journal article·2024-12

Macroscopic and microscopic element distribution in transition zones of GTAW Alloy 52M weld joint and its PWSCC growth behaviour

Jiarong Ma, Xinhe Xu, Deng Pan, Tongming Cui, Zhanpeng Lu, Sergio Lozano-Perez, Junjie Chen, Donghui Wang, Kai Li, Hui Zheng

Publisher page

Abstract

The microstructure and element distribution in the transition zone (TZ) of Alloy 52M buttering (52Mb) layer near the fusion boundary to the SA508III low alloy steel in a dissimilar metal weld joint with post-weld heat treatment (PWHT) is characterized. Two macroscopic TZs in the heat-affected zone have lower Cr and Ni contents than the bulk Alloy 52Mb. The first TZ near the fusion boundary has the lowest Cr and Ni compositions, accompanying the highest Fe content. Cr depletion and Ni enrichment along with slight Fe enrichment at the dendrite boundaries in the TZs, are more significant than those in the bulk Alloy 52Mb. The number and the maximum depth of local oxidation penetrations at the alloy-inner oxide interface based on the oxidation tests, the number and the maximum length of locally interdendritic cracks, as well as the average crack growth rate (CGR) in terms of the stress corrosion cracking (SCC) band based on the SCC tests in the first TZ are higher than those in the second TZ. The average SCC CGR is enhanced by macroscopic element dilution, while local oxidation penetration, as well as locally interdendritic SCC, are thought to be enhanced by both the macroscopic dilution of Cr in the TZs and the microscopic Cr depletion at dendrite boundaries.
Source: expertdata · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Crack growth response of alloy 152 and 52 weld metals in simulated PWR primary water
2. Stress corrosion crack growth response for alloy 152/52 dissimilar metal welds in PWR primary water
3. Development of a highly weldable and corrosion resistant nickel-chromium filler metal
4. Effect of material chemical composition on oxidation and stress corrosion cracking of the submerged arc welding Alloy 52M overlay in a simulated PWR primary water10.1016/j.jnucmat.2023.154753 ↗
5. Effects of welding columnar grain orientation and strain rate on corrosion fatigue behavior of Alloy 52/52M weld metal in high-temperature water10.1016/j.corsci.2020.109196 ↗
6. Weldability, Thermal aging and PWSCC behavior of nickel weld metals containing 15 to 30% chromium
7. Effect of welding dilution and dendrite orientation on SCC behavior of Alloy 52M welding metal in simulated PWR primary water
8. SCC of Alloy 690 and its weld metals
9. P.L. Andresen, M.M. Morra, K. Ahluwalia, SCC of Alloy 690 and its weld metals in high temperature water, Corrosion Paper No. 3759 (2014).
10. SCC of Alloy 152/52 welds defects, repairs and dilution zones in PWR water
11. Characterization of microstructure, local deformation and microchemistry in Alloy 690 heat-affected zone and stress corrosion cracking in high temperature water10.1016/j.jnucmat.2015.06.025 ↗
12. Precursor evolution and stress corrosion cracking initiation of cold-worked Alloy 690 in simulated pressurized water reactor primary water10.5006/2470 ↗
13. Linking grain boundary microstructure to stress corrosion cracking of cold-rolled Alloy 690 in pressurized water reactor primary water10.5006/0808 ↗
14. Stress corrosion cracking of fusion boundary for 316L/52M dissimilar metal weld joints in borated and lithiated high temperature water10.1016/j.corsci.2017.01.024 ↗
15. Effects of phosphorus segregation on stress corrosion cracking in the heat-affected zone of a dissimilar weld joint between a Ni-base alloy and a low alloy steel10.1016/j.corsci.2014.10.037 ↗
16. Oxidation resistance and stress corrosion cracking susceptibility of 308L and 309L stainless steel cladding layers in simulated pressurized water reactor primary water10.5006/3699 ↗
17. Microstructure and stress corrosion cracking behavior of the weld metal in Alloy 52-A508 dissimilar welds10.2320/matertrans.M2010294 ↗
18. Cyclic and SCC behavior of Alloy 52M/182 weld overlay in a PWR environment
19. SCC of Alloy 152/52 welds defects, repairs and dilution zones in PWR water
20. Effects of matrix and dendrite boundary composition on stress corrosion cracking performance of Alloy 52M buttering layer in simulated pressurized water reactor primary water10.5006/4392 ↗
21. Stress corrosion cracking of alloy 52/152 weldments near dissimilar metal weld interfaces
22. Corrosion behavior of stainless steels in simulated PWR primary water “effect of chromium content in alloys and dissolved hydrogen10.1080/18811248.2008.9711883 ↗
23. Intergranular stress corrosion cracking behavior of austenitic stainless steels in hydrogenated high-temperature water10.5006/1.3278254 ↗
24. Influence of carbide precipitation and rolling direction on intergranular stress corrosion cracking of austenitic stainless steels in hydrogenated high-temperature water10.5006/1.3280670 ↗
25. Effects of composition and microstructure on oxidation and stress corrosion cracking susceptibility of stainless steel claddings in hydrogenated PWR primary water10.1016/j.jnucmat.2021.153057 ↗
26. Correlating oxidation resistance to stress corrosion cracking of 309L and 308L stainless steel claddings in simulated PWR primary water10.1016/j.jnucmat.2022.153509 ↗
27. Effects of iron content in Ni-Cr-xFe alloys and immersion time on the oxide films formed in a simulated PWR water environment10.1016/j.jnucmat.2017.10.048 ↗
28. Effects of iron content in Ni-Cr-Fe alloys on the oxide films formed in an oxygenated simulated PWR water environment10.1016/j.jnucmat.2018.06.014 ↗
29. Determining SCC resistance of stainless steel claddings in high-temperature water by constant load crack growth tests and slow strain rate tests10.1016/j.jnucmat.2023.154796 ↗
30. Intergranular stress corrosion cracking growth behavior of Ni-Cr-Fe alloys in pressurized water reactor primary water10.5006/1205 ↗
31. Effect of Cr and Ni on stress corrosion cracking susceptibility in Ni-Cr-Fe alloys under simulated pressurized water reactor primary conditions10.5006/1696 ↗
32. The effects of cold rolling orientation and water chemistry on stress corrosion cracking behavior of 316L stainless steel in simulated PWR water environments10.1016/j.jnucmat.2016.01.018 ↗
33. The effect of cold work and dissolved hydrogen in the stress corrosion cracking of Alloy 82 and Alloy 182 weld metal
34. Effect of deformation and orientation on SCC of alloy 690
35. Effect of cold work and processing orientation on stress corrosion cracking behavior of Alloy 60010.5006/1.3287659 ↗
36. Evaluation of the temperature dependence of alloy 690 and alloy 690 weld metal SCC growth in