Ni coating on 316L stainless steel using cage plasma treatment: Feasibility and swelling studies
Source abstract
Abstract
Abstract A modified cage plasma nitriding technique is used to coat a Ni film onto a 316L substrate as a protective layer for austenitic steels in molten fluoride salts. The coating is achieved by deposition of Ni atoms sputtered from a Ni cage with a 316L substrate floated at the same potential as the cage to reduce plasma sputtering on the substrate. The Ni coating is porosity-free and precipitation-free and forms a γ-(Fe, Ni) phase due to interdiffusion from the substrate. Beneath the interdiffusion layer exists a thick γ-phase layer mainly affected by long-range nitrogen diffusion along the grain boundary. This layer develops grain boundary Cr nitride precipitates. Ion irradiation on the polished cross-section of the plasma-treated sample shows no void swelling in the surface-deposited Ni layer, very limited void formation in N diffusion layer, and significant void swelling in bulk unaffected by nitrogen. The studies demonstrate the feasibility of the technique for Ni coating and show good swelling resistance of the coating layer and N diffusion-affected layer. Mechanisms are discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Fusion materials and technologies · Ion-surface interactions and analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. S-phase surface engineering of Fe-Cr, Co-Cr and Ni-Cr alloys10.1179/095066009X12572530170589 ↗
2. Pye · 2003
3. Bernal · 2006
4. The wear and corrosion properties of stainless steel nitrided by low-pressure plasma-arc source ion nitriding at low temperatures10.1016/S0257-8972(00)00713-1 ↗
5. Plasma nitriding of AISI 304 austenitic stainless steel with pre-shot peening10.1016/j.surfcoat.2010.03.018 ↗
6. Surface modification of AISI 304 austenitic stainless steel by plasma nitriding10.1016/S0169-4332(03)00260-5 ↗
7. Stainless steel 2000 : proceedings of an international current status seminar on thermochemical surface engineering of stainless steel : held in osaka, Japan, november 2000
8. Environmentally friendly low temperature plasma processing of stainless steel components for nuclear industry
9. New trends in DECR plasma technology: applications to novel duplex treatments and process combinations with extreme plasma specifications10.1016/S0257-8972(01)01020-9 ↗
10. Microstructure and corrosion of nitrogen implanted AISI 304 stainless steel10.1016/0257-8972(92)90209-S ↗
11. Use of cathodic cage in plasma nitriding10.1016/j.surfcoat.2006.04.014 ↗
12. Cathodic cage plasma nitriding: an innovative technique10.1155/2012/385963 ↗
13. Introduction to surface hardening of steels
14. 14 - low temperature surface hardening of stainless steel
15. Corrosion of hastelloy-N in molten flinak loop
16. Sridharan · 2008
17. Materials corrosion in molten LiF–NaF–KF salt10.1016/j.jfluchem.2008.05.008 ↗
18. High temperature corrosion studies in molten salt-FLiNaK, Corrosion Engineering
19. Corrosion-induced microstructural developments in 316 stainless steel during exposure to molten Li2BeF4(FLiBe) salt10.1016/j.jnucmat.2016.10.023 ↗
20. Nickel-plating for active metal dissolution resistance in molten fluoride salts10.1016/j.jnucmat.2011.01.032 ↗
21. Neutron-induced swelling and embrittlement of pure iron and pure nickel irradiated in the BN-350 and BOR-60 fast reactors10.1016/j.jnucmat.2008.01.015 ↗
22. Swelling resistance of advanced austenitic alloy A709 and its comparison with 316 stainless steel at high damage levels10.1016/j.jnucmat.2019.151818 ↗
23. J.L. Vossen, W. Kern, Thin Film Processes II, Elsevier.
24. The effect of argon admixing on nitriding of plain carbon steel in N2 and N2-H2 plasma10.1016/j.surfcoat.2018.07.004 ↗
25. Spectroscopy of flowing discharges and post-discharges in reactive gases10.1016/0257-8972(93)90056-T ↗
26. Nitriding of stainless steel in an rf plasma10.1063/1.343664 ↗
27. Phase stability in the Fe–Ni system: investigation by first-principles calculations and atomistic simulations10.1016/j.actamat.2005.05.001 ↗
28. Critical evaluation of the Fe–Ni, Fe–Ti and Fe–Ni–Ti alloy systems10.1016/j.intermet.2005.11.028 ↗
29. Anon · 1984
30. The stopping and range of ions in mater10.1016/j.nimb.2010.02.091 ↗
31. The influence of ion beam rastering on the swelling of self-ion irradiated pure iron at 450 °C10.1016/j.jnucmat.2015.05.025 ↗
32. Effect of irradiation mode on the microstructure of self-ion irradiated ferritic-martensitic alloys10.1016/j.jnucmat.2015.05.016 ↗
33. Beam-contamination-induced compositional alteration and its neutron-atypical consequences in ion simulation of neutron-induced void swelling10.1080/21663831.2017.1323808 ↗
34. Carbon contamination, its consequences and its mitigation in ion-simulation of neutron-induced swelling of structural metals
35. Impact of composition modification induced by ion beam Coulomb-drag effects on the nanoindentation hardness of HT910.1016/j.nimb.2018.12.051 ↗
36. Sputter-deposited nanocrystalline Cr and CrN coatings on steels10.1016/S0257-8972(00)01120-8 ↗
37. Structure and corrosion resistance of plasma nitrided stainless steel10.1179/sur.1985.1.2.131 ↗
38. Structure and properties of plasma-nitrided stainless steel10.1016/0257-8972(95)08246-8 ↗
39. Characteristics of martensitic stainless steel nitrided in a low-pressure RF plasma10.1016/S0257-8972(02)00631-X ↗
40. Thermal stability and phase decomposition of nitrided layers on 316L and 310 austenitic stainless steels10.1016/j.surfcoat.2017.07.014 ↗
41. Nitriding of austenitic stainless steel by plasma immersion ion implantation10.1016/0257-8972(95)08370-7 ↗
42. Decomposition kinetics of expanded austenite with high nitrogen contents10.1515/ijmr-2006-0012 ↗
43. DeVan · 1962 · 14
44. Effect of nitrogen and stacking-fault energy on twinning in Fe-15Mn-2Cr-0.6C-xN single crystals of austenitic stainless steels10.1134/S0031918X09090117 ↗
45. Was · 2007 · 1
46. Corrosion of structural alloys in high-temperature molten fluoride salts for applications in molten salt reactors