journal article·2016-02

Fuel cladding behavior under rapid loading conditions

K. Yueh, J. Karlsson, J. Stjärnsäter, D. Schrire, G. Ledergerber, C. Munoz-Reja, L. Hallstadius

Publisher page

Abstract

Abstract A modified burst test (MBT) was used in an extensive test program to characterize fuel cladding failure behavior under rapid loading conditions. The MBT differs from a normal burst test with the use of a driver tube to simulate the expansion of a fuel pellet, thereby producing a partial strain driven deformation condition similar to that of a fuel pellet expansion in a reactivity insertion accident (RIA). A piston/cylinder assembly was used to pressurize the driver tube. By controlling the speed and distance the piston travels the loading rate and degree of sample deformation could be controlled. The use of a driver tube with a machined gauge section localizes deformation and allows for continuous monitoring of the test sample diameter change at the location of maximum hoop strain, during each test. Cladding samples from five irradiated fuel rods were tested between 296 and 553 K and loading rates from 1.5 to 3.5/s. The test rods included variations of Zircaloy-2 with different liners and ZIRLO, ranging in burn-up from 41 to 74 GWd/MTU. The test results show cladding ductility is strongly temperature and loading rate dependent. Zircaloy-2 cladding ductility degradation due to operational hydrogen pickup started to recover at approximately 358 K for test condition used in the study. This recovery temperature is strongly loading rate dependent. At 373 K, ductility recovery was small for loading rates less than 8 ms equivalent RIA pulse width, but longer than 8 ms the ductility recovery increased exponentially with increasing pulse width, consistent with literature observations of loading rate dependent brittle-to-ductile (BTD) transition temperature. The cladding ductility was also observed to be strongly loading rate/pulse width dependent for BWR cladding below the BTD temperature and Pressurized Water Reactor (PWR) cladding at both 296 and 553 K.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Nuclear and radioactivity studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Papin · 2003
2. Yegorova · 1999 · vol. 1
3. Boiling water reactor fuel behavior at burnup of 26 GWd/tonne U under reactivity-initiated accident conditions10.13182/NT94-A35042 ↗
4. Behavior of PWR and BWR fuels during reactivity-initiated accident conditions
5. Reevaluation of fuel enthalpy in nsrr test for high burnup fuels
6. Nuclear Fuel Behavior Under Reactivity-Initiated Accident (RIA) Conditions, State-of-the-art Report, NEA No. 6847, 2010.
7. Ductility and strain rate sensitivity of Zircaloy-4 nuclear fuel cladding10.1016/S0022-3115(01)00509-8 ↗
8. The effect of hydrogen and strain rate on the “ductile-brittle” behavior of zircaloy10.1016/0022-3115(67)90023-2 ↗
9. “RIA Fuel Codes Benchmark – Volume 1”, NEA/CSNI/R(2013)7.
10. Quantification of the margin provided by M5 cladding in accidental conditions
11. Analysis methodologies utilized to demonstrate compliance to fuel design limits for the AP1000 reactor
12. Failure of Zircaloy cladding under transverse plane-strain deformation10.1016/S0029-5493(98)00284-2 ↗
13. The PROMETRA program: fuel cladding mechanical behavior under high strain rate10.13182/NT07-A3814 ↗
14. High temperature expansion due to compression test for the determination of a cladding material failure criterion under RIA loading conditions
15. Failure characteristics of cladding tubes under RIA conditions10.1016/j.nucengdes.2008.03.017 ↗
16. Fracture of Zircaloy-4 cladding tubes with or without hydride blisters in uniaxial to plane strain conditions with standard and optimized expansion due to compression tests10.1016/j.msea.2014.02.075 ↗
17. Development of advanced expansion due to compression (A-EDC) test method for safety evaluation of degraded nuclear fuel cladding materials10.1080/00223131.2015.1056560 ↗
18. Failure of hydrided Zircaloy-4 under equal-biaxial and plane-strain tensile deformation
19. Behavior and failure of uniformly hydrided Zircaloy-4 fuel claddings between 25°C and 480°C under various stress states, including RIA loading conditions10.1016/j.engfailanal.2009.07.001 ↗
20. RIA failure of high burnup fuel rod irradiated in the leibstadt reactor: Out-of-pile mechanical simulation and comparison with pulse reactor tests
21. New techniques for the testing of cladding material under RIA conditions
22. Zircaloy-2 ductility recovery under RIA transient conditions
23. Arsène · Metallurgical Mater. Trans. A · 2003 · 34A · 55310.1007/s11661-003-0091-3 ↗
24. Enhancement of aqueous corrosion of Zircaloy-4 due to hydride precipitation at the metal-oxide interface
25. Fracture mechanics approach for failure mode analysis in CABRI and NSRR RIA tests
26. Ghosh · 2011
27. Radial-hydride embrittlement of high-burnup Zircaloy-4 fuel cladding10.1080/18811248.2006.9711195 ↗
28. Effect of radial hydrides on the axial and hoop mechanical properties of Zircaloy-4 cladding10.1016/j.jnucmat.2006.11.008 ↗
29. JAEA studies on high burnup fuel behaviors during reactivity-initiated accident and loss-of-coolant accident
30. Thermal solubility and partinioning of hydrides in the alpha phase of zirconium, zircaloy-2 and zircaloy-410.1016/0022-3115(67)90047-5 ↗
31. Effects of irradiation and hydriding on the mechanical properties of zircaloy-4 at high fluence
32. Geelhood · 2008
33. Alvis · 2010
34. A comparative analysis of CABRI CIPO-1 and NSRR VA-2 reactivity initiated accident tests