journal article·2023-04Open access

Performance and evolution of cold spray Cr-coated optimized ZIRLO™ claddings under simulated loss-of-coolant accident conditions

Andrea Fazi, Mohammad Sattari, Krystyna Stiller, Hans-Olof Andrén, Mattias Thuvander

Abstract

The performance of Cr-coated Optimized ZIRLO™ as accident tolerant fuel cladding material for pressurized water reactors (PWRs) is assessed. The coating oxidation mechanisms, oxide stability, and the transformation of the Cr-coating/Optimized ZIRLO™ interface are among the studied phenomena. For this purpose, samples were exposed at 1200°C in steam for 3 min, 20 min and 40 min. As-fabricated coated claddings, plus specimens tested in autoclave at 415°C for 90 days in simulated PWR water chemistry were employed for comparison. Characterization techniques such as scanning electron microscopy, energy dispersive x-ray spectroscopy, electron backscattered diffraction, and transmission electron microscopy were used to determine the chemistry and crystalline structure of the various phases formed during the different exposures. When exposed to loss-of-coolant accident (LOCA) conditions for 40 min, a layer of Cr2O3 up to 8 µm thick was measured on the outer surface of the Cr-coating. No significant oxidation of the underlaying Optimized ZIRLO™ alloy occurred, and the applied coating appears to be very effective at delaying the cladding degradation under accident conditions. At the coating-substrate interface, a 1–2 µm thick layer of (Cr,Fe)2Zr Laves phase was found. The presence of this phase appears to have no detrimental effects on the coating performance, and it might play a role in slowing down the dissolution of the coating into the substrate. ZrO2 particles were frequently found at grain boundaries in the coating after exposure to LOCA conditions. For longer exposure time, these particles are expected to grow into a ZrO2-network, creating a fast diffusion path for O, and compromising the oxidation protection offered by the coating.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (64)

Show source-provided references
1. Accident tolerant fuels for LWRs: A perspective10.1016/j.jnucmat.2013.12.005 ↗
2. Accident tolerant fuel cladding development: Promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
3. On-going studies at CEA on chromium coated zirconium based nuclear fuel claddings for enhanced Accident Tolerant LWRs Fuel
4. Development of cold spray chromium coatings for improved accident tolerant zirconium-alloy cladding10.1016/j.jnucmat.2019.03.039 ↗
5. High temperature oxidation and microstructural evolution of cold spray chromium coatings on Zircaloy-4 in steam environments10.1016/j.jnucmat.2019.151737 ↗
6. Out-of-pile performance of surface-modified Zr cladding for accident tolerant fuel in LWRs10.1016/j.jnucmat.2018.07.061 ↗
7. Development of Cr cold spray–coated fuel cladding with enhanced accident tolerance10.1016/j.net.2017.12.011 ↗
8. Fuel performance of chromium-coated zirconium alloy and silicon carbide accident tolerant fuel claddings10.1016/j.anucene.2018.06.001 ↗
9. Semi-integral LOCA test of cold-spray chromium coated zircaloy-4 accident tolerant fuel cladding10.1016/j.jnucmat.2021.152940 ↗
10. Mechanical and chemical properties of PVD and cold spray Cr-coatings on Zircaloy-410.1016/j.jnucmat.2020.152420 ↗
11. High temperature steam oxidation of chromium-coated zirconium-based alloys: Kinetics and process10.1016/j.corsci.2020.108537 ↗
12. Fiber texture-dependent oxidation behaviour of Cr-coated zirconium alloy in high temperature steam10.1016/j.corsci.2022.110449 ↗
13. Cold Spray Coatings for Accident Tolerant Zr-Alloy Cladding in Light Water Reactors
14. Indication of chromium oxide hydroxide evaporation during oxidation of 304L at 873 K in the presence of 10% water vapor10.1023/A:1018875024306 ↗
15. Effects of water vapour on isothermal oxidation of chromia-forming alloys in Ar/O2 and Ar/H2 atmospheres10.1016/j.corsci.2009.08.032 ↗
16. Oxide evolution on Alloy X-750 in simulated BWR environment10.1016/j.jnucmat.2016.09.026 ↗
17. Corrosion of pre-oxidized nickel alloy X-750 in simulated BWR environment10.1016/j.jnucmat.2017.01.051 ↗
18. Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.002 ↗
19. Revised pourbaix diagrams for chromium at 25–300°C10.1016/S0010-938X(97)89244-X ↗
20. p-Type and n-Type Behavior of Chromium Oxide as a Function of the Applied Potential10.1149/1.2100850 ↗
21. Chromia Scale Thermally Grown on Pure Chromium Under Controlled p(O2) Atmosphere: II—Spallation Investigation Using Photoelectrochemical Techniques at a Microscale10.1007/s11085-018-9848-3 ↗
22. Duplex n- and p-Type Chromia Grown on Pure Chromium: A Photoelectrochemical and Microscopic Study10.1007/s11085-016-9648-6 ↗
23. The role of metal vacancies during high-temperature oxidation of alloys10.1038/s41529-018-0046-1 ↗
24. Paralinear Oxidation of Chromium in O2 + H2O Environment at 600–700°C10.1007/s11085-008-9114-1 ↗
25. High temperature oxidation of chromium: Kinetic modeling and microstructural investigation10.1016/j.ssi.2013.02.017 ↗
26. Characterization of chromia scales grown on pure chromium in different oxidizing atmospheres10.1179/mht.2000.17.2.008 ↗
27. The Volatilization of Chromium Oxide10.1149/1.2428106 ↗
28. Effect of water vapour partial pressure on the chromia (Cr2O3)-based scale stability10.1080/00084433.2017.1373968 ↗
29. Cr coated cladding Development At Framatome
30. Review of manufacturing technologies for coated accident tolerant fuel cladding10.1016/j.jnucmat.2022.153562 ↗
31. Cold spray technology in nuclear energy applications: A review of recent advances10.1016/j.anucene.2020.107835 ↗
32. Cavaliere · 2017
33. A. G2-88(2002), Standard Test Method for Corrosion Testing of Products of Zirconium, Hafnium, and Their Alloys in Water at 680°F or in Steam at 750°F, 88 (1988) 1–8. doi:10.1520/G0002-88R02.10.1520/G0002-88R02 ↗
34. In situ site-specific specimen preparation for atom probe tomography10.1016/j.ultramic.2006.06.008 ↗
35. In situ lift-out: Steps to improve yield and a comparison with other FIB TEM sample preparation techniques10.1016/j.micron.2008.02.006 ↗
36. Oxidation kinetics of Cr-coated zirconium alloy: Effect of coating thickness and microstructure10.1016/j.corsci.2020.108883 ↗
37. Characterization of as-deposited cold sprayed Cr-coating on Optimized ZIRLOTM claddings10.1016/j.jnucmat.2021.152892 ↗
38. Cold sprayed Cr-coating on Optimized ZIRLOTM claddings: the Cr/Zr interface and its microstructural and chemical evolution after autoclave corrosion testing10.1016/j.jnucmat.2022.153505 ↗
39. The Cr-Zr (Chromium-Zirconium) System10.1007/BF02868997 ↗
40. Mapping the tetragonal to monoclinic phase transformation in zirconia core dental crowns10.1016/j.dental.2011.09.004 ↗
41. Phase diagram of the system: ZrO2–Cr2O310.1016/S0272-8842(00)00071-7 ↗
42. The Effect of Oxide Grain Structure on the High-Temperature Oxidation of Fe, Ni and Cr10.1179/cmq.1979.18.3.283 ↗
43. Mechanism for secondary electron dopant contrast in the SEM10.1093/oxfordjournals.jmicro.a023811 ↗
44. Oxidation of Advanced Zirconium Cladding Alloys in Steam at Temperatures in the Range of 600–1200°C10.1007/s11085-011-9249-3 ↗
45. High-temperature oxidation and quenching of chromium-coated zirconium alloy ATF cladding tubes with and w/o pre-damage10.1016/j.jnucmat.2021.153470 ↗
46. Effects of hydrogen on thermal creep behaviour of Zircaloy fuel cladding10.1016/j.jnucmat.2017.10.015 ↗
47. Creep studies for zircaloy life prediction in water reactors10.1007/s11837-999-0184-6 ↗
48. Corrosion of Zirconium Alloys Used for Nuclear Fuel Cladding10.1146/annurev-matsci-070214-020951 ↗
49. Effect of grain size on corrosion: A review10.5006/1.3462912 ↗
50. Self-diffusion in chromium10.1080/14786436508224234 ↗
51. Thermodynamic modeling and experimental study of the Fe–Cr–Zr system10.1016/j.jnucmat.2013.05.061 ↗
52. Nano-scale chemical evolution in a proton-and neutron-irradiated Zr alloy10.1016/j.jnucmat.2017.01.049 ↗
53. Formation and fine-structures of nano-precipitates in ZIRLO10.1016/j.jallcom.2016.06.131 ↗
54. Self-diffusion in Zr-Cr and Zr-Fe alloys10.1080/01418618108236174 ↗
55. Early studies on Cr-Coated Zircaloy-4 as enhanced accident tolerant nuclear fuel claddings for light water reactors10.1016/j.jnucmat.2019.02.018 ↗
56. High temperature Cr-Zr interaction of two types of Cr-coated Zr alloys in inert gas environment10.1016/j.jnucmat.2021.152806 ↗
57. Diffusion in the c15-type intermetallic laves phase NbCo210.1080/01418610008212113 ↗
58. Effect of residual stress on recrystallization behavior of mechanically alloyed steels10.1016/j.scriptamat.2009.09.023 ↗
59. On the evolution of substrate's residual stress during cold spray process: A parametric study10.1016/j.matdes.2017.10.062 ↗
60. The effect of a simple annealing heat treatment on the mechanical properties of cold-sprayed aluminum10.1361/105996306X108138 ↗
61. Atomic-scale interface structure of a Cr-coated Zircaloy-4 material10.1007/s10853-018-2333-1 ↗
62. In Prague, Experimental Behavior of Chromium-Based Coatings
63. Structural analysis of Arc-PVD multilayer metal nitride coatings CrN/MoN using electron backscatter diffraction (EBSD)
64. Atom Probe Analysis of Thin Oxide Layers on Zircaloy Needles10.1051/jphyscol:1989851 ↗