Abstract

Abstract We report on the low energy helium ion irradiation induced surface morphology changes on tungsten (W) surfaces under extreme conditions. Surface morphology changes on W surfaces were monitored as a function of helium ion energy (140–300 eV), fluence (2.3 × 10 24 –1.6 × 10 25 ions m −2 ), and flux (2.0 × 10 20 –5.5 × 10 20 ion m −2 s −1 ). All the experiments were performed at 900° C. Our study shows significant effect of all the three ion irradiation parameters (ion flux, fluence, and energy) on the surface morphology. However, the effect of ion flux is more pronounced. Variation of helium ion fluence allows to capture the very early stages of fuzz growth. The observed fuzz growth and morphology changes were understood in the realm of various possible phenomena. The study has relevance and important impact in the current and future nuclear fusion applications.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Ion-surface interactions and analysis · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Investigation of tungsten alloys as plasma facing materials for the ITER divertor10.1016/S0920-3796(02)00113-8 ↗
2. Formation process of tungsten nanostructure by the exposure to helium plasma under fusion relevant plasma conditions10.1088/0029-5515/49/9/095005 ↗
3. Fukai · 2005
4. A review of recent experiments on W and high Z materials as plasma-facing components in magnetic fusion devices10.1016/S0022-3115(97)80042-6 ↗
5. Helium induced nanoscopic morphology on tungsten under fusion relevant plasma conditions10.1088/0029-5515/48/3/035001 ↗
6. Formation of helium induced nanostructure ‘fuzz’ on various tungsten grades10.1016/j.jnucmat.2010.06.034 ↗
7. Observations of suppressed retention and blistering for tungsten exposed to deuterium–helium mixture plasmas10.1088/0029-5515/49/6/065035 ↗
8. Comparison of tungsten nano-tendrils grown in Alcator C-Mod and linear plasma devices10.1016/j.jnucmat.2013.01.013 ↗
9. Formation of nanostructured tungsten with arborescent shape due to helium plasma irradiation10.1585/pfr.1.051 ↗
10. Formation mechanism of bubbles and holes on tungsten surface with low-energy and high-flux helium plasma irradiation in NAGDIS-II10.1016/j.jnucmat.2004.04.129 ↗
11. Microstructure evolution in tungsten during low-energy helium ion irradiation10.1016/S0022-3115(00)00289-0 ↗
12. Key ITER plasma edge and plasma–material interaction issues10.1016/S0022-3115(02)01327-2 ↗
13. Tungsten nano-tendril growth in the Alcator C-Mod divertor10.1088/0029-5515/52/4/042003 ↗
14. Exposure of tungsten nano-structure to TEXTOR edge plasma10.1016/j.jnucmat.2010.08.019 ↗
15. Plasma–surface interaction issues of an all-metal ITER10.1088/0029-5515/49/3/035007 ↗
16. Dolan · 1982
17. Exfoliation of the tungsten fibreform nanostructure by unipolar arcing in the LHD divertor plasma10.1088/0029-5515/51/10/102001 ↗
18. Experimental investigation on the effect of surface electric field in the growth of tungsten nano-tendril morphology due to low energy helium irradiation10.1016/j.jnucmat.2016.09.018 ↗
19. Nanostructure formation on tungsten exposed to low-pressure rf helium plasmas: a study of ion energy threshold and early stage growth10.1016/j.jnucmat.2010.10.050 ↗
20. Nanostructuring of molybdenum and tungsten surfaces by low-energy helium ions10.1116/1.4731196 ↗
21. Tungsten nano-tendril growth in the Alcator C-Mod divertor10.1088/0029-5515/52/4/042003 ↗
22. Some problems arising due to plasma–surface interaction for operation of the in-vessel mirrors in a fusion reactor10.1016/S0022-3115(00)00634-6 ↗
23. First mirror tests for ITER: influence of material choice on the erosion/deposition mechanisms affecting optical reflectivity10.1016/j.jnucmat.2007.01.024 ↗
24. Diagnostic mirrors for ITER: a material choice and the impact of erosion and deposition on their performance10.1016/j.jnucmat.2007.01.281 ↗
25. Degradation of optical properties in Mo mirrors under irradiation with low energy helium and deuterium ions10.1016/j.jnucmat.2010.12.143 ↗
26. Irradiation effects of low energy helium ions on optical reflectivity of metallic mirror10.1016/j.jnucmat.2007.01.153 ↗
27. On the choice of materials for the first mirrors of plasma diagnostics in a fusion reactor10.1016/S0022-3115(98)00129-9 ↗
28. An equilibrium model for tungsten fuzz in an eroding plasma environment10.1088/0029-5515/51/4/043001 ↗
29. A description of bubble growth and gas release of helium implanted tungsten10.1016/j.jnucmat.2008.12.318 ↗
30. Loop punching and bubble rupture causing surface roughening —a model for W fuzz growth10.1209/0295-5075/105/25002 ↗
31. MD simulations of onset of tungsten fuzz formation under helium irradiation, Nucl10.1016/j.nimb.2012.11.029 ↗
32. Impact of low energy helium irradiation on plasma facing metals10.1016/j.jnucmat.2004.10.162 ↗
33. Microstructural evolution induced by low energy hydrogen ion irradiation in tungsten10.1016/0022-3115(94)00622-9 ↗
34. Microstructure evolution in tungsten during low-energy helium ion irradiation10.1016/S0022-3115(00)00289-0 ↗
35. Nastasi · 1996
36. Reduction of laser power threshold for melting tungsten due to subsurface helium holes10.1063/1.2387151 ↗
37. Breakaway bubble growth during the annealing of helium bubbles in metals10.1016/j.jnucmat.2004.04.349 ↗
38. The density and pressure of helium in bubbles in implanted metals: a critical review10.1080/00337578508222514 ↗
39. In-situ TEM observations of loop punching from helium platelet cavities in molybdenum10.1016/0036-9748(83)90351-4 ↗
40. Suppression of blister formation and deuterium retention on tungsten surface due to mechanical polishing and helium pre-exposure10.1088/0029-5515/45/7/016 ↗
41. Helium bubble bursting in tungsten10.1063/1.4860315 ↗
42. Blister formation on tungsten surface under low energy and high flux hydrogen plasma irradiation in NAGDIS-I10.1016/S0022-3115(02)01349-1 ↗
43. IMPACT: a facility to study the interaction of low-energy intense particle beams with dynamic heterogeneous surfaces10.1063/1.2805677 ↗
44. Helium and deuterium implantation in tungsten at elevated temperatures10.1016/j.jnucmat.2005.08.009 ↗
45. The response of polycrystalline tungsten to 30keV helium ion implantation at normal incidence and high temperatures10.1016/j.jnucmat.2011.10.029 ↗
46. Moulder · 1992
47. Carbon contamination and oxidation of Au surfaces under extreme ultraviolet radiation: an x-ray photoelectron spectroscopy study10.1116/1.4737160 ↗
48. Investigation on the effect of temperature excursion on the helium defects of tungsten surface by using compact plasma device10.1016/j.jnucmat.2010.12.021 ↗
49. W nano-fuzzes: a metastable state formed due to large-flux He+ irradiation at an elevated temperature10.1016/j.jnucmat.2016.10.018 ↗
50. Growth annealing equilibrium of tungsten nanostructures by helium plasma irradiation in non-eroding regimes10.1016/j.jnucmat.2013.04.040 ↗