The corrosion of zirconium under deep geologic repository conditions
Source abstract
Abstract
Abstract Zirconium alloys are widely used in nuclear reactors as fuel cladding and as reactor structural elements (i.e., CANDU reactor pressure tubes), and are therefore a component of the waste materials that could be emplaced in a deep geologic repository. Therefore, the corrosion mechanisms and rates for relevant zirconium alloys under repository conditions have been reviewed. Since titanium and zirconium alloys have many similarities, and because the data base for the corrosion of titanium alloys under repository conditions is considerably more extensive than that for zirconium alloys, the electrochemical and corrosion behavior of both materials have been compared and evaluated. Although electrochemical studies suggest Zircaloy cladding could be susceptible to pitting, redox conditions within a failed waste container will remain reducing and unable to support pitting. This leaves passive corrosion as the only long-term corrosion mechanism. The available data indicates that the rate of passive corrosion will be very low. A rate of 20 nm/year would be a reasonable upper limit but it is likely the rate will be less than 1 nm/year.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. P.T. Truant, CANDU fuel Performance: Power Reactor Experience, Atomic Energy of Canada Limited Report AECL-MISC-250 Chalk River, Canada, 1983.
2. J.C. Tait, H. Roman, C.A. Morrison, Characteristics and Radionuclide Inventories of Used Fuel from OPG Nuclear Generating Stations, vols. 1 and 2, Ontario Power Generation, Report 06819-REP-01200-10029-R00, Toronto, Canada, 2000.
3. D.W. Shoesmith, B.M. Ikeda, The Resistance of Titanium to Pitting, Microbially Induced Corrosion, and Corrosion under Unsaturated Conditions, Atomic Energy of Canada Limited, Report AECL-11709, COG-96-557-I, Chalk River, Canada, 1997.
4. F. Hua, K. Mon, P. Pasupathi, G. Gordon, D.W. Shoesmith, Corrosion of Grade-7 and other Ti alloys in nuclear waste repository environments — a review, in: Corrosion 2004, NACE, Houston, Texas, 2004.10.2172/837505 ↗
5. Hua · Corrosion · 2005 · 61 · 98710.5006/1.3280899 ↗
6. Hua · JOM-US · 2005 · 57 · 2010.1007/s11837-005-0059-4 ↗
7. F. Hua, K. Mon, P. Pasupathi, G. Gordon, D.W. Shoesmith, Hydrogen induced cracking of titanium alloys in environments anticipated in the Yucca Mountain Nuclear Waste Repository, in: Ciorrosion 2005, NACE, Houston, Texas, USA, 2005.
8. Shoesmith · Corrosion · 2006 · 62 · 70310.5006/1.3278296 ↗
9. R.W. Schutz, D.E. Thomas, Corrosion of titanium and titanium alloys, in: ASM Metal Handbook, 1987, pp. 669–706.
10. Titanium and titanium alloys
11. Corrosion of titanium and its alloys
12. Torresi · Electrochim. Acta · 1987 · 32 · 129110.1016/0013-4686(87)85058-2 ↗
13. Z.M. Jarzebski, Oxide semiconductors, in: International Series of Monographs in Science of the Solid-State, Pergamon Press, New York, New-York, USA, 1973.
14. Meisterjahn · J. Electroanal. Chem. · 1987 · 217 · 15910.1016/0022-0728(87)85072-6 ↗
15. Noel · J. Electrochem. Soc. · 2008 · 155 · C44410.1149/1.2937306 ↗
16. Tun · J. Electrochem. Soc. · 1999 · 146 · 98810.1149/1.1391710 ↗
17. Cox · J. Electrochem. Soc. · 1970 · 117 · 65410.1149/1.2407598 ↗
18. Leach · Corros. Sci. · 1988 · 28 · 4310.1016/0010-938X(88)90005-4 ↗
19. Ortega · J. Electrochem. Soc. · 1982 · 129 · 190510.1149/1.2124323 ↗
20. Shibata · Corros. Sci. · 1995 · 37 · 25310.1016/0010-938X(94)00133-Q ↗
21. Noel · Electrochem. Solid State · 2000 · 3 · 47310.1149/1.1391183 ↗
22. Khalil · Electrochim. Acta · 1986 · 31 · 127910.1016/0013-4686(86)80148-7 ↗
23. Y. Zeng, Passive Film Properties and Their Influence on Hydrogen Absorption into Titanium, Ph. D. Thesis, University of Western Ontario, London, Ontario, Canada, 2009.
24. Nowierski · Electrochem. Commun. · 2009 · 11 · 123410.1016/j.elecom.2009.04.008 ↗
25. C. Nowierski, Analysis of the Electrochemistry and Surface Microstructure of Zirconium Alloys Under Cathodic Polarization, M. Sc. Thesis, University of Western Ontario, London, Ontario, Canada, 2009.
26. Ohtsuka · J. Electrochem. Soc. · 1987 · 134 · 240610.1149/1.2100212 ↗
27. Zhu · Chem. Mater. · 2007 · 19 · 253310.1021/cm070023d ↗
28. Zhu · Anal. Chem. · 2008 · 80 · 143710.1021/ac701796u ↗
29. Casillas · J. Electrochem. Soc. · 1994 · 141 · 63610.1149/1.2054783 ↗
30. Y. Ito, T. Furuya, Correlation between electrochemical properties and corrosion resistance of zirconium alloys, in: E.R. Bradley, G.P. Sabol (Eds.), Zirconium in the Nuclear Industry: Eleventh International Symposium, ASTM STP 1295, American Society for Testing and Materials, 1996, pp. 163–180.
31. H. Jensen, Properties of Anodic Oxide Films on Zirconium Alloys, Ph. D. Thesis, University of Western Ontario, London, Ontario, Canada, 2002.
32. Waterside Corrosion of Zirconium Alloys in Nuclear Power Plants, International Atomic Energy Agency, Technical Document IAEA-TECDOC-996, Vienna, Austria, 1998.
33. Cox · Electrochem. Technol. · 1966 · 4 · 121
34. Cox · J. Nucl. Mater. · 1968 · 28 · 7310.1016/0022-3115(68)90058-5 ↗
35. Cox · J. Nucl. Mater. · 1969 · 31 · 4810.1016/0022-3115(69)90043-9 ↗
36. Yilmazbayhan · J. Nucl. Mater. · 2006 · 349 · 26510.1016/j.jnucmat.2005.10.012 ↗
37. Hutchinson · J. ASTM Int. · 2007 · 410.1520/JAI101106 ↗
38. Ai · J. Nucl. Mater. · 2008 · 379 · 16210.1016/j.jnucmat.2008.06.011 ↗
39. Hatano · J. Nucl. Sci. Technol. · 1996 · 33 · 94410.3327/jnst.33.944 ↗
40. Shaltiel · J. Less-Common Met. · 1977 · 53 · 11710.1016/0022-5088(77)90162-X ↗
41. Cox · J. Nucl. Mater. · 1968 · 27 · 110.1016/0022-3115(68)90002-0 ↗
42. Cox · J. Nucl. Mater. · 1987 · 148 · 33210.1016/0022-3115(87)90027-4 ↗
43. F. Garisto, T. Kempe, P. Gierszewski, Technical Summary of the Safety Aspects of the Deep Geological Repository Concept for Used Nuclear Fuel, Nuclear Waste Management Organization, Technical Report NWMO TR-2009-12, Toronto, Canada, 2009.
44. P. Maak, Development of a used fuel container for nuclear fuel waste, in: Materials Research Society Symposium, 2007, pp. 447–451.
45. R. Little, J. Avis, N. Calder, N. Garisto, P. Humphreys, F. King, L. Limer, R. Metcalf, J. Penfold, J. Rees, D. Savage, P. Suckling, G. Towler, R. Walke, R. Walsh, Postclosure Safety Assessment (V1) Report, Nuclear Waste Management Organization Report NWMO DGR-TR-2009-01, Toronto, Canada, 2009.
46. D.W. Shoesmith, Used Fuel and Uranium Dioxide Dissolution Studies – A Review, Nuclear Waste Management Organization Report NWMO-TR-2007-03 2007.
47. P. Wersin, L.H. Johnson, B. Schwyn, U. Berner, E. Curti, Redox Conditions in the Near Field of a Repository for SF/HLW and ILW in Opalinus Clay, Nagra, Technical Report 02-13, Wettingen, Switzerland, 2003.
48. L. Duro, M. Grive, E. Cera, X. Gaona, C. Domench, J. Bruno, Determination and Assessment of the Concentration Limits to be Used in SR-Can, Swedish Nuclear Fuel and Waste Management Company, Technical Report TR-06-32, Stockholm, Sweden, 2006.
49. D.J. Blackwood, C.C. Naish, N. Platts, K.J. Taylor, M.I. Thomas, The Anaerobic Corrosion of Carbon Steel in Granite Groundwater, Swedish Nuclear Fuel and Waste Management Company, Technical Report TR-95-03, Stockholm, Sweden, 1995.
50. Smart · Corrosion · 2002 · 58 · 62710.5006/1.3287691 ↗
51. Smart · Corrosion · 2002 · 58 · 54710.5006/1.3277646 ↗
52. Lee · Electrochim. Acta · 2006 · 51 · 155810.1016/j.electacta.2005.02.115 ↗
53. Xu · Electrochim. Acta · 2009 · 54 · 572710.1016/j.electacta.2009.05.020 ↗
54. A.J. Elliott, D.M. Bartels, The reaction Set, Rate Constants and g-Values for the Simulation of Radiolysis of Light Water Over the Range 20° to 350°C based on Information Available in 2008, Atomic Energy of Canada Limited, Report 153-127160-450-001, Chalk River, Canada, 2009.
55. D.W. Shoesmith, The Role Of Dissolved Hydrogen on the Corrosion/Dissolution of Spent Nuclear Fuel, Nuclear Waste Management Organization Technical Report NWMO-TR-2008-19, Totonto, Canada, 2008.
56. Jonsson · Environ. Sci. Technol. · 2007 · 41 · 708710.1021/es070832y ↗
57. J.J. Noël, The electrochemistry of Titanium Corrosion, Ph. D. Thesis, University of Manitoba, Winnipeg, Manitoba, Canada, 1999.
58. X. He, Effects of Temperature, Impurities, and Alloying Elements on the Crevice Corrosion of Alpha Titanium Alloys, Ph. D. Thesis, University of Western Ontario, London, Ontario, Canada, 2003.
59. Cheng · Mater. Chem. Phys. · 1993 · 36 · 15610.1016/0254-0584(93)90025-H ↗
60. Hodgkiess · Desalination · 1987 · 66 · 14710.1016/0011-9164(87)90202-5 ↗
61. Knittel · Corrosion · 1984 · 40 · 910.5006/1.3579296 ↗
62. Jangg · Werkst Korros. · 1978 · 29 · 1610.1002/maco.19780290104 ↗
63. Mamun · Electrochim. Acta · 2001 · 46 · 334310.1016/S0013-4686(01)00544-8 ↗
64. Knittel · Corrosion · 1982 · 38 · 26510.5006/1.3577349 ↗
65. C.A. Greene, C.S. Brossia, D.S. Dunn, G.A. Cragnolino, Environmental and electrochemical factors on the localized corrosion of Zircaloy-4, in: Corrosion 2000, Houston, Texas, 2000.
66. Fahey · Corrosion · 1997 · 53 · 5410.5006/1.3280434 ↗
67. Hornkjoel · Electrochim. Acta · 1988 · 33 · 28910.1016/0013-4686(88)80016-1 ↗
68. M. Maguire, The Pitting Susceptibility of Zirconium in Aqueous Chloride, Bromide, and Iodide Solutions, vol. 830, ASTM Special Technical Publication, 1984, pp. 177–189.
69. Mankowski · Mater. Sci. Forum · 1989 · 44-45 · 27910.4028/www.scientific.net/MSF.44-45.279 ↗
70. Satpati · Corros. Sci. · 2005 · 47 · 144510.1016/j.corsci.2004.08.004 ↗
71. Bellanger · J. Mater. Sci. · 2000 · 35 · 175910.1023/A:1004732703500 ↗
72. Gardiazabal · J. Electroanal. Chem. · 1981 · 119 · 38910.1016/S0022-0728(81)80070-8 ↗
73. Gomez · J. Electroanal. Chem. · 1985 · 188 · 3910.1016/S0022-0728(85)80048-6 ↗
74. Chen · Corrosion · 1985 · 41 · 43810.5006/1.3583824 ↗
75. Galvele · Corros. Sci. · 1990 · 31 · 56310.1016/0010-938X(90)90163-Y ↗
76. Schennach · J. Vac. Sci. Technol. A · 2000 · 18 · 147810.1116/1.582372 ↗
77. D.W. Shoesmith, F. King, The Effects of Gamma Radiation on the Corrosion of Candidate Materials for the Fabrication of Nuclear Waste Packages, Atomic Energy of Canada Limited, Report AECL-11999, Chalk River, Canada, 1999.
78. D. Landolt, A. Davenport, J. Payer, D.W. Shoesmith, A Review of Materials and Corrosion Issues Regarding Canisters for Disposal of Spent Fuel and High Level Waste in Opalinus Clay, Nagra, Technical Report NTB-09-02, Wettingen, Switzerland, 2008.
79. B.M. Ikeda, M.G. Bailey, C.F. Clarke, D.W. Shoesmith, Crevice Corrosion and Hydrogen Embrittlement of Titanium Grades-2 and -12 Under Canadian Waste Vault Conditions, Atomic Energy of Canada Limited, Report AECL-10121, Chall River, Canada, 1990.
80. J.J. Noël, D.W. Shoesmith, B.M. Ikeda, Crevice corrosion of alpha titanium alloys, Localized Corrosion, Proceedings of the Corrosion/2001 Research Topical Symposium, Houston, TX, United States, 2001, pp. 65–102.
81. Pan · J. Biomed. Mater. Res. · 1994 · 28 · 11310.1002/jbm.820280115 ↗
82. Pan · J. Biomed. Mater. Res. · 1996 · 30 · 39310.1002/(SICI)1097-4636(199603)30:3<393::AID-JBM14>3.0.CO;2-L ↗
83. Kim · Corrosion · 1987 · 43 · 8510.5006/1.3583122 ↗
84. Kim · Corrosion · 1987 · 43 · 9210.5006/1.3583123 ↗
85. C.F. Baes Jr., R.E. Mesmer, The Hydrolysis of Cations, 1976.
86. Oxide surfaces in solution
87. Grenthe · 1992
88. R. Guillamont, R.T. Fanghanel, I. Grenthe, V. Neck, D. Palmer, M.H. Rand, Update on the chemical thermodynamics of uranium, neptunium, plutonium, americium and technetium, in: Chemical Thermodynamics, Elsevier, Amsterdam, Holland, 2003, pp. 182–187.
89. Jones · J. Chem. Soc. Faraday Trans. · 1977 · 73 · 171010.1039/f19777301710 ↗
90. Pease · J. Chem. Soc. Faraday Trans. · 1986 · 82 · 75910.1039/f19868200759 ↗
91. Hurlen · Electrochim. Acta · 1991 · 36 · 18910.1016/0013-4686(91)85200-Q ↗
92. Blackwood · Electrochim. Acta · 1988 · 33 · 114310.1016/0013-4686(88)80206-8 ↗
93. Macdonald · Pure Appl. Chem. · 1999 · 71 · 95110.1351/pac199971060951 ↗
94. Blackwood · Electrochim. Acta · 1990 · 35 · 107310.1016/0013-4686(90)90045-2 ↗
95. Leitner · J. Electrochem. Soc. · 1986 · 133 · 156110.1149/1.2108969 ↗
96. Fonseca · Corros. Sci. · 2001 · 43 · 54710.1016/S0010-938X(00)00107-4 ↗
97. Hydrogen-induced Cracking of the Drip Shield, Bechtel SAIC Company, ANL-EBS-MD-000006. Rev. 02, Las Vegas, Nevada, 2004.
98. Mattsson · Werkst Korros · 1990 · 41 · 38310.1002/maco.19900410703 ↗
99. E. Smailos, W. Schwarzkopf, R. Koster, Corrosion behavior of container materials for disposal of high-level wastes in rock salt environments, Commission of the European Communities, EUR-10400-EN, Luxemburg, 1986.
100. E. Smailos, R. Koster, Corrosion studies on selected packaging materials for disposal of high level wastes, in: Materials Reliability in the Back End of the Nuclear Fuel Cycle, International Atomic Energy Agency TECDOC-421, Vienna, Austria, 1987, pp. 7–24.