journal article·2013-01

Influence of hydrogen content on fracture toughness of CWSR Zr–2.5Nb pressure tube alloy

R.N. Singh, A.K. Bind, N.S. Srinivasan, P. Ståhle

Journal of Nuclear Materials· Volume 432· Issue 1-3
Publisher page

Abstract

In this work, influence of hydrogen and temperature on the fracture toughness parameters of unirradiated, cold worked and stress relieved (CWSR) Zr-2.5Nb pressure tube alloys used in Indian Pressurized Heavy Water Reactor is reported. The fracture toughness tests were carried out using 17 mm width curved compact tension specimens machined from gaseously hydrogen charged tube-sections. Metallography of the samples revealed that hydrides were predominantly oriented along axial-circumferential plane of the tube. Fracture toughness tests were carried out in the temperature range of 30-300 degrees C as per ASTM standard E-1820-06, with the crack length measured using direct current potential drop (DCPD) technique. The fracture toughness parameters (J(Q), J(Max) and dJ/da), were determined. The critical crack length (CCL) for catastrophic failure was determined using a numerical method. It was observed that for a given test temperature, the fracture toughness parameters representing crack initiation (J(Q)) and crack propagation (J(Max), and dJ/da) is practically unaffected by hydrogen content. Also, for given hydrogen content, all the aforementioned fracture toughness parameters increased with temperature to a saturation value. (c) 2012 Elsevier B.V. All rights reserved. (Less)
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear and radioactivity studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. W. Dietz, Structural materials, in: R.W. Cahn, P. Haasen, E.J. Kramer (Eds.), Materials Science & Technol. A Comprehensive Treatment, Nuclear Materials, vol. 10B, 1994, p. 53 (Chapter 8).
2. Lemaignan · Nucl. Mater. · 1994 · 10B · 1
3. C.E. Coleman, B.A. Cheadle, C.D. Cann, J.R. Theaker, Development of pressure tubes with service life greater than 30 years, in: E.R. Bradley, G.P. Sabol (Eds.), Zr in the Nucl Ind.: 11th Intl. Symp., ASTM STP 1295, 1996, p. 884.
4. Field · Can. Metall. Q · 1985 · 24 · 18110.1179/000844385795448623 ↗
5. Puls · Nucl. Eng. Des. · 1997 · 171 · 13710.1016/S0029-5493(96)01310-6 ↗
6. G.D. Maon, P.J. Richinson, Leak before break in CANDU pressure tubes: recent advances, in: Pressure Vessel and Piping Conference 1993, Denver, CO., USA, 25–29 July 1993, 1993, p. 205.
7. J.R. Theaker, R. Choubey, G.D. Moan, S.A. Aldridge, L. Davis, R.A. Graham, C.E. Coleman, Fabrication of Zr–2.5Nb pressure tubes to minimize the harmful effects of trace elements, in: E.R. Bradley, G.P. Sabol (Eds.), Zr in Nucl. Ind.: 11th Intl. Symp., ASTM STP 1295, 1996, p. 221.
8. P.H. Davies, R.R. Hosbons, M. Griffiths, C.K. Chow, Correlation between irradiated and unirradiated fracture Toughness of Zr–2.5Nb pressure tubes, in: A.M. Garde, E.R. Bradley (Eds.), Zr in Nucl Ind.: 10th Intl. Symp., ASTM STP 1245, Philadelphia, 1994, p. 135.
9. M.B. Elmoselhi, B.D. Warr, A study of hydrogen uptake mechanism in zirconium alloys, in: A.M. Garde, E.R. Bradley (Eds.), Zr in Nucl Ind.: 10th Intl. Symp., ASTM STP 1245, Philadelphia, 1994, p. 62.
10. Northwood · Int. Met. Rev. · 1983 · 28 · 9210.1179/095066083790411759 ↗
11. Singh · J. Alloys Compd. · 2005 · 389 · 10210.1016/j.jallcom.2004.07.048 ↗
12. Pan · J. Nucl. Mater. · 1996 · 228 · 22710.1016/S0022-3115(95)00217-0 ↗
13. Davies · 1986
14. F.H. Huang, Fracture toughness evaluation for zircaloy-2 pressure tubes with the electric-potential method, in: ASTM Intl. Symp. on Small Specimen Test Techniques Applied to Nuclear Reactor Vessel Thermal Annealing and Plant Life Extension, New Orlearns, LA, USA, 29–31 January 1992, 1993, pp. 182–198.10.1520/STP12729S ↗
15. Chan · Acta Metall. Mater. · 1995 · 43 · 432510.1016/0956-7151(95)00133-G ↗
16. Simpson · 1987
17. Honda · Nucl. Eng. Des. · 1984 · 81 · 50910.1016/0029-5493(84)90003-7 ↗
18. Simpson · J. Nucl. Mater. · 1979 · 87 · 30310.1016/0022-3115(79)90567-1 ↗
19. Erickson · J. Inst. Met. · 1964 · 241 · 444
20. Simpson · Metall. Trans. · 1981 · 12A · 211310.1007/BF02644181 ↗
21. Singh · Mater. Sci. Eng. A · 2009 · 523 · 11210.1016/j.msea.2009.05.066 ↗
22. Pressure tube development for CANDU reactors
23. Singh · J. Nucl. Mater. · 2004 · 325 · 2610.1016/j.jnucmat.2003.10.009 ↗
24. A.C. Wallace, G.K. Shek, O.E. Lepik, Effects of hydride morphology on Zr–2.5Nb fracture toughness, in: L.F.P. Van Swam, C.M. Eucken (Eds.), Zr in Nucl. Ind.: 8th Intl. Symp., ASTM STP 1023, 1989, p. 66.10.1520/STP18858S ↗
25. Chow · J. Nucl. Mater. · 1997 · 246 · 8410.1016/S0022-3115(97)00087-1 ↗
26. Singh · J. Nucl. Mater. · 2005 · 345 · 14610.1016/j.jnucmat.2005.05.008 ↗
27. Singh · Nucl. Eng. Des. · 2011 · 241 · 242510.1016/j.nucengdes.2011.04.024 ↗
28. Singh · J. Nucl. Mater. · 2002 · 304 · 18910.1016/S0022-3115(02)00880-2 ↗
29. Singh · Mater. Sci. Eng. A · 2004 · 374 · 34210.1016/j.msea.2004.03.008 ↗
30. Standard Test Method for Measurement of Fracture Toughness – Designation: ASTM E 1820-06.
31. Puls · Metall. Trans. A · 1990 · 21A · 290510.1007/BF02647211 ↗
32. Srivastava · Metall. Trans. A · 1995 · 26A · 270710.1007/BF02669427 ↗