Comparison of the corrosion behavior of four Fe-Cr-Ni austenitic alloys in supercritical water
Source abstract
Abstract
The corrosion behavior of four Fe-Cr-Ni austenitic alloys were investigated after exposure to deaerated supercritical water (SCW) at 650°C. Results show that the corrosion resistance follows the trend:Fe-29Cr-61Ni > Fe-16Cr-75Ni > Fe-25Cr-20Ni > Fe-21Cr-31Ni. The increase in Cr and Ni contents promote a transition from low-protective multilayer oxide scales to protective Cr 2O 3 scales. After surface grinding, the weight gains of all specimens dropped by one order of magnitude. Surface grinding induces the formation of ultrafine grains and a high density of dislocations, which enhances the corrosion resistance among all studied austenitic alloys. However, the beneficial effects of grinding diminish with increased Cr and Ni contents due to the pre-existing portion of Cr 2O 3 scales. The lower critical Cr content required to form Cr 2O 3 scales in high Ni austenitic alloys is primarily attributed to their lower solubility of O and the slower diffusion rates of Ni, which inhibit corrosion behavior.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. Supercritical water-cooled reactor materials – summary of research and open issues10.1016/j.pnucene.2014.02.008 ↗
2. Materials for future nuclear energy systems10.1016/j.jnucmat.2019.151837 ↗
3. Corrosion of austenitic alloys in supercritical water10.5006/1.3278237 ↗
4. Characteristics of oxidation and oxygen penetration of alloy 690 in 600°C aerated supercritical water10.1016/j.jmst.2016.11.001 ↗
5. Corrosion behavior of Alloy 690 in aerated supercritical water10.1016/j.corsci.2012.10.001 ↗
6. Corrosion of engineering materials in a supercritical water cooled reactor: Characterization of oxide scales on Alloy 800H and stainless steel 31610.1016/j.corsci.2015.07.035 ↗
7. Corrosion characteristics and mechanisms of typical Ni-based corrosion-resistant alloys in sub- and supercritical water10.1016/j.supflu.2020.105138 ↗
8. Corrosion resistance of candidate cladding materials for supercritical water reactor10.1016/j.anucene.2018.12.007 ↗
9. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
10. The effects of grain boundary structure and bulk Cr content on grain boundary degradation behavior of Ni-Cr binary alloys in high temperature CO210.1016/j.actamat.2023.119496 ↗
11. Predicting the transition from internal to external oxidation of alloys using an extended Wagner model10.1016/j.crme.2013.01.003 ↗
12. Reaktionstypen bei der Oxydation von Legierungen, Z. Für Elektrochem
13. Young · 2016
14. Diffusion of iron in Cr2O3: polycrystals and thin films10.1016/j.msea.2004.09.033 ↗
15. Diffusion of nickel in single- and polycrystalline Cr2O310.1080/14786430701848046 ↗
16. Corrosion mechanisms of 316L stainless steel in supercritical water: The significant effect of work hardening induced by surface finishes10.1016/j.corsci.2019.05.014 ↗
17. Effect of shot-peening on the oxidation of alloy 800H exposed to supercritical water and cyclic oxidation10.1016/j.corsci.2008.04.008 ↗
18. Effect of surface modification on the corrosion resistance of austenitic stainless steel 316L in supercritical water conditions10.1016/j.supflu.2013.05.002 ↗
19. Surface characterization of austenitic stainless steel 304L after different grinding operations10.1186/s40712-017-0074-6 ↗
20. Grain boundary oxidation in iron-based alloys, investigated by 18O enriched water vapour–The effect of mixed oxides in binary and ternary Fe–{Al, Cr, Mn, Si} systems10.1016/j.corsci.2015.04.009 ↗
21. Understanding the surface oxide evolution of T91 ferritic-martensitic steel in supercritical water through advanced characterization10.1016/j.actamat.2020.05.016 ↗
22. Revealing the oxidation mechanism of 310S stainless steel in supercritical water via high-resolution characterization10.1016/j.corsci.2022.110212 ↗
23. Oxide scale growth behavior of alumina-forming austenitic stainless steel exposed to supercritical water10.1016/j.corsci.2023.111681 ↗
24. Investigation on the corrosion behavior of Alloy 800H at various levels of deformation10.1016/j.corsci.2022.110926 ↗
25. A novel strategy to fabricate thin 316L stainless steel rods by continuous directed energy deposition in Z direction
26. Time-dependent power laws in the oxidation and corrosion of metals and alloys10.1038/s41598-022-10748-1 ↗
27. Quantitative Approach for Determining the Critical Volume Fraction for the Transition from Internal to External Oxidation10.1007/s11085-014-9516-1 ↗
28. Corrosion behavior of alloy 800H (Fe–21Cr–32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
29. Investigation on the corrosion behavior of Alloy 800H at various levels of deformation10.1016/j.corsci.2022.110926 ↗
30. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe–Cr and Fe–Cr–X alloys10.1007/s11085-010-9215-5 ↗
31. Internal-external transition for the oxidation of Fe-Cr-Ni austenitic stainless steels in steam10.1007/BF00665267 ↗
32. Diffusion of oxygen in nickel: A variable charge molecular dynamics study10.1016/j.ssc.2009.12.012 ↗
33. Börnstein · Cryst. Res. Technol. · 1982 · 1710.1002/crat.2170170310 ↗
34. Characterization of dealloying and associated stress corrosion cracking: The effect of crystallographic orientation
35. Selective oxidation and nickel enrichment hinders the repassivation kinetics of multi-principal element alloy surfaces
36. Oxygen solubility in austenitic Fe-Ni alloys at high temperatures10.1016/j.jallcom.2017.10.226 ↗
37. Internal oxidation of austenitic Fe-Ni-Cr alloys at high temperatures: Deduction of oxygen permeability and the influence of carbon-bearing gases10.1016/j.corsci.2023.111465 ↗
38. Thermodynamic modelling of the Cr–Fe–Ni–O system10.1016/j.calphad.2008.04.005 ↗
39. The influence of metal lattice vacancies on the oxidation of high temperature materials10.1016/0010-938X(77)90004-X ↗
40. The role of metal lattice vacancies in the hightemperature oxidation of nickel10.1016/S0010-938X(72)80013-1 ↗
41. Effect of Fe on corrosion of Ni-20Cr and Ni-30Cr alloys in wet CO2 gas at 650 and 700 °C10.1016/j.corsci.2019.04.007 ↗
42. Microstructure understanding of high Cr-Ni austenitic steel corrosion in high-temperature steam10.1016/j.actamat.2022.117634 ↗
43. The kinetic behaviour of metals in water vapour at high temperatures: can general rules be proposed?10.4028/www.scientific.net/MSF.369-372.231 ↗
44. Thermal oxidation kinetics and oxide scale adhesion of Fe–15Cr alloys as a function of their silicon content10.1016/j.actamat.2006.04.023 ↗
45. The effect of Al and Ti on the microstructure, mechanical properties and oxidation resistance of γ′-Ni3(Al, Ti) strengthened austenitic stainless steels10.1016/j.jmrt.2023.04.156 ↗
46. A high-resolution study of the different surface state effects on the corrosion behaviors of a ferritic steel and an austenitic steel in supercritical water10.1016/j.corsci.2022.110757 ↗
47. Microstructural understanding of the oxidation of an austenitic stainless steel in high-temperature steam through advanced characterization10.1016/j.actamat.2020.05.010 ↗
48. Time, temperature, and dissolved oxygen dependence of oxidation of austenitic and ferritic-martensitic alloys in supercritical water