Stress-induced reorientation of hydrides in Zr-1Nb-0.01Cu cladding tube studied by synchrotron X-ray diffraction and EBSD

Shengjie Wang, Shilei Li, Runguang Li, Xinxing Zhang, Youkang Wang, Fei Xue, Guanghai Bai, Yan-Dong Wang

Abstract

Abstract High-energy X-ray diffraction and electron backscatter diffraction techniques were employed to investigate the hydride precipitation in Zr-1Nb-0.01Cu cladding tube under different internal pressures up to 30 MPa. Hydride reorientation occurs when the internal pressure exceeds 10 MPa. Higher internal pressure applied to the cladding tube induced plastic deformation, which significantly increases the nucleation sites of the δ-hydrides. The different evolutions of the (111) d -spacing with the azimuth angles indicated that the δ-hydrides precipitated from the cladding tubes under different internal pressures possessed different residual stress fields. Detail analysis of stereo-graphic projections confirmed that both the circumferential and radial δ-hydrides precipitated under different internal pressures followed the {0001}α-Zr // {111}δ-hydride and 2 ¯ 0>α-Zr // δ-hydride orientation relationship with their parent α-Zr matrix. The δ-hydride {111} 2 ¯ > twins may form when the Shockley partial dislocations glide on the alternate close-packed (0001) basal planes and the alternating distribution of δ-hydride twins may result in a deflection of hydride packet. The δ-hydride precipitates along the radial direction of the cladding tube under internal pressure is more adaptable to the volume expansion induced by phase transformation.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. The development and applications of zirconium alloys10.1016/0261-3069(85)90165-7 ↗
2. A review on hydride precipitation in zirconium alloys10.1016/j.jnucmat.2015.07.014 ↗
3. Kinetics of hydrogen absorption and release in zirconium alloys during steam oxidation10.1007/s11085-008-9113-2 ↗
4. The terminal solid solubility of hydrogen in irradiated Zircaloy-2 and microscopic modeling of hydride behavior10.1016/j.jnucmat.2009.01.017 ↗
5. Hydrogen in Zircaloy: mechanism and its impacts10.1016/j.ijhydene.2015.03.049 ↗
6. Effects of applied load on formation and reorientation of zirconium hydrides: a multiphase field modeling study10.1016/j.commatsci.2021.110367 ↗
7. Delayed hydride cracking of Zr-2.5%Nb pressure tube material due to partially constrained precipitates10.1016/j.jnucmat.2018.10.040 ↗
8. Observation of the δ to ε Zr-hydride transition by in-situ synchrotron X-ray diffraction10.1002/crat.201600234 ↗
9. Investigation of mechanical properties of ε-zirconium hydride using micro- and nano-indentation techniques10.1016/j.jnucmat.2004.02.004 ↗
10. The precipitation of γ-hydride plates in zirconium10.1016/0001-6160(81)90074-2 ↗
11. Characterizing the crystal structure and formation induced plasticity of γ-hydride phase in zirconium10.1016/j.mtla.2019.100454 ↗
12. Identification and characterization of a new zirconium hydride10.1111/j.1365-2818.2008.02136.x ↗
13. Investigations of deformation-induced δ → ζ phase transformation in zirconium hydride by in situ high-energy X-ray diffraction10.1016/j.actamat.2017.08.047 ↗
14. Effect of radial hydrides on the axial and hoop mechanical properties of Zircaloy-4 cladding10.1016/j.jnucmat.2006.11.008 ↗
15. Cooling rate- and hydrogen content-dependent hydride reorientation and mechanical property degradation of Zr–Nb alloy claddings10.1016/j.jnucmat.2013.06.006 ↗
16. Stress and temperature-dependent hydride reorientation of Zircaloy-4 cladding and its effect on the ductility degradation10.1080/00223131.2014.978829 ↗
17. The effect of neutron irradiation on hydride reorientation and mechanical property degradation of zirconium alloy cladding10.1016/j.net.2017.05.006 ↗
18. Hydride precipitation by cathodic hydrogen charging method in zirconium alloys10.1016/j.matchemphys.2007.12.028 ↗
19. EBSD studies on microstructure and crystallographic orientation of δ-hydrides in Zircaloy-4, Zr–1% Nb and Zr–2.5% Nb10.1016/j.msea.2011.05.022 ↗
20. Hydride reorientation in Zircaloy-4 cladding10.1016/j.jnucmat.2007.06.012 ↗
21. A study on hydride reorientation of Zircaloy-4 cladding tube under stress10.1016/j.jnucmat.2014.09.032 ↗
22. Cooling rate and hydrogen content-dependent hydride reorientation and mechanical property degradation of Zr–Nb alloy claddings10.1016/j.jnucmat.2013.06.006 ↗
23. The effect of hydrogen and oxygen contents on hydride reorientations of zirconium alloy cladding tubes10.1016/j.net.2015.06.004 ↗
24. Effect of texture, grain size, and cold work on the precipitation of oriented hydrides in Zircaloy tubing and plate10.1016/0022-3115(66)90036-5 ↗
25. Microstructural and crystallographic analysis of hydride reorientation in a zirconium alloy cladding tube10.1016/j.jnucmat.2020.152232 ↗
26. In situ high-energy X-ray diffraction mapping of Lüders band propagation in medium-Mn transformation-induced plasticity steels10.1080/21663831.2018.1530698 ↗
27. Identification and quantification of hydride phases in Zircaloy-4 cladding using synchrotron X-ray diffraction10.1016/j.jnucmat.2009.04.004 ↗
28. Synchrotron X-ray diffraction study of zirconium hydride distribution in Zr-2.5%Nb and its redistribution during thermal cycling10.1016/j.matchar.2017.12.012 ↗
29. Hydride reorientation in Zr2.5Nb studied by synchrotron X-ray diffraction10.1016/j.actamat.2012.07.029 ↗
30. Mechanisms of hydride reorientation in Zircaloy-4 studied in-situ
31. Hydride platelet reorientation in Zircaloy studied with synchrotron radiation diffraction10.1520/JAI103033 ↗
32. Hydride reorientation in Zircaloy-4 examined by in situ synchrotron X-ray diffraction10.1016/j.jnucmat.2016.05.029 ↗
33. Effect of thermo-mechanical cycling on zirconium hydride reorientation studied in situ with synchrotron X-ray diffraction10.1016/j.jnucmat.2013.04.047 ↗
34. Hydrogen in zirconium alloys: a review10.1016/j.jnucmat.2019.02.042 ↗
35. Tensile hoop stress-, hydrogen content- and cooling rate-dependent hydride reorientation behaviors of Zr alloy cladding tubes10.1016/j.jnucmat.2015.04.027 ↗
36. The precipitation of γ-zirconium hydride in zirconium10.1016/0001-6160(78)90006-8 ↗
37. The dilatational misfit of zirconium hydrides precipitated in zirconium10.1016/0022-3115(73)90022-6 ↗
38. Hydride precipitation and stresses in Zircaloy-4 observed by synchrotron X-ray diffraction10.1016/j.actamat.2010.08.022 ↗
39. Microscopic stress and crystallographic orientation of hydrides precipitated in Zr-1Nb-0.01Cu cladding tube investigated by high-energy X-ray diffraction and EBSD10.1016/j.jnucmat.2020.152534 ↗
40. Microstructure and formation mechanisms of δ-hydrides in variable grain size Zircaloy-4 studied by electron backscatter diffraction10.1016/j.actamat.2019.02.042 ↗
41. Hydride precipitation in α/β zirconium alloys10.1016/0001-6160(83)90008-1 ↗
42. Autocatalytic nucleation and elastic stabilization of linear arrays of plate-shaped precipitates10.1016/0001-6160(81)90131-0 ↗
43. Intergranular δ-hydride nucleation and orientation in zirconium alloys10.1016/j.actamat.2011.07.054 ↗
44. The role of chemical free energy and elastic strain in the nucleation of zirconium hydride10.1016/j.jnucmat.2013.06.013 ↗
45. The long-range migration of hydrogen through Zircaloy in response to tensile and compressive stress gradients
46. Multidimensional simulations of hydrides during fuel rod lifecycle10.1016/j.jnucmat.2015.06.037 ↗
47. Effects of applied load on formation and reorientation of zirconium hydrides: a multiphase field modeling study10.1016/j.commatsci.2021.110367 ↗
48. The phase field model for hydrogen diffusion and γ-hydride precipitation in zirconium under non-uniformly applied stress10.1016/j.mechmat.2005.05.005 ↗