Abstract

One of the most critical issues affecting the integrity of nuclear fuel cladding tubes is hoop stress-induced hydride reorientation from the circumferential to the radial direction. The theoretical prediction of the threshold stress for the hydride reorientation is a long-standing but unrealized objective of material-design engineers in the nuclear industry. In this paper, we propose a criterion to determine the threshold stress based on the thermodynamic model. The results obtained this way agree very well with experimental observations. Multiple factors, such as crystallographic texture, grain-boundary structure and distribution, grain morphology and size, the hydride-matrix misfit strain, hydrogen content, the chemical composition, the temperature and the mechanical strength and anisotropy of the zirconium matrix, simultaneously control the difficulty level of hydride reorientation. Strengthening only the radial basal pole texture of the zirconium alloy tube is not enough to effectively enhance the threshold stress of hydride reorientation; other factors, especially the grain-boundary structure and distribution, also need to be considered. The model presented in this study elucidates the mechanism of stress reorientation of hydrides and offers new insight on how to further increase the resistance to hoop stress-induced hydride reorientation in nuclear fuel cladding tubes
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (55)

Show source-provided references
1. Puls · 2012
2. Brittle nature and the related effects of zirconium hydrides in Zircaloy-410.1016/j.msea.2019.138396 ↗
3. Effect of hydrogenation conditions on the microstructure and mechanical properties of zirconium hydride10.1016/j.jnucmat.2017.12.027 ↗
4. Identifying the true structure and origin of the water-quench induced hydride phase in Zr-2.5Nb alloy10.1016/j.actamat.2021.117369 ↗
5. 1983 Hydride precipitation in α/β zirconium alloys10.1016/0001-6160(83)90008-1 ↗
6. M.P. Puls, Hydrogen-induced delayed cracking: 2. Effect of stress on nucleation, growth and coarsening of zirconium hydride precipitates, Atomic Energy of Canada Limited Report, AECL-8381, Atomic Energy of Canada, Mississauga, Ontario, 1984.
7. EBSD studies on microstructure and crystallographic orientation of delta-hydrides in Zircaloy-4, Zr-1% Nb and Zr-2.5% Nb10.1016/j.msea.2011.05.022 ↗
8. Phase and texture analysis of a hydride blister in a Zr-2.5%Nb tube by synchrotron X-ray diffraction10.1016/j.actamat.2010.12.024 ↗
9. The precipitation of γ-hydride plates in zirconium10.1016/0001-6160(81)90074-2 ↗
10. Hydride reorientation in Zr2.5Nb studied by synchrotron X-ray diffraction10.1016/j.actamat.2012.07.029 ↗
11. Phase-field modeling of stacking structure formation and transition of δ-hydride precipitates in zirconium10.1016/j.actamat.2018.12.009 ↗
12. Hydride reorientation in Zircaloy-4 cladding10.1016/j.jnucmat.2007.06.012 ↗
13. Stress-reorientation of hydrides and hydride embrittlement10.1016/j.jnucmat.2003.10.009 ↗
14. Influence of temperature on threshold stress for reorientation of hydrides and residual stress variation across thickness of Zr-2.5Nb alloy pressure tube10.1016/j.jnucmat.2006.09.004 ↗
15. Effect of texture, grain size, and cold work on the precipitation of oriented hydrides in Zircaloy tubing and plate10.1016/0022-3115(66)90036-5 ↗
16. Stress reorientation of hydrides in zirconium−2.5% niobium10.1016/0022-3115(75)90132-4 ↗
17. Hydrogen in Zircaloy: mechanism and its impacts10.1016/j.ijhydene.2015.03.049 ↗
18. The effect of stress on orientation of hydrides in zirconium alloy pressure tube materials10.1179/cmq.1985.24.3.235 ↗
19. A study on hydride reorientation of Zircaloy-4 cladding tube under stress10.1016/j.jnucmat.2014.09.032 ↗
20. Understanding hydride- and hydrogen-related processes in high-burnup cladding in spent-fuel-storage and accident situations
21. Stress Reorientation of hydrides in recrystallized Zircaloy-2 sheet10.1080/18811248.2006.9711205 ↗
22. A study on the effects of hydrogen content and peak temperature on threshold stress for hydride reorientation in Zircaloy-4 cladding10.1016/j.jnucmat.2018.07.005 ↗
23. Hydrogen in zirconium alloys: a review10.1016/j.jnucmat.2019.02.042 ↗
24. Formation path of δ hydrides in zirconium by multiphase field modeling10.1016/j.actamat.2016.10.056 ↗
25. Hydride-induced degradation of hoop ductility in textured zirconium-alloy tubes: a theoretical analysis10.1016/j.actamat.2012.06.003 ↗
26. The stress orientation of hydride in zirconium alloys10.1016/0022-3115(70)90214-X ↗
27. The nucleation of hydrides in a Zr-2.5 wt% Nb alloy10.1016/0022-3115(84)90086-2 ↗
28. Intergranular δ-hydride nucleation and orientation in zirconium alloys10.1016/j.actamat.2011.07.054 ↗
29. Crystallography of zirconium hydrides in recrystallized zircaloy-2 fuel cladding by electron backscatter diffraction10.1080/18811248.2004.9715540 ↗
30. C.E. Ells, C.J. Simpson, Hydrogen in Metals, in: I.M. Bernstein, A.W. Thompson (Eds.), A.S.M., Metals Park, 1974, pp. 345-366.
31. Solubility of hydrogen isotopes in stressed hydride-forming metals10.1016/0036-9748(83)90074-1 ↗
32. Identification and characterization of a new zirconium hydride10.1111/j.1365-2818.2008.02136.x ↗
33. Plastic relaxation of the transformation strain energy of a misfitting spherical precipitate: Ideal plastic behavior10.1007/BF02655099 ↗
34. The effect of metallurgical factors on hydride phases in zirconium10.1016/0022-3115(84)90029-1 ↗
35. Kiran Kumar · 2011
36. The dilatational misfit of zirconium hydrides precipitated in zirconium10.1016/0022-3115(73)90022-6 ↗
37. Temperature dependence of misfit strains of δ-hydrides of zirconium10.1016/j.jallcom.2006.07.049 ↗
38. Lloyd · 1963
39. Thermal and mechanical properties of zirconium hydride10.1016/S0925-8388(99)00389-8 ↗
40. Elastic constants of zirconium alloys10.1016/0022-3115(75)90071-9 ↗
41. Effects of crack tip stress states and hydride-matrix interaction stresses on delayed hydride cracking10.1007/BF02647211 ↗
42. δ-hydride habit plane determination in α-Zirconium at 298 K by strain energy minimization technique10.4028/www.scientific.net/DDF.279.105 ↗
43. The values of the coherent and the incoherent interfacial energies of hydride formation in the Zr matrix are not available in the literature. We assume σαδ,⊥c = 0.1 J/m2 for δ-hydride formation on the prism (1010α) plane (typical of the coherent interface). Considering that coherent interfacial energy depends on the extent of coherent strain at the interface [44], and χ decreases with the relationships changing from 1010α//111δ, 1011α//111δ, 1013α//111δ, 1017α//111δ to 0001α//111δ, the coherent interfacial energies for hydride formation on 1011α, 1013α, 1017α and 0001α are, respectively, assumed to be 0.09 J/m2, 0.08 J/m2, 0.07 J/m2 and 0.06 J/m2. For incoherent interfacial energies, we take σαδ,⊥=σαδ,//= 1 J/m2 (typical of the incoherent interfaces).
44. Theoretical study of interface structure and energetics in semicoherent Fe(001)ÕMX(001) systems (M=Sc, Ti, V, Cr, Zr, Nb, Hf, Ta; X=C or N)10.1103/PhysRevB.82.195410 ↗
45. Dilation of h.c.p. zirconium by interstitial deuterium10.1016/0001-6160(85)90098-7 ↗
46. Hydride embrittlement in ZIRCALOY-4 plate: part II. interaction between the tensile stress and the hydride morphology10.1007/BF02652294 ↗
47. Anisotropic behavior and rupture of hydride ZIRCALOY-4 sheets10.1007/s11661-000-0010-9 ↗
48. Environmentally-induced cracking of zirconium alloys - a review10.1016/0022-3115(90)90321-D ↗
49. Crystallography of zirconium hydrides in recrystallized Zircaloy-2 fuel cladding by electron backscatter diffraction10.1080/18811248.2004.9715540 ↗
50. Accommodation of misfit across the interface between crystals of semiconducting elements or compounds10.1063/1.1659510 ↗
51. Hydride embrittlement in ZIRCALOY-4 plate: part I. Influence of microstructure on the hydride embrittlement in ZIRCALOY-4 at 20°C and 350°C10.1007/BF02652293 ↗
52. Resistance to hydride formation in zirconium: an emerging possibility10.1016/j.actamat.2006.06.004 ↗
53. A review of factors influencing the hydride reorientation phenomena in zirconium alloy cladding during long-term dry storage
54. Effect of microstructure factors and cold work on the hydride precipitation in Zircaloy-4 sheet10.2978/jsas.3.188 ↗
55. The role of crystallographic orientations on heterogeneous deformation in a zirconium alloy: A combined experimental and modeling study10.1016/j.ijplas.2020.102785 ↗