Variation of martensite phase transformation mechanism in minor-stressed T91 ferritic steel
Source abstract
Abstract
Abstract The effects of compressive stress applied at different temperatures on martensite transformation process of the T91 steel were studied by high-resolution differential dilatometer. The stress applied above 850 °C exhibits no influence on the martensite formation. The stress applied below 850 °C not only facilitates the formation of martensite, but also enhances the onset temperature of the martensite transformation. There are two different transformation mechanisms occurring: when the compressive stress is applied at high temperature, the mechanism of strain-induced martensite transformation takes place, as a result, the microstructure tends to be refined with irregular grain boundary. When the compressive stress is applied at low temperature, the stress-induced martensite transformation occurs, and its morphology is similar to that of thermal-activated martensite. In addition, it is summarized that 200 MPa is the critical stress and 440 °C is critical temperature for the onset of the stress-induced martensite transformation for the investigated T91 ferritic steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (11)
Show source-provided references
1. Paul · J. Nucl. Mater. · 2008 · 378 · 27310.1016/j.jnucmat.2008.06.033 ↗
2. Seok Kim · J. Nucl. Mater. · 2008 · 377 · 49610.1016/j.jnucmat.2008.04.012 ↗
3. Sawada · Mater. Sci. Eng. A · 2008 · 480 · 55810.1016/j.msea.2007.09.031 ↗
4. Kim · Mater. Sci. Eng. A · 2008 · 483&484 · 54410.1016/j.msea.2006.12.151 ↗
5. Sasikala · Mater. Sci. Eng. A · 2008 · 479 · 10510.1016/j.msea.2007.06.021 ↗
6. Xu · 1999
7. Xu · Heat Treat. · 2004 · 19 · 1
8. Liu · Acta Mater. · 2003 · 51 · 50710.1016/S1359-6454(02)00434-2 ↗
9. Liu · Acta Mater. · 2009 · 57 · 285810.1016/j.actamat.2009.02.044 ↗
10. Klueh · Scripta Mater. · 2005 · 53 · 27510.1016/j.scriptamat.2005.04.019 ↗
11. Zhu · Steel Pipe · 1999 · 28 · 8