Silk-based multilayer coatings for anticoagulation and durability improvement in ECMO hollow fiber membranes
Source abstract
Abstract
In clinical extracorporeal membrane oxygenation (ECMO), prolonged blood residence time in oxygenators can lead to thrombus formation and complications. Heparin-based bioactive coatings are commonly used for anticoagulation, but prolonged shear stress during blood flow can cause heparin desorption, degradation, and inactivation, reducing durability and antithrombotic efficacy. In this study, we developed a silk fibroin (SF)-based multilayer coating to enhance both mechanical stability and anticoagulant performance. A SF foundation layer was first fabricated on hollow-fiber membranes using layer-by-layer (LbL) self-assembly. Then SF acted as a bridge to assemble heparin and albumin through electrostatic interactions, followed by crosslinking to stabilize the structure, resulting in a uniform SF-heparin-albumin composite coating with controllable thickness. 10-day shear oscillation and nanoscratch tests showed that the SF bridging layer significantly improved mechanical robustness and interfacial adhesion. In vitro and in vivo blood circulation assays demonstrated hemocompatibility, with reduced platelet adhesion, prolonged coagulation time, and enhanced antithrombotic performance. Blood-gas exchange tests using a miniaturized oxygenator confirmed that the coating did not impair gas transfer efficiency. In summary, the SF bridging layer effectively links the substrate to bioactive components, improving long-term mechanical integrity and anticoagulant properties without compromising oxygenator function. STATEMENT OF SIGNIFICANCE: During clinical ECMO use, shear stress often compromises the integrity of anticoagulant coatings, leading to detachment and reduced functionality. Here, we present a silk fibroin (SF)-based multilayer coating engineered to enhance the long-term stability and anticoagulant performance of ECMO hollow-fiber membranes. Utilizing a layer-by-layer self-assembly strategy, heparin and albumin were stably incorporated into the SF matrix, resulting in a coating with improved shear resistance and preserved gas exchange. As the first silk-based coating specifically designed for ECMO applications, this work bridges biomolecular design with device-level functionality. Moreover, it demonstrates biocompatibility with no detectable cytotoxicity, offering a promising approach for safe and durable blood-contacting applications.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Silk-based biomaterials and applications · Electrospun Nanofibers in Biomedical Applications · Surface Modification and Superhydrophobicity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Clinical features of patients infected with 2019 novel coronavirus in wuhan, China10.1016/S0140-6736(20)30183-5 ↗
2. Extracorporeal membrane oxygenation (ECMO): does it have a role in the treatment of severe COVID-19?10.1016/j.ijid.2020.03.058 ↗
3. Extracorporeal membrane oxygenation support in COVID-19: an international cohort study of the extracorporeal life support organization registry10.1016/S0140-6736(20)32008-0 ↗
4. Longitudinal trends in bleeding complications on extracorporeal life support over the past two decades—extracorporeal Life Support Organization registry analysis10.1097/CCM.0000000000005466 ↗
5. Hemocompatibility challenge of membrane oxygenator for artificial lung technology10.1016/j.actbio.2022.09.003 ↗
6. Oxygenation and membrane oxygenators: emergence evolution and progress in material development and process enhancement for biomedical applications
7. Anti-thrombogenic surface coatings for extracorporeal membrane oxygenation: a narrative review10.1021/acsbiomaterials.1c00758 ↗
8. Unravelling surface modification strategies for preventing medical device-induced thrombosis10.1002/adhm.202301039 ↗
9. Coatings for biomaterials to improve hemocompatibility10.1016/B978-0-08-100497-5.00007-0 ↗
10. The blood compatibility challenge. Part 1: blood-contacting medical devices: the scope of the problem10.1016/j.actbio.2019.06.021 ↗
11. Antifouling zwitterionic polymer coatings for blood-bearing medical devices10.1021/acs.langmuir.4c04532 ↗
12. Aggregation-disruption-induced multi-scale mediating strategy for anticoagulation in blood-contacting devices10.1002/adma.202412701 ↗
13. Bioinspired zwitterionic block polymer-armored nitric oxide-generating coating combats thrombosis and biofouling10.34133/research.0423 ↗
14. Nitric oxide-delivering surface modification for tailoring cell-material interactions on medical device surface: from surface-functionalized design to therapeutic applications10.1016/j.cej.2025.162378 ↗
15. Engineered endothelium-mimicking antithrombotic surfaces via combination of nitric oxide-generation with fibrinolysis strategies
16. Endogenous nitric oxide-releasing microgel coating prevents clot formation on oxygenator fibers exposed to In vitro blood flow10.3390/membranes12010073 ↗
17. Steps toward recapitulating endothelium: a perspective on the next generation of hemocompatible coatings10.1002/mabi.202400152 ↗
18. Antithrombotic coating with sheltered positive charges prevents contact activation by controlling factor XII–biointerface binding
19. Why we need safer anticoagulant strategies for patients on short-term percutaneous mechanical circulatory support10.1007/s00134-019-05897-3 ↗
20. Biomedical applications of engineered heparin-based materials
21. Mechanism of action and pharmacology of unfractionated heparin10.1161/hq0701.093686 ↗
22. Medtronic. Cortiva bioactive surface for cpb circuit devices. https://global.medtronic.com/xg-en/healthcareprofessionals/products/cardiovascular/cardiopulmonary/cortiva-bioactive-surface.html.
23. Reduced complement activation with heparin-coated oxygenator and tubings in coronary bypass operations10.1016/S0022-5223(19)34966-9 ↗
24. Synthetic protein treated versus heparin coated cardiopulmonary bypass surfaces: similar clinical results and minor biochemical differencesq
25. Medos, Hilite Product Family, Xenios, Heilbronn, Germany, (n.d.). https://www.xenios-ag.com/wp-content/uploads/2019/04/Medos-hilite-Product-Family-Brochure_EN_001_2018_10.pdf.
26. A prospective, double-blind study on the efficacy of the bioline surface-heparinized extracorporeal perfusion circuit10.1016/S0003-4975(03)00338-2 ↗
27. Heparin coatings for improving blood compatibility of medical devices10.1016/j.addr.2016.12.002 ↗
28. Modification strategies to improve the membrane hemocompatibility in extracorporeal membrane oxygenator (ECMO)10.1007/s42114-021-00244-x ↗
29. Heparin surfaces: impact of immobilization chemistry on hemocompatibility and protein adsorption10.1002/jbm.b.33154 ↗
30. Surface monofunctionalized polymethyl pentene hollow fiber membranes by plasma treatment and hemocompatibility modification for membrane oxygenators10.1016/j.apsusc.2015.11.236 ↗
31. Plasma surface modification of biomaterials for biomedical applications10.1007/978-981-10-3328-5_3 ↗
32. Development of zwitterionic sulfobetaine block copolymer conjugation strategies for reduced platelet deposition in respiratory assist devices10.1002/jbm.b.34085 ↗
33. The biomedical use of silk: past, present, future10.1002/adhm.201800465 ↗
34. Silk fibroin-based biomaterials for biomedical applications: a review10.3390/polym11121933 ↗
35. Layer-by-Layer deposition of regenerated silk fibroin-an approach to the surface coating of biomedical implant materials10.1021/acsbiomaterials.3c00852 ↗
36. Coating topologically complex electrospun fibers with nanothin silk fibroin enhances neurite outgrowth in vitro10.1021/acsbiomaterials.9b01487 ↗
37. Silk fibroin as a green material10.1021/acsbiomaterials.1c00493 ↗
38. Electrospun silk fibroin/fibrin vascular scaffold with superior mechanical properties and biocompatibility for applications in tissue engineering10.1038/s41598-024-54638-0 ↗
39. Structures, mechanical properties and applications of silk fibroin materials10.1016/j.progpolymsci.2015.02.001 ↗
40. Silk fibroin layer-by-layer microcapsules for localized gene delivery10.1016/j.biomaterials.2014.05.062 ↗
41. The effects of silk layer-by-layer surface modification on the mechanical and structural retention of extracellular matrix scaffolds10.1039/D0BM00448K ↗
42. Cell membrane-biomimetic coating via click-mediated liposome fusion for mitigating the foreign-body reaction10.1016/j.biomaterials.2021.120768 ↗
43. Janus decellularized membrane with anisotropic cell guidance and anti-adhesion silk-based coatings for spinal dural repair10.1038/s41467-025-56872-0 ↗
44. Hybrid cell membrane coating orchestrates foreign-body reactions, anti-adhesion, and pro-regeneration in abdominal wall reconstruction10.1016/j.biomaterials.2025.123289 ↗
45. Characterization of membrane blood oxygenation devices using computational fluid dynamics10.1016/j.memsci.2006.11.041 ↗
46. Water-insoluble silk films with silk I structure10.1016/j.actbio.2009.10.041 ↗
47. Stem cell-based tissue engineering with silk biomaterials10.1016/j.biomaterials.2006.07.008 ↗
48. Silk fibroin as sustainable advanced material: material properties and characteristics, processing, and applications10.1002/adfm.202210764 ↗
49. Controlling silk fibroin particle features for drug delivery10.1016/j.biomaterials.2010.02.024 ↗
50. Interactions of proteins with heparan sulfate10.1042/EBC20230093 ↗
51. Heparin coating on 3D printed poly (l-lactic acid) biodegradable cardiovascular stent via mild surface modification approach for coronary artery implantation10.1016/j.cej.2019.122116 ↗
52. Collagen and heparin co-modification of NK110 microspheres for enhanced bilirubin adsorption and improved blood compatibility in hemoperfusion10.1016/j.seppur.2025.133541 ↗
53. Kinetic analysis reveals the role of secondary nucleation in regenerated silk fibroin self-assembly10.1021/acs.biomac.2c01479 ↗
54. Materials fabrication from bombyx mori silk fibroin10.1038/nprot.2011.379 ↗
55. Hydrodynamic simulation of an orbital shaking test for the degradation assessment of blood-contact biomedical coatings10.3390/mi8040132 ↗
56. R.H.J. Hendrix, The membrane oxygenator: from a black to a white box, maastricht university, 2024. https://doi.org/10.26481/dis.20240312rh.10.26481/dis.20240312rh ↗
57. Nanoscratch test — a tool for evaluation of cohesive and adhesive properties of thin films and coatings10.1051/epjconf/20134800027 ↗
58. Mechanism of adhesion of natural polymer coatings to chemically modified siloxane polymer10.1021/acs.langmuir.1c00047 ↗
59. ELSO guidelines for adult and pediatric extracorporeal membrane oxygenation circuits10.1097/MAT.0000000000001630 ↗
60. A comprehensive study of oxygenator gas transfer efficiency and thrombosis risk
61. S. Saha, C. Sarkar, eds., Biodegradable Polymers and Their Emerging Applications, Springer Nature Singapore, Singapore, 2023. https://doi.org/10.1007/978-981-99-3307-5.10.1007/978-981-99-3307-5 ↗
62. Chemical surface modification of polymeric biomaterials for biomedical applications10.1002/marc.201900430 ↗
63. Improved computational fluid dynamic simulations of blood flow in membrane oxygenators from X-ray imaging10.1007/s10439-013-0824-4 ↗
64. Comparative aspects of blood coagulation10.1016/j.tvjl.2003.09.013 ↗
65. Comparison of animal and human blood for in vitro dynamic thrombogenicity testing of biomaterials10.1111/aor.14366 ↗
66. Blood flow and oxygen transfer rate of an outside blood flow membrane oxygenator10.1016/S0376-7388(00)00331-8 ↗
67. Collagen/heparin coating on titanium surface improves the biocompatibility of titanium applied as a blood-contacting biomaterial10.1002/jbm.a.32847 ↗
68. Zwitterionic poly-carboxybetaine coating reduces artificial lung thrombosis in sheep and rabbits10.1016/j.actbio.2019.05.019 ↗
69. Extracorporeal circulation models in small animals: beyond the limits of preclinical research10.4266/acc.2023.00381 ↗
70. Combination of polycarboxybetaine coating and factor XII inhibitor reduces clot formation while preserving normal tissue coagulation during extracorporeal life support10.1016/j.biomaterials.2021.120778 ↗