journal article·2023-04

The transformation of fretting corrosion mechanism of zirconium alloy tube mating with 304 stainless steel in high temperature high pressure water

Wenhua Zhuang, Ping Lai, Hui Lu, Zhongli Han, Junqiang Lu, Lefu Zhang, Libing Zhu, Xianglong Guo

Publisher page

Abstract

Studying the fretting wear mechanism of zirconium alloy in high temperature high pressure water is of great importance for understanding the failure behavior of fuel assembly. In this work, the tangential fretting wear of zirconium alloy tube at different displacement amplitudes (40 µm and 80 µm) and normal forces (6 N and 12 N) was investigated in high temperature high pressure water. The results show that the wear depth and wear volume of zirconium alloy tested at 6 N-80 µm are the highest among all the tests. When the testing condition is 6 N-80 µm, the fretting is located in the gross slip regime. Oxidation and abrasive wear dominate the fretting wear behavior. The increase in normal force and decrease in displacement reduces the relative sliding distance between the contact interfaces, which reduces the ejection of wear debris and changes the wear mechanism. When the test conditions are 6 N-40 µm and 12 N-40 µm, the fretting regime is located in the partial slip regime, and the dominant wear mechanisms are adhesive wear and oxidation. Under the synergistic effect of mechanical wear and high-temperature water corrosion, a dual-layer structure oxide scale is formed on the worn area. The mixed oxide layer with loose and porous structure is formed by the accumulation of granular wear debris, while the dense inner oxide layer is mainly formed by oxidation of the matrix alloy. Fretting wear accelerates material corrosion by wear debris refinement and cracking. The integrity of the oxide layer is negatively correlated with its thickness. As the thickness of the oxide layer increases, more cracks can be observed in the oxide layer.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Mechanical stress and fatigue analysis · Nuclear Materials and Properties · Cardiac Structural Anomalies and Repair

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Mechanical and experimental investigation on nuclear fuel fretting10.1016/j.triboint.2006.02.027 ↗
2. Materials challenges in nuclear energy10.1016/j.actamat.2012.11.004 ↗
3. Phase transformations during cooling from the βZr phase temperature domain in several hydrogen-enriched zirconium alloys studied by in situ and ex situ neutron diffraction10.1016/j.actamat.2020.08.061 ↗
4. In-situ electrochemical study of zirconium alloy in high temperature hydrogenated Water conditions10.1016/j.corsci.2020.108745 ↗
5. Oxidation kinetics of Cr-coated zirconium alloy: effect of coating thickness and microstructure10.1016/j.corsci.2020.108883 ↗
6. Arc welding of zirconium and its alloys: a review10.1016/j.pnucene.2021.103630 ↗
7. 2019
8. A review of fretting study on nuclear power equipment10.1016/j.triboint.2019.106095 ↗
9. Sliding wear and friction behavior of zirconium alloy with heat-treated Inconel 71810.1016/j.nucengdes.2013.08.008 ↗
10. Standard test method for damage to contacting solid surfaces under fretting conditions. ASTM G204-15. 2022.
11. On the fretting wear mechanism of Zr-alloys10.1016/j.triboint.2006.02.053 ↗
12. A comparative study on the wear behaviors of cladding candidates for accident-tolerant fuel10.1016/j.jnucmat.2015.05.017 ↗
13. Study on the fretting maps of Zircaloy-4 alloy against Inconel 718 alloy10.1016/j.triboint.2021.107024 ↗
14. Comparative study on rod fretting behavior of different spacer spring geometries10.1016/j.wear.2008.06.010 ↗
15. Influence of contact shape and supporting condition on tube fretting wear10.1016/S0043-1648(03)00068-1 ↗
16. Influence of nanoparticle additions on structure and fretting corrosion behavior of micro-arc oxidation coatings on zirconium alloy10.1016/j.surfcoat.2021.126949 ↗
17. Investigating grid-to-rod fretting wear of nuclear fuel claddings using a unique autoclave fretting rig
18. Autoclave grid-to-rod fretting wear evaluation of a candidate cladding coating for accident-tolerant fuel10.1016/j.wear.2020.203578 ↗
19. Fretting wear behavior of zirconium alloy in B-Li water at 300 °C10.1016/j.jnucmat.2017.12.003 ↗
20. Effect of micro-arc oxidation on fretting wear behavior of zirconium alloy exposed to high temperature water
21. Role of ZrO2 oxide layer on the fretting wear resistance of a nuclear fuel rod
22. A microstructure-based wear model for grid-to-rod fretting of clad nuclear fuel rods10.1016/j.wear.2019.01.056 ↗
23. On the mechanisms of various fretting wear modes10.1016/j.triboint.2011.02.010 ↗
24. Cracking behavior of various aluminium alloys during fretting10.1016/0043-1648(92)90091-L ↗
25. Frequency effects in fretting wear10.1016/0043-1648(86)90149-3 ↗
26. Sliding wear and friction behaviour of zircaloy-4 in water10.1016/j.jnucmat.2009.09.001 ↗
27. Modification methodology of fretting wear in involute spline10.1016/j.wear.2016.10.015 ↗
28. A stress based damage mechanics model to simulate fretting wear of Hertzian line contact in partial slip10.1016/j.wear.2013.08.008 ↗
29. Characterization and simulation methods applied to the study of fretting wear in Zircaloy-410.1016/j.wear.2018.01.012 ↗
30. Effects of amplitude and frequency on the wear mode change of Inconel 690 SG tube mated with SUS 40910.1016/j.wear.2014.02.019 ↗
32. A study on wear coefficients and mechanisms of steam generator tube materials10.1016/S0043-1648(01)00680-9 ↗
33. Progress in fretting maps10.1016/j.triboint.2006.02.001 ↗
34. Fretting debris and delamination theory of wear10.1016/0043-1648(74)90019-2 ↗
35. Introduction of a new sliding regime criterion to quantify partial, mixed and gross slip fretting regimes: correlation with wear and cracking processes10.1016/j.wear.2010.05.002 ↗
36. Understanding the fretting corrosion mechanism of zirconium alloy exposed to high temperature high pressure water10.1016/j.corsci.2022.110300 ↗
37. Effect of test conditions on the temperature at which a protective debris bed is formed in fretting of a high strength steel10.1016/j.wear.2017.01.057 ↗
38. The effect of rapidly varying contact stress fields on fretting fatigue10.1016/S0142-1123(01)00191-8 ↗
39. In situ observation of wear particle formation on lubricated sliding surfaces10.1016/j.actamat.2011.09.046 ↗
40. Effect of microstructure on corrosion behavior of a Zr-Sn-Nb-Fe-Cu-O alloy10.1016/j.matdes.2015.12.067 ↗
41. The role of alloying elements in the initiation of nanoscale porosity in oxide films formed on zirconium alloys10.1016/j.corsci.2013.08.006 ↗
42. G Sele U. Influence of surface diffusion on the formation of hollow nanostructures induced by the Kirkendall effect: the basic concept10.1021/nl070026p ↗
43. The effect of Sn concentration on oxide texture and microstructure formation in zirconium alloys10.1016/j.actamat.2015.08.005 ↗
44. A study of the stresses generated in zirconia films during the oxidation of zirconium alloys10.1007/BF00614620 ↗
45. Corrosion mechanisms of candidate structural materials for supercritical water-cooled reactor10.1007/s11708-009-0024-y ↗
46. Microstructure evolution of oxide films formed on Zircaloy-4 during autoclave tests
47. Focussed ion beam sectioning for the 3D characterisation of cracking in oxide scales formed on commercial ZIRLO (TM) alloys during corrosion in high temperature pressurised water10.1016/j.corsci.2011.08.013 ↗
48. Finite element analysis of Hertz contact problem with friction10.1016/0168-874X(87)90032-1 ↗
49. Analysis of the slipping contact between a cylinder and a plane on the base of Hertz theory
50. Review of stress fields in zirconium alloys corrosion scales10.1016/j.corsci.2015.03.004 ↗