Effect of temperature and hydrogen concentration on the threshold stress intensity factor of radial delayed hydride cracking in fuel cladding
Source abstract
Abstract
Three-point bending tests provide the ability to measure the propagation of axially oriented cracks in thin-walled fuel cladding in a radial outside-in direction. Via three-point bending, unirradiated Zircaloy-2 cladding containing 155 and 305 wppm hydrogen was mechanically loaded at different temperatures, sufficient to initiate delayed hydride cracking (DHC) whereupon the unloading rate was fast enough to arrest further propagation. The crack front dimensions were measured through fractography and implemented with the final load into a finite element model (FEM). Given the average crack length and final load, the FEM was able to back-calculate the stress intensity factor. Over a temperature range of 210–330 °C, around 6 MPa√m was calculated as the minimum threshold stress intensity factor for DHC. The trend shows that the ideal temperature for DHC with lowest threshold stress intensity factors may depend on the hydrogen concentration, and that the threshold stress intensity factors quickly increase with higher test temperatures. It has also been shown that creep affects the threshold stress intensity factor for optimal DHC less for lower hydrogen concentrations than for higher hydrogen concentrations. At low hydrogen concentration, the temperature of terminal solid solubility for precipitation (TSSP) is low enough so that creep-induced crack tip rounding plays a less significant role compared to the hydrogen kinetics.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. International Atomic Energy Agency, “Waterside corrosion of zirconium alloys in nuclear power plants,” IAEA-TECDOC-996, 1998, doi: IAEA-TECDOC-996.
2. Hydrogen diffusion and precipitation in duplex zirconium nuclear fuel cladding quantified by high-resolution neutron imaging10.1016/j.jnucmat.2019.151757 ↗
3. Hydride reorientation and delayed hydride cracking of spent fuel rods in dry storage10.1007/s11661-009-0044-6 ↗
4. Hydrogen in Zircaloy: mechanism and its impacts10.1016/j.ijhydene.2015.03.049 ↗
5. Puls · 2012
6. The hydrogen embrittlement of zirconium in slow-bend tests10.1016/0022-3115(66)90123-1 ↗
7. The influence of the matrix on the hydrogen embrittlement of zirconium in bend tests10.1016/0022-3115(72)90082-7 ↗
8. The first step for delayed hydride cracking in zirconium alloys10.1016/j.jnucmat.2009.08.019 ↗
9. Mechanisms of hydrogen induced delayed cracking in hydride forming materials10.1007/BF02644858 ↗
10. Hydrides and delayed hydrogen cracking in zirconium and its alloys10.1179/imr.1983.28.1.92 ↗
11. Stage I and II behaviors of delayed hydride cracking velocity in zirconium alloys10.1016/j.jallcom.2006.11.197 ↗
12. IAEA - International Atomic Energy Agency, “Delayed hydride cracking in zirconium alloys in pressure tube nuclear reactors IAEA-TECDOC-1410,” October, no. October, p. 43, 2004.
13. Crack growth in the through-thickness direction of hydrided thin-wall Zircaloy sheet10.1016/j.jnucmat.2011.09.005 ↗
14. The effects of stress, temperature and hydrogen content on hydride-induced crack growth in Zr-2.5 Pct Nb10.1007/BF02811655 ↗
15. Delayed hydride cracking in Zr-2.5Nb tube with the cooling rate and the notch tip shape10.1016/j.jnucmat.2004.07.046 ↗
16. Delayed hydrogen embrittlement in Zr-2.5 wt% Nb10.1016/0022-3115(74)90174-3 ↗
17. Hydrogen diffusion under stress in Zircaloy: high-resolution neutron radiography and finite element modeling10.1016/j.jnucmat.2018.05.079 ↗
18. Delayed hydride cracking in Zircaloy-2 with and without liner at various temperatures investigated by high-resolution neutron radiography10.1016/j.jnucmat.2022.153549 ↗
19. Multi-physics modeling of delayed hydride cracking in zirconium alloys10.1016/j.jmps.2019.07.020 ↗
20. Threshold stress intensity factor of delayed hydride cracking in irradiated and unirradiated zircaloy-4 cladding10.1016/j.jnucmat.2020.152596 ↗
21. On the effect of temperature on the threshold stress intensity factor of delayed hydride cracking in light water reactor fuel cladding10.1016/j.net.2017.04.002 ↗
22. Analysis of stresses and strains near the end of a crack traversing a plate’10.1115/1.4011547 ↗
23. Evaluation of Conditions for Hydrogen Induced Degradation of Zirconium Alloys during Fuel Operation and Storage
24. Evaluation of a delayed hydride cracking in Zr-2.5Nb CANDU and RBMK pressure tubes10.1016/j.matdes.2008.06.011 ↗
25. The issue of stress state during mechanical tests to assess cladding performance during a reactivity-initiated accident (RIA)10.1016/j.jnucmat.2011.03.015 ↗
26. Post-test examinations on Zr-1%Nb claddings after ballooning and burst, high-temperature oxidation and secondary hydriding10.1016/j.jnucmat.2018.05.072 ↗
27. Supercharging of zircaloy-410.1016/S0022-3115(97)00147-5 ↗
28. Standard test method for measurement of fracture toughness
29. Dissolution and precipitation behavior of hydrides in Zircaloy-2 and high Fe Zircaloy10.1016/S0022-3115(03)00320-9 ↗
30. SHORT NOTE terminal solid solubility of hydrogen in unalloyed zirconium by differential scanning calorimetry
31. The terminal solid solubility of hydrogen in irradiated Zircaloy-2 and microscopic modeling of hydride behavior10.1016/j.jnucmat.2009.01.017 ↗
32. (ASTM D 5054) - standard test methods for plane-strain fracture toughness and strain energy release rate of plastic materials
33. Bower · 2010
34. Standard test method for linear-elastic plane-strain fracture toughness K Ic of
35. Measurements of delayed hydride cracking propagation rate in the radial direction of Zircaloy-2 cladding tubes10.1016/j.jnucmat.2012.04.012 ↗
36. Yielding of steel sheets containing slits10.1016/0022-5096(60)90013-2 ↗