About the role of iron on the alteration of simplified nuclear glasses in deaerated solutions at 50°C
Source abstract
Abstract
The effect of Fe on the alteration of two SiO2-B2O3-Na2O based glasses (Fe2O3-free or containing 3.1 mol.% Fe2O3) was studied by measurement of initial alteration rates and long-term leaching experiments at 50°C in initially pure water or in a 10−2 mol.L−1 FeCl2 solution. The glass alteration kinetics were monitored by periodical leachate analyses; and morphology, structure and composition of solid alteration products were characterized at the end of long-term experiments (i.e. after 323 days).Iron(III) initially incorporated in the glass strengthens the glass network, leading to a decrease of the initial dissolution rate (from 0.15 to 0.026 g.m−2.d−1 at 50°C). The environment of Fe(III) incorporated into the gel depends on the pH of the leaching solution. A change of Fe(III) coordination from fourfold (i.e. charge-compensated by Na+ ions) to sixfold is expected when the pH decreases. Whatever its coordination, Fe3+ hinders the gel restructuring into a passivating barrier. Thus, the addition of Fe in the glass composition ultimately leads to higher alteration extent (≈1.5 times greater after 323 days of leaching in our experiments).In experiments where Fe cations are provided by the leaching medium (mainly at the +II oxidation state), precipitation of Fe-silicates is systematically observed, as well as an increase in glass alteration compared to experiments led in initially pure water (by a factor slightly less than 2). A drastic change in the average pH of experiments (from ≈9 in initially pure water to ≈6 in FeCl2 solution) is also observed. Among mechanisms proposed in the literature to explain the detrimental effect of Fe-silicates precipitation, it seems that the decrease in pH resulting from this precipitation is the main cause of increase in glass alteration observed in this study.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Nuclear materials and radiation effects · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (57)
Show source-provided references
1. 2005 – Andra research on the geological disposal of high-level long-lived radioactive waste – Results and perspectives
2. SON68 nuclear glass dissolution kinetics: current state of knowledge and basis of the new GRAAL model10.1016/j.jnucmat.2008.06.044 ↗
3. Long-term behavior science: the cornerstone approach for reliably assessing the long-term performance of nuclear waste10.1016/j.jnucmat.2011.09.012 ↗
4. Hydrogen-sodium interdiffusion in borosilicate glasses investigated from first principles10.1016/j.jnoncrysol.2006.04.023 ↗
5. Modeling of the effect of iron corrosion products on nuclear waste glass performance10.1557/PROC-84-471 ↗
6. Insight into silicate-glass corrosion mechanisms10.1038/nmat2301 ↗
7. Origin and consequences of silicate glass passivation by surface layers10.1038/ncomms7360 ↗
8. Borosilicate glass corrosion in the presence of steel corrosion products10.1557/PROC-84-459 ↗
9. Effects of metals, metal oxides and metal hydroxide on the leaching of simulated nuclear waste glass10.1524/ract.1997.79.3.199 ↗
10. Effects of redox condition on waste glass corrosion in the presence of magnetite10.1557/PROC-412-257 ↗
11. Metal corrosion and argillite transformation at the water-saturated, high-temperature iron-clay interface: a microscopic-scale study10.1016/j.apgeochem.2008.05.019 ↗
12. Anodic activation of iron corrosion in clay media under water-saturated conditions at 90°C: characterization of the corrosion interface10.1021/es9021987 ↗
13. Corrosion of metal iron in contact with anoxic clay at 90 degrees C: Characterization of the corrosion products after two years of interaction10.1016/j.apgeochem.2014.09.002 ↗
14. Effect of iron metal and siderite on the durability of simulated archeological glassy material10.1016/j.corsci.2013.07.014 ↗
15. Silicate glass alteration enhanced by iron: origin and long-term implications10.1021/es304057y ↗
16. Impact of iron and magnesium on glass alteration: Characterization of the secondary phases and determination of their solubility constants10.1016/j.apgeochem.2017.04.010 ↗
17. Impact of iron on nuclear glass alteration in geological repository conditions: a multiscale approach10.1016/j.apgeochem.2012.12.016 ↗
18. Fe K-edge X-ray absorption spectroscopy of silicate minerals and glasses10.1051/jphyscol:19868160 ↗
19. Transition-metal ions in silicate melts. 2. iron in sodium-silicate glasses
20. Structural evolution of glass surface during alteration: Application to nuclear waste glasses10.1016/j.jnoncrysol.2010.02.022 ↗
21. Property modification of a high level nuclear waste borosilicate glass through the addition of Fe2O3, Glass Technol
22. New insight into the residual rate of borosilicate glasses: effect of S/V and glass composition10.1111/ijag.12048 ↗
23. The BET-Method
24. Jeffery · 1989
25. Effect of composition on the short-term and long-term dissolution rates of ten borosilicate glasses of increasing complexity from 3 to 30 oxides10.1016/j.jnoncrysol.2012.05.024 ↗
26. Glass–water interphase reactivity with calcium rich solutions10.1016/j.gca.2011.05.005 ↗
27. Atom-Probe Tomography, TEM and ToF-SIMS study of borosilicate glass alteration rim: A multiscale approach to investigating rate-limiting mechanisms10.1016/j.gca.2016.12.029 ↗
28. The fate of silicon during glass corrosion under alkaline conditions: a mechanistic and kinetic study with the International Simple Glass10.1016/j.gca.2014.12.009 ↗
29. Study of emission and sputtering yields in some alloys and oxide by glow discharge optical spectrometry: Quantification of analysis10.1002/sia.740070404 ↗
30. Mechanism of hydrogen absorption during the exposure of alloy 600-like single-crystals to PWR primary simulated media10.1016/j.jnucmat.2011.04.066 ↗
31. Hydrogen absorption associated with the corrosion mechanism of 316L stainless steels in primary medium of Pressurized Water Reactor (PWR)10.1016/j.corsci.2014.04.025 ↗
32. Quantitative surface analysis by glow discharge optical spectrometry10.1002/sia.740090105 ↗
33. Corrosion of the International Simple Glass under acidic to hyperalkaline conditions10.1038/s41529-018-0050-5 ↗
34. Alteration kinetics of a simplified nuclear glass in an aqueous medium: Effects of solution chemistry and of protective gel properties on diminishing the alteration rate10.1016/S0022-3115(00)00039-8 ↗
35. Characterization of Alteration Phases on HLW Glasses After 15 Years of PCT Leaching
36. Glass–iron–clay interactions in a radioactive waste geological disposal: An integrated laboratory-scale experiment10.1016/j.apgeochem.2010.11.004 ↗
37. Composition effects on synthetic glass alteration mechanisms: Part 1. Experiments10.1016/j.chemgeo.2010.10.010 ↗
38. Structural identification of a trioctahedral smectite formed by the aqueous alteration of a nuclear glass10.1016/j.clay.2010.04.016 ↗
39. Full Characterization of smectites
40. Mineralogy and thermodynamic properties of magnesium phyllosilicates formed during the alteration of a simplified nuclear glass10.1016/j.jnucmat.2016.04.008 ↗
41. The effect of iron on montmorillonite stability. (II) Experimental investigation10.1016/j.gca.2005.09.023 ↗
42. The sedimentary cycle of the boron isotopes10.1016/0016-7037(87)90183-9 ↗
43. Boron isotope geochemistry during diagenesis. Part I. Experimental determination of fractionation during illitization of smectite10.1016/S0016-7037(01)00557-9 ↗
44. Intracrystalline boron isotope partitioning in illite-smectite: Testing the geothermometer10.2138/am.2007.2531 ↗
45. Silicic acid ionization and calculation of silica solubility at elevated temperature and pH – Application to geothermal fluid processing and reinjection10.1016/0375-6505(82)90004-9 ↗
46. The Ionization Constant of Water over a Wide Range of Temperatures and Densities10.1063/1.1928231 ↗
47. Effect of natural and synthetic iron corrosion products on silicate glass alteration processes10.1016/j.gca.2015.09.033 ↗
48. SON68 glass alteration enhanced by magnetite10.1016/j.proeps.2013.03.039 ↗
49. Reactive transport processes occurring during nuclear glass alteration in presence of magnetite10.1016/j.apgeochem.2015.02.018 ↗
50. Experimental tests to validate the rate-limiting step assumption used in the kinetic analysis of solid-state reactions10.1016/j.tca.2008.08.013 ↗
51. Predictive modeling of leachate pH for simulated high-level waste glass
52. The role of aluminium in the durability of alumino-borosilicate glasses
53. 17O 3Q-MAS NMR characterization of a sodium aluminoborosilicate glass and its alteration gel10.1016/S0009-2614(01)00423-7 ↗
54. Monte Carlo simulations of the corrosion of aluminoborosilicate glasses10.1016/j.jnoncrysol.2013.07.014 ↗
55. Molecular mechanisms for corrosion of silica and silicate glasses10.1016/0022-3093(94)90708-0 ↗
56. SON 68 nuclear glass alteration kinetics between pH 7 and pH 11.510.1016/S0022-3115(01)00434-2 ↗
57. Glass dissolution as a function of pH and its implications for understanding mechanisms and future experiments10.1016/j.gca.2017.09.008 ↗