Source abstract
Abstract
Abstract A part of the radioactive waste produced in the Thorium Molten Salt Reactor (TMSR) will be present as fluorides. Because of some characters of fluoride, it is undesirable for immobilizing the waste as other usual oxide waste in borosilicate glass that often produces immiscibility. However, iron phosphate glasses have been made with up to 30 wt% SrF2 and 20 wt% CeF3, and about 20 wt% SrF2 and CeF3 combined. The iron phosphate glass matrix mixed with fluoride waste could be melted at temperatures between 1050 °C and 1200 °C in only 30–60 min, its melting temperature is lower than that of borosilicate glass. Powder X-ray diffraction (XRD) showed that the glassy wasteforms that contains more than 20% wt% SrF2 and CeF3 mixture, or more than 20 wt% CeF3 would start crystallizing. The product consistency test (PCT) was used to identify the chemical durability of the glass. Glass powder (−100 to +200 mesh) after washing was soaked in 10 ml of deionized water at 90 °C for 7 days. The normalized elemental mass release of elements Sr, Ce and F were calculated at the level of 10−3 g/m2, through the concentration of element measured after PCT, that was equivalent to or better than that of borosilicate glass wasteforms. Iron phosphate glasses are concluded to be a practical alternative for vitrifying the radioactive waste of TMSR.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Glass properties and applications · Nuclear materials and radiation effects · Recycling and utilization of industrial and municipal waste in materials production
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Qiu · Atomic Energy Sci. Technol. · 2009 · 51
2. Cai · Prog. Nucl. Energy · 2014 · 74 · 110.1016/j.pnucene.2014.02.007 ↗
3. Ojovan · Phosphate Glasses. · 2005 · 227
4. Brow · J. Non-Cryst. Solids · 2000 · 263 · 110.1016/S0022-3093(99)00620-1 ↗
5. Sengupta · J. Hazard Mater. · 2012 · 235 · 1710.1016/j.jhazmat.2012.07.039 ↗
6. Brezhneva · 1973 · 2
7. Properties of phosphate-glass waste forms containing fluorides from molten salt reactor10.1007/s41365-016-0059-9 ↗
8. Lavrinovich · Atom. Energy · 2003 · 95 · 78110.1023/B:ATEN.0000016764.68862.5f ↗
9. Mesko · Waste Manag. · 2000 · 20 · 27110.1016/S0956-053X(99)00331-1 ↗
10. Day · J. Non-Cryst. Solids · 1998 · 241 · 110.1016/S0022-3093(98)00759-5 ↗
11. G.K. Marasinghe, M. Karabulut, C.S. Ray, D.E. Day, M.G. Shumsky, W.B. Yelon, C.H. Booth, P.G. Allen, D.K. Shuh. Structural features of iron phosphate glasses, J. Non-Cryst. Solids vol. 222, p. 144–152.10.1016/S0022-3093(97)90107-1 ↗
12. ASTM C1285–C1294.
13. Structure and chemical durability of Ce-Doped iron borophosphate glasses
14. Development and characterization of the defense waste processing facility (DWPF) environmental assessment (EA) glass standard reference material
15. Effect of minor components on vitrification of low-level simulated nuclear waste glasses
16. Yu · J. Non-cryst. Solids · 1997 · 215 · 2110.1016/S0022-3093(97)00022-7 ↗
17. Greaves · Philos. Mag. A B · 1988 · 58 · 21710.1080/13642818808208482 ↗
18. Structural properties of sodiumiron phosphate glasses
19. Mesko · 1993
20. Phosphate glass dissolution in aqueous solutions10.1016/0022-3093(84)90184-4 ↗
21. Fou de Kerdaniel · J. Nucl. Mater. · 2007 · 362 · 45110.1016/j.jnucmat.2007.01.132 ↗
22. Veilly · Inorg. Chem. · 2008 · 47 · 1097110.1021/ic801169d ↗
23. Mesbah · Cryst. Growth Des. · 2014 · 14 · 509010.1021/cg500707b ↗
24. Gausse · Eur. J. Inorg. Chem. · 2016 · 461510.1002/ejic.201600517 ↗