↗
12. Atomistic wear in a single asperity sliding contact10.1103/PhysRevLett.101.125501 ↗
13. Nanoscale wear as a stress-assisted chemical reaction10.1038/nnano.2012.255 ↗
14. Ultralow nanoscale wear through atom-by-atom attrition in silicon-containing diamond-like carbon10.1038/nnano.2010.3 ↗
15. Insights into tribology from in situ nanoscale experiments10.1557/mrs.2019.122 ↗
16. In situ single asperity wear at the nanometre scale10.1080/09506608.2016.1213942 ↗
17. Mechanisms of antiwear tribofilm growth revealed in situ by single-asperity sliding contacts10.1126/science.1258788 ↗
18. Chemical and physical origins of friction on surfaces with atomic steps10.1126/sciadv.aaw0513 ↗
19. Direct observation of corrosive wear by in situ scanning probe microscopy10.1021/acsami.0c02256 ↗
20. Enhanced bond strength and bioactivity of interconnected 3D TiO2 nanoporous layer on titanium implants10.1016/j.surfcoat.2016.05.038 ↗
21. Titanium in biomedical applications—properties and fabrication: a review10.1166/jbt.2015.1361 ↗
22. Passive film on orthopaedic TiAlV alloy formed in physiological solution investigated by X-ray photoelectron spectroscopy10.1016/S0142-9612(00)00145-9 ↗
23. Corrosion at the head-neck taper as a cause for adverse local tissue reactions after total hip arthroplasty10.2106/JBJS.K.01352 ↗
24. Friction and wear of titanium alloys sliding against metal, polymer, and ceramic counterfaces10.1016/j.wear.2004.09.062 ↗
25. Wear characterization of Ti-6Al-4V under fretting-reciprocating sliding conditions10.1016/j.wear.2007.08.004 ↗
26. Area-dependent impedance-based voltage shifts during tribocorrosion of Ti-6Al-4V biomaterials: theory and experiment
27. Tribocorrosion response of the Ti6Al4V alloys commonly used in femoral stems10.1016/j.triboint.2013.09.022 ↗
28. Nano-scale wear of hard materials: an overview10.1016/j.cocis.2020.01.001 ↗
29. An AFM study of single-contact abrasive wear: the Rabinowicz wear equation revisited10.1016/j.wear.2008.12.024 ↗
30. Nanoabrasive wear induced by an AFM diamond tip on stainless steel10.1016/j.wear.2006.10.020 ↗
31. Nano-scale wear characterization of CoCrMo biomedical alloys10.1016/j.triboint.2015.03.037 ↗
32. Calibration of rectangular atomic force microscope cantilevers10.1063/1.1150021 ↗
33. Surface characterization of implant materials c.p. Ti, Ti-6Al-7Nb and Ti-6Al-4V with different pretreatments10.1023/A:1008840026907 ↗
34. Basic assumptions and recent developments in quantitative XPS10.1002/sia.740040402 ↗
35. Indentation size effect in polycrystalline FCC metals10.1016/S1359-6454(02)00175-1 ↗
36. Quantification of fretting damage10.1016/S0043-1648(96)07306-1 ↗
37. Is the wear coefficient dependent upon slip amplitude in fretting? Vingsbo and Söderberg revisited10.1016/j.wear.2014.11.005 ↗
38. Fretting corrosion of CoCrMo and Ti6Al4V interfaces10.1016/j.biomaterials.2012.04.015 ↗
39. Graphitic tribological layers in metal-on-metal hip replacements10.1126/science.1213902 ↗
40. A new asperity-scale mechanistic model of tribocorrosive wear: synergistic effects of mechanical wear and corrosion10.1115/1.4041246 ↗
41. The effect of crystallographic grain orientation of polycrystalline Ti on ploughing under scratch testing10.1016/j.wear.2018.05.013 ↗
42. Numerical study of atomic scale deformation mechanisms of Ti grains with different crystallographic orientation subjected to scratch testing10.1016/j.apsusc.2018.12.021 ↗
43. How grain size controls friction and wear in nanocrystalline metals