Co-Cr-Mo atomized powders containing 0.05 wt.% C were sintered at temperatures above 900 degrees C for 1h and then rapidly cooled to room temperature. As a result, various amounts of athermal epsilon-martensite were produced which increased with increasing sintering temperatures (from 30 vol.% at 950 degrees C to 70 vol.% at 1250 degrees C). Apparently, the development of epsilon-embryos was strongly promoted by increasing sintering temperatures due to the development of a high density of epsilon-nucleation site defects. In addition, athermal martensite readily formed in these powders, suggesting that its development was strongly favored by a significant reduction in the carbon supersaturation levels from 0.25 wt.% for most commercial alloys to 0.05 wt.% C. The amounts of epsilon-martensite were 3-4-fold those found in conventional alloys, suggesting that the powder structure provides increasing nucleation sites for athermal epsilon-martensite. Apparently free surfaces and grain development at powder contact surfaces combined with recrystallization and grain growth within powder particles lead to favorable dislocation configuration arrays for the development of epsilon-embryos.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Entropy Alloys Studies · Advanced materials and composites · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (19)
Show source-provided references
1. 1996 · 116
2. Powder metallurgical processing improves high-carbon Co–Cr–Mo alloy for orthopaedic implants
3. Kinetics of the martensitic fcc→hcp transformation in Co–Cr–Mo alloy powders10.1016/0001-6160(84)90077-4 ↗
4. Room temperature strengthening mechanisms in a Co–Cr–Mo alloy10.1007/BF00540374 ↗
5. A transmission electron microscopy study of the mechanisms of strengthening in heat-treated Co–Cr–Mo–C alloys10.1007/BF02642835 ↗
6. Effect of temperature on the lattice constants and crystalline structure of a Co–27Cr–5Mo low carbon alloy10.1007/s11661-006-0232-6 ↗
7. Effects of grain size on the development of athermal and strain induced ε-martensite in a Co–Cr–Mo implant alloy10.1179/026708399101505699 ↗
8. Microstructural effects on the wear resistance of wrought and As-cast Co–Cr-Mo–C implant alloys10.1002/jbm.a.30392 ↗
9. Tribological behavior of cast and wrought Co–Cr–Mo implant alloys10.1179/026708399101505284 ↗
10. Methode d’analyse quantitative des varites allotropiques du cobalt par les rayons X10.1051/metal/195047020139 ↗
11. Slow growth of isothermal lath martensite in an Fe–21Ni–4Mn alloy10.1016/0001-6160(84)90032-4 ↗
12. Effect of solution treatments on the fcc/hcp isothermal martensitic transformation in Co–27Cr–5Mo–0.05C aged at 800°C10.1016/S1359-6462(98)00489-8 ↗
13. Phase transformations in a wrought Co–Cr–Mo–C alloy10.1007/BF02645497 ↗
14. A general mechanism of martensitic nucleation. Part III: Kinetics of martensitic nucleation10.1007/BF02659824 ↗
15. Thermodynamics of stacking faults10.1007/BF03038365 ↗
16. Hirth · 1983
17. Direct evidence for Suzuki segregation and Cottrell Pinning in MP 159 superalloy obtained by FEG(S) TEM/EDX10.1016/S1359-6454(02)00359-2 ↗
18. The temperature and concentration dependence of the stacking fault energy in the Co–Ni system10.1016/0001-6160(66)90006-X ↗
19. The C–Co (carbon–cobalt) system10.1007/BF02645959 ↗