journal article·2018-01

Effect of temperature and dissolved oxygen on stress corrosion cracking behavior of P92 ferritic-martensitic steel in supercritical water environment

Z. Zhang, Z.F. Hu, L.F. Zhang, K. Chen, P.M. Singh

Publisher page

Abstract

Abstract The effect of temperature and dissolved oxygen (DO) on stress corrosion cracking (SCC) of P92 martensitic steel in supercritical water (SCW) was investigated using slow strain rate test (SSRT) and fractography analysis. The SSRT was carried out at temperatures of 400, 500, 600 °C in deaerated supercritical water and at DO contents of 0, 200, 500 ppb at the temperature of 600 °C, respectively. The results of SSRT show that the decrease of ductility at the temperature of 400 °C may be related to the dynamic strain aging (DSA) of P92 steel. The degradation of the mechanical properties in SCW is the joint effect of temperature and SCC. Compared with the effect of temperature, DO in SCW has no significant effect on the SCC susceptibility of P92 steel. The observation of oxide layer shows that large numbers of pores are nucleated in the oxide layer, which is related to vacancy accumulation and hydrogen generated in the oxide layer. Under the combined action of the growth stress and tensile stress, micro cracks, nucleated from the pores in the oxide layer, are easily propagated intergranularly outward to the surface of specimen, and fewer cracks can extend inward along the intrinsic pores to the inner oxide/metal interface, which is the reason for the exfoliation of oxide films.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (60)

Show source-provided references
1. Recent progress in solid breeder blanket development at JAEA10.13182/FST07-A1620 ↗
2. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
3. SCC behavior of austenitic and martensitic steels in supercritical pressurized water10.1016/j.jnucmat.2011.02.033 ↗
4. Stress corrosion cracking susceptibility of austenitic stainless steels in supercritical water conditions10.1016/j.jnucmat.2010.09.018 ↗
5. Watanabe · 2003
6. Corrosion behavior of Ni-based alloys for advanced high temperature water-cooled nuclear plants10.1016/j.corsci.2008.08.024 ↗
7. Allen · 2002
8. Ferritic/martensitic steels for next-generation reactors10.1016/j.jnucmat.2007.05.005 ↗
9. Recent advances in creep-resistant steels for power plant applications10.1007/BF02706455 ↗
10. Carbide reactions and phase equilibria in low alloy Cr–Mo–V steels tempered at 773–993 K. Part I: experimental measurements10.1016/S1359-6454(97)00238-3 ↗
11. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
12. Corrosion behavior of 9–12% Cr ferritic–martensitic steels in supercritical water10.1016/j.corsci.2009.12.032 ↗
13. Oxidation behavior of ferritic–martensitic and ODS steels in supercritical water10.1016/j.jnucmat.2012.03.009 ↗
14. Analysis of high temperature deformation mechanism in ODS EUROFER 97 alloy10.1016/j.jnucmat.2008.08.009 ↗
15. SCC and corrosion evaluations of the F/M steels for a supercritical water reactor10.1016/j.jnucmat.2007.03.168 ↗
16. Improvement of compatibility of advanced ferritic steels with super critical pressurized water toward a higher thermally efficient water-cooled blanket system10.1016/j.fusengdes.2005.09.056 ↗
17. Influence of alloy composition and temperature on corrosion behavior of ODS ferritic steels10.1016/j.jnucmat.2010.12.279 ↗
18. Stress corrosion cracking susceptibility of oxide dispersion strengthened ferritic steel in supercritical pressurized water dissolved with different hydrogen and oxygen contents10.1016/j.corsci.2013.09.016 ↗
19. Influence of the dissolved oxygen content on corrosion of the ferritic- martensitic steel P92 in supercritical water10.1016/j.corsci.2011.11.013 ↗
20. Porosity prediction in supercritical water exposed ferritic/martensitic steel HCM12A10.1016/j.corsci.2006.05.026 ↗
21. 2003
22. The evolution of dislocation density during heat treatment and creep of tempered martensite ferritic steel10.1016/S1359-6454(03)00324-0 ↗
23. Microstructural observation of tempered martensite in medium- carbon low-alloy steel by atomic force microscopy10.2320/jinstmet1952.64.6_460 ↗
24. Observations of prior austenite grain boundaries and carbides in the same area of tempered martensite in medium-carbon steel by atomic force microscopy10.2320/jinstmet1952.65.8_734 ↗
25. 2013
26. Influence of dynamic strain aging pre-treatment on the low-cycle fatigue behavior of modified 9Cr-1Mo steel10.1016/j.ijfatigue.2012.07.011 ↗
27. Comparison of various 9-12 % Cr steels under fatigue and creep-fatigue loadings at high temperature10.1016/j.msea.2011.05.046 ↗
28. Dynamic strain aging behavior of modified 9Cr-1Mo steel under monotonic and cyclic loading10.1016/j.proeng.2017.04.155 ↗
29. Influence of temperature on tensile flow and work hardening behaviour of modified 9Cr–1Mo steel10.1179/0960340913Z.0000000008 ↗
30. The effect of temperature on fatigue crack growth behavior of a low-alloy pressure vessel steel in a simulated BWR environment10.1016/0010-938X(85)90006-X ↗
31. Role of dynamic strain-ageing in the environment assisted cracking observed in pressure vessel steels10.1111/j.1460-2695.1997.tb00396.x ↗
32. Dependence of stress corrosion cracking of alloy 690 on temperature, cold work, and carbide precipitation—role of diffusion of vacancies at crack tips10.5006/1.3563640 ↗
33. Characterizing the effect of creep on stress corrosion cracking of cold worked alloy 690 in supercritical water environment10.1016/j.jnucmat.2017.05.018 ↗
34. Miyasaka · 1990
35. Cyclic slip irreversibilities and the evolution of fatigue damage10.1007/s11661-009-9839-8 ↗
36. Deformation and cracking behavior of protective oxide scales on heat-resistant steels under tensile strain10.1007/BF00664232 ↗
37. Schütze · 1997
38. Effects of exposure temperature and time on corrosion behavior of a ferritic-martensitic steel P92 in aerated supercritical water10.1016/j.corsci.2014.10.022 ↗
39. Microstructural examination of oxide layers formed on an oxide dispersion strengthened ferritic steel exposed to supercritical water10.1016/j.jnucmat.2006.07.021 ↗
40. Evolution of the oxide structure of 9CrODS steel exposed to supercritical water10.1016/j.jnucmat.2009.03.015 ↗
41. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
42. Corrosion of ferritic–martensitic steels in steam and supercritical water10.1016/j.jnucmat.2012.09.037 ↗
43. EFTEM and EELS analysis of the oxide layer formed on HCM12A exposed to SCW10.1016/j.jnucmat.2012.06.017 ↗
44. Oxidation of ferritic–martensitic alloys T91, HCM12A and HT-9 in supercritical water10.1016/j.jnucmat.2007.05.023 ↗
45. Magnetite solubility and phase stability in alkaline media at elevated temperatures10.1007/BF00973442 ↗
46. Predictive model for equilibrium constants of aqueous inorganic species at subcritical and supercritical conditions10.1021/ie010956y ↗
47. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part III)10.1016/j.corsci.2008.06.049 ↗
48. Superabundant vacancies formed in metal-hydrogen alloys10.1238/Physica.Topical.103a00011 ↗
49. The role of dissolved oxygen in supercritical water in the oxidation of ferritic–martensitic steel10.1016/j.supflu.2015.10.017 ↗
50. Transport processes during the growth of oxide films at elevated temperature10.1103/RevModPhys.57.437 ↗
51. Oxygen transport during the high temperature oxidation of pure nickel10.1007/s11085-005-6560-x ↗
52. Continuous and cyclic oxidation of T91 ferritic steel under steam10.1016/S0010-938X(03)00173-2 ↗
53. Steam oxidation of 9–12%Cr steels: critical evaluation and implications for practical application10.5006/1065 ↗
54. Oxide structures produced on iron-chromium alloys by a dissociative mechanism10.1149/1.2425624 ↗
55. The mechanism of the high-temperature oxidation of iron-chromium alloys in water vapor10.1149/1.2425963 ↗
56. Birks · 2006
57. Oxidation behavior of iron-based alloy HCM12A exposed in supercritical water10.1016/j.corsci.2005.10.010 ↗
58. Gangloff · 2003 · vol. 6 · 31
59. Hydrogen embrittlement phenomena and mechanisms10.1515/corrrev-2012-0502 ↗
60. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗