Effect of cold work level on the crack propagation behaviour of 316LN stainless steel in high-temperature pressurized water
Source abstract
Abstract
We investigated the microstructure, mechanical properties, and stress corrosion cracking (SCC) propagation behaviour of 316LN austenitic stainless steel with various cold work (CW) levels. CW increased the crack growth rate of 316LN. The stress corrosion crack growth rate (SCCGR) for 316LN with 5% CW was approximately 6.52% higher than that of the solution-annealed state; 10%, 20%, and 30% CW resulted in 1.20, 3.18, and 6.10 times higher SCCGRs, respectively. A larger residual strain and proliferation of slip bands via cold deformation augmented the SCCGR. The SCC propagation mechanism of 316LN changed with increasing CW levels owing to slip bands.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Féron, 2 - Overview of nuclear materials and nuclear corrosion science and engineering. (2012) 31-56, https://doi.org/10.1533/9780857095343.1.31.10.1533/9780857095343.1.31 ↗
2. Effects of dissolved hydrogen on low-cycle fatigue behaviors and hydrogen uptake of 316LN austenitic stainless steel in simulated pressurized water reactor primary water10.1016/j.ijfatigue.2019.105457 ↗
3. Fatigue model of domestic 316LN steel in simulated primary coolant environment of CAP1400
4. Effects of cold work and stress on oxidation and SCC behavior of stainless steels in PWR primary water environments10.1051/rgn/20111050 ↗
5. A review of stress corrosion cracking of austenitic stainless steels in PWR primary water10.1016/j.jnucmat.2023.154815 ↗
6. Caustic Stress Corrosion of Fe-Cr-Ni Austenitic Alloys10.5006/0010-9312-33.12.425 ↗
7. Effect of Strain Hardened Inner Surface Layers on Stress Corrosion Cracking of Type 316 Stainless Steel in Simulated PWR Primary Water10.1007/s11661-019-05137-9 ↗
8. SCC crack growth rate of cold worked 316L stainless steel in PWR environment10.1016/j.jnucmat.2014.09.054 ↗
9. Cold roiling behaviour and textural evolution in AISI 316L austenitic stainless steel
10. Cold Work and Temperature Dependence of Stress Corrosion Crack Growth of Austenitic Stainless Steels in Hydrogenated and Oxygenated High-Temperature Water
11. Effect of cold work on stress corrosion cracking of non-sensitized AISI stainless steel in high temperature oxygenated water10.5006/1.3582020 ↗
12. Effects of cold working degrees on grain boundary characters and strain concentration at grain boundaries in Alloy 60010.1016/j.corsci.2010.11.022 ↗
13. Microstructural Characterization of SCC Crack Tip and Oxide Film for SUS 316 Stainless Steel in Simulated PWR Primary Water at 320°C10.1080/18811248.2005.9726383 ↗
14. A Potential Anti-oxidation Barrier in Simulated Primary Water10.1016/j.jmst.2014.08.011 ↗
15. Effects of Hydrogen on Stress Corrosion Crack Growth Rate of Nickel Alloys in High-Temperature Water
16. Dependence of Stress Corrosion Cracking for Cold-Worked Stainless Steel on Temperature and Potential, and Role of Diffusion of Vacancies at Crack Tips10.5006/1.3278507 ↗
17. Effect of yield strength on stress corrosion crack propagation under PWR and BWR environments of hardened stainless steels10.1533/9781845693466.3.200 ↗
18. The effect of martensite on stress corrosion crack initiation of austenitic stainless steels in high-temperature hydrogenated water
19. Stress corrosion cracking of fusion boundary for 316L/52M dissimilar metal weld joints in borated and lithiated high temperature water10.1016/j.corsci.2017.01.024 ↗
20. Effect of deformation level and orientation on SCC of 316L stainless steel in simulated light water environments10.1016/j.jnucmat.2020.152038 ↗
21. The effect of roll-processing orientation on stress corrosion cracking of warm-rolled 304L stainless steel in oxygenated and deoxygenated high temperature pure water10.1016/j.corsci.2010.03.027 ↗
22. 2011
23. Multi-scale characterization of stress corrosion cracking of cold-worked stainless steels and the influence of Cr content10.1016/j.actamat.2009.07.040 ↗
24. Stress corrosion cracking of 316L HAZ for 316L stainless steel/Inconel 52M dissimilar metal weld joint in simulated primary water10.1016/j.corsci.2016.07.031 ↗
25. A physical model of the twinning-induced plasticity effect in a high manganese austenitic steel10.1016/j.msea.2004.01.060 ↗
26. Tailoring hydrogen embrittlement resistance of pure Ni by grain boundary engineering10.1016/j.corcom.2022.02.003 ↗
27. Effect of cold deformation on corrosion behavior of selective laser melted 316L stainless steel bipolar plates in a simulated environment for proton exchange membrane fuel cells10.1016/j.corsci.2022.110257 ↗
28. Cold rolling behaviour and textural evolution in AISI 316L austenitic stainless steel10.1016/j.actamat.2005.05.006 ↗
29. Microstructural Characterization of SCC Crack Tip and Oxide Film for SUS 316 Stainless Steel in Simulated PWR Primary Water at 320°C10.1080/18811248.2005.9726383 ↗
30. Multi-scale characterization of stress corrosion cracking of cold-worked stainless steels and the influence of Cr content10.1016/j.actamat.2009.07.040 ↗
31. The effect of cold rolling on grain boundary structure and stress corrosion cracking susceptibility of twins in alloy 690 in simulated PWR primary water environment10.1016/j.corsci.2017.11.002 ↗
32. SCC in PWRs: Learning from a Bottom-Up Approach
33. Degradation of Grain Boundary Strength by Oxidation in Alloy 600
34. The role of cold work and applied stress on surface oxidation of 304 stainless steel10.1016/j.corsci.2011.11.021 ↗
35. Detecting Classical and Martensite-Induced Sensitization Using the Electrochemical Potentiokinetic Reactivation Test10.5006/1.3278194 ↗
36. Stacking fault energies of seven commercial austenitic stainless steels10.1007/BF02641927 ↗
37. A general mechanism of martensitic nucleation: Part I. General concepts and the FCC→HCP transformation10.1007/BF02654987 ↗
38. Hansen · Scr. Mater. · 2004 · 51 · 80110.1016/j.scriptamat.2004.06.002 ↗
39. The dependency of the crack growth rate on the loading pattern and temperature in stress corrosion cracking of strain-hardened 316L stainless steels in a simulated BWR environment10.1016/j.corsci.2007.08.022 ↗
40. Effects of water chemistry and loading conditions on stress corrosion cracking of cold-rolled 316NG stainless steel in high temperature water10.1016/j.corsci.2010.09.018 ↗
41. The effect of roll-processing orientation on stress corrosion cracking of warm-rolled 304L stainless steel in oxygenated and deoxygenated high temperature pure water10.1016/j.corsci.2010.03.027 ↗
42. The role of cold work and applied stress on surface oxidation of 304 stainless steel10.1016/j.corsci.2011.11.021 ↗
43. The influence of surface oxides on the mechanical response of oxidized grain boundaries10.1016/j.tsf.2017.03.060 ↗
44. Investigations on the SCC initiation behavior of cold worked 316 L in high temperature oxygenated water at constant loads10.1016/j.corsci.2022.110336 ↗
45. Electron backscatter diffraction: Strategies for reliable data acquisition and processing10.1016/j.matchar.2009.05.011 ↗
46. Optimization of grain boundary character distribution for intergranular corrosion resistant 304 stainless steel by twin-induced grain boundary engineering10.1016/S1359-6454(02)00064-2 ↗
47. Study of grain boundary character along intergranular stress corrosion crack paths in austenitic alloys10.1016/S1359-6454(01)00064-7 ↗
48. Electron backscatter diffraction: Strategies for reliable data acquisition and processing10.1016/j.matchar.2009.05.011 ↗
49. Low temperature grain boundary diffusion of chromium in SUS316 and 316L stainless steels10.2320/matertrans.45.2945 ↗
50. Stress Corrosion Cracking Growth Rate Behavior of Alloy 22 (UNS N06022) in Concentrated Groundwater[J]
51. IGSCC of non-sensitized stainless steels in high temperature water10.1016/j.jnucmat.2008.08.005 ↗
52. Insights into the SCC crack tip of Alloy 690TT in caustic solution at high temperature10.1016/j.jnucmat.2021.153034 ↗
53. Fundamental modeling of environmental cracking for improved design and lifetime evaluation in BWRs10.1016/0308-0161(94)90142-2 ↗
54. Dependence of crack growth kinetics on dendrite orientation and water chemistry for Alloy 182 weld metal in high-temperature water10.1016/j.jnucmat.2014.12.083 ↗
55. Quantitative prediction of environmentally assisted cracking based on a theoretical model and computer simulation10.1016/S0022-3115(98)00421-8 ↗
56. Elastic plastic fields in steady crack growth in a strain hardening material
57. Effect of cold work on the stress corrosion cracking behavior of Alloy 690 in supercritical water environment10.1016/j.jnucmat.2017.10.003 ↗
58. The effect of residual stress on the Preferential Intergranular Oxidation of Alloy 60010.1016/j.corsci.2016.05.022 ↗
59. Marc. Mechanical Behavior of Materials (2nd ed.)10.1108/aeat.2009.12781bae.001 ↗
60. Life prediction by mechanistic modeling and system monitoring of environmental cracking of iron and nickel alloys in aqueous systems10.1016/0025-5416(88)90564-2 ↗
61. The influence of surface oxides on the mechanical response of oxidized grain boundaries10.1016/j.tsf.2017.03.060 ↗
62. The role of surface deformation in the oxidation response of type 304 SS in high temperature deaerated water10.1016/j.corsci.2018.06.033 ↗