journal article·2025-01Open access

Thermal evolution of helium bubbles in tungsten by GISAXS and TDS

Soon Han Bryan Teo, Matt Andrew Trevor Thompson, Nigel Kirby, Danielle Rose Hughes, Nour Hammoud, Aneeqa Khan, Hirohiko Tanaka, Noriyasu Ohno, Paul Mummery, Sarah Louise Harmer, Cormac Seamus Corr

Abstract

Grazing-incidence small-angle x-ray scattering (GISAXS) and thermal desorption spectroscopy (TDS) were used to study the thermal evolution of helium (He) bubbles in tungsten (W). W samples were exposed to a low ion energy (∼20 eV, sheath accelerated) He plasma at two sample temperatures: 573 K (low-temperature) and 1050 K (high-temperature). They were then annealed to temperatures of 773 K, 873 K and 998 K. GISAXS analysis showed an increase in the median bubble radius of the high-temperature samples from 6.42 Å to 12.87 Å as a result of annealing to 998 K. No changes in the bubble radii distributions were observed for the low-temperature samples and the median radius remained at ∼4 Å even after annealing. TDS showed that the desorption behaviour of He in W has a dependence on the sample temperature during plasma irradiation. The higher-temperature sample experienced a maximum desorption rate that is an order of magnitude larger than the low-temperature sample. The desorption profile of the high-temperature sample spanned a wider temperature range, 500 K - 1500 K, than the low-temperature sample, 500 K - 750 K. The formation and thermal evolution of He bubbles in W have a clear dependence on sample temperature during plasma exposure. The differences in annealing behaviour observed in this work agree with prior in-situ TEM annealing experiments and help explain macroscopic plasma-material interaction effects such as recrystallisation suppression. • Annealing causes growth in He bubbles in W exposed to plasma at 1050 K. • No growth in He bubbles after annealing W exposed to He plasma at 573 K. • He desorption by annealing is higher in W exposed at 1050 K than at 573 K. • He desorption in W exposed to 1050 K is a symptom of the bubble growth mechanism. • GISAXS trends agree with prior in-situ TEM annealing experiments.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Nuclear Physics and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. A full tungsten divertor for iter: physics issues and design status10.1016/j.jnucmat.2013.01.008 ↗
2. Physics basis for the first iter tungsten divertor
3. A. Loarte, R.A. Pitts, T. Wauters, I. Nunes, F. Köchl, A.R. Polevoi, S.H. Kim, M. Lehnen, M. Schneider, L. Zabeo, et al., Initial evaluations in support of the new iter baseline and research plan, 2024.
4. Retention and surface blistering of helium irradiated tungsten as a first wall material10.1016/j.jnucmat.2005.08.017 ↗
5. Helium bubble bursting in tungsten10.1063/1.4860315 ↗
6. Interaction between hydrogen and helium in tungsten successively exposed by helium and hydrogen plasma10.1016/j.jnucmat.2022.154184 ↗
7. Helium concentration measurement in tungsten fuzz-like nanostructures by means of thermal desorption spectroscopy10.1088/0029-5515/56/5/054002 ↗
8. Effect of he on d retention in w exposed to low-energy, high-fluence (d, he, ar) mixture plasmas10.1088/0029-5515/51/10/103021 ↗
9. In situ transmission electron microscope observation of the formation of fuzzy structures on tungsten
10. D.J. Campbell, A. Loarte, D. Boilson, X. Bonnin, P. de Vries, L. Giancarli, Y. Gribov, S.H. Kim, M. Lehnen, T. Luce, I. Nunes, A.R. Polevoi, S.D. Pinches, R.A. Pitts, R. Reichle, M. Schneider, J. Van Der Laan, G. Vayakis, Iter research plan within the staged approach, 2024.
11. Helium accumulation in metals during irradiation–where do we stand?10.1016/j.jnucmat.2003.09.001 ↗
12. Investigating the temperature dependence of helium bubble dynamics in plasma exposed tungsten via in-situ tem annealing10.1016/j.mtla.2024.102110 ↗
13. Peering into the self-assembly of surfactant templated thin-film silica mesophases10.1021/ja0295523 ↗
14. Analysis of 2d gisaxs patterns obtained on semiconductor nanocrystals10.1016/S0042-207X(02)00715-7 ↗
15. Particle layering in the ceramic-metal thin film pt- al 2 o 310.1103/PhysRevB.63.193407 ↗
16. Probing surface and interface morphology with grazing incidence small angle X-ray scattering10.1016/j.surfrep.2009.07.002 ↗
17. Gisaxs modelling of helium-induced nano-bubble formation in tungsten and comparison with tem10.1016/j.jnucmat.2016.01.038 ↗
18. Design and characterization of the magnetized plasma interaction experiment (magpie): a new source for plasma–material interaction studies10.1088/0963-0252/21/5/055033 ↗
19. Thermal expansion of periclase (mgo) and tungsten (w) to melting temperatures10.1007/s002690050070 ↗
20. On the rationale of maximum-entropy methods10.1109/PROC.1982.12425 ↗
21. Why least squares and maximum entropy? An axiomatic approach to inference for linear inverse problems
22. Large-scale atomistic simulations of low-energy helium implantation into tungsten single crystals10.1016/j.actamat.2017.09.061 ↗
23. Temperature dependence of retarded recrystallisation in helium plasma-exposed tungsten10.1088/1741-4326/ab2e3c ↗
24. Identifying microstructural changes responsible for retarded grain growth during tungsten recrystallization after helium plasma exposure10.1016/j.jnucmat.2021.153448 ↗
25. Formation of helium induced nanostructure ‘fuzz’ on various tungsten grades10.1016/j.jnucmat.2010.06.034 ↗
26. Helium bubble formation in ultrafine and nanocrystalline tungsten under different extreme conditions10.1016/j.jnucmat.2014.12.095 ↗
27. Irradiation effects of hydrogen and helium plasma on different grade tungsten materials10.1016/j.nme.2017.01.018 ↗
28. Tungsten evolution under helium irradiation: shape of bubbles by tem and in-situ gisaxs analysis
29. Clustering of h and he, and their effects on vacancy evolution in tungsten in a fusion environment10.1088/0029-5515/54/10/103007 ↗
30. Molecular dynamics simulation of helium cluster diffusion and bubble formation in bulk tungsten10.1016/j.jnucmat.2014.08.028 ↗
31. Noble gas bubbles in bcc metals: ab initio-based theory and kinetic Monte Carlo modeling10.1016/j.actamat.2021.116961 ↗
32. Formation of helium-bubble networks in tungsten10.1016/j.actamat.2018.07.075 ↗
33. Temperature-dependent model of helium bubble expansion and bursting in tungsten10.1016/j.jnucmat.2021.153101 ↗
34. Retarded recrystallization of helium-exposed tungsten10.1088/1741-4326/aad2b0 ↗
35. Effects of helium on mechanical properties of tungsten for fusion applications10.1016/j.nme.2018.04.003 ↗
36. Helium effects on recovery and recrystallization of powder metallurgically processed tungsten