Corrosion behavior of pre-oxidized HR-224 superalloy in supercritical water environment at 700 °C
Source abstract
Abstract
Abstract Corrosion of cladding materials in supercritical water (SCW) environment is a key reliability issue for the safety of nuclear power plant. In this study, we propose to use the pre-oxidized treatment to provide better corrosion resistance of cladding materials in the SCW environment. The nickel-based superalloy HR-224 was first pre-oxidized in flowing air at 982 °C for 100 h to establish a continuous and dense scales and then exposed in the SCW environment with high oxygen content (8.3 ppm) at 700 °C and 24.8 MPa for cyclic oxidation testing up to 1300 h. The pre-oxidized samples exhibit better corrosion resistance than as-received samples in the SCW environment. After pre-oxidizing process, triple scales, Ni(Cr, Fe)2O4 spinel/Cr2O3/α-Al2O3 were observed, and the growth of inner α-Al2O3 layer is predominant in the SCW environment. The α-Al2O3 layer in pre-oxidized samples was found to effectively decrease outward migration of metal ions in Alloy HR-224 and thus provides better corrosion resistance than as-received samples in SCW environment.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Subcritical and Supercritical Water Processes · Advanced Materials Characterization Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (43)
Show source-provided references
1. U.D.N.E.R.A.C.a.t.G.I.I.F. (GIF-002–00) · 2002
2. The system hydrogen - water up to 440°C and 2500 bar pressure10.1002/bbpc.19810850103 ↗
3. High pressure phase equilibria and PVT-data of the water-oxygen system including water-air to 673 K and 250 MPa10.1002/bbpc.19850891206 ↗
4. Selection and corrosion evaluation tests of candidate SCWR fuel cladding materials10.1016/j.nucengdes.2011.08.086 ↗
5. Lumpkin · 2018 · 333
6. Predicted water chemistry in the primary coolant circuit of a supercritical water reactor10.13182/NSE12-16 ↗
7. Localized corrosion of magnetite on ferritic–martensitic steels exposed to supercritical water10.1016/j.corsci.2009.08.021 ↗
8. Corrosion of ferritic–martensitic steel HT9 in supercritical water10.1016/j.jnucmat.2006.07.010 ↗
9. Oxidation behavior of iron-based alloy HCM12A exposed in supercritical water10.1016/j.corsci.2005.10.010 ↗
10. Corrosion behavior of ferritic–martensitic steel T91 in supercritical water10.1016/j.corsci.2005.08.021 ↗
11. Corrosion and stress corrosion cracking in supercritical water10.1016/j.jnucmat.2007.05.017 ↗
12. Corrosion behavior of Ni-base alloys for advanced high temperature water-cooled nuclear plants10.1016/j.corsci.2008.08.024 ↗
13. Microstructure tailoring for property improvements by grain boundary engineering10.1016/j.jnucmat.2007.08.015 ↗
14. The effect of grain boundary engineering on the oxidation behavior of INCOLOY alloy 800H in supercritical water10.1016/j.jnucmat.2005.09.023 ↗
15. Corrosion behavior of alloy 800H (Fe–21Cr–32Ni) in supercritical water10.1016/j.corsci.2010.10.021 ↗
16. Corrosion of pre-oxidized nickel alloy X-750 in simulated BWR environment10.1016/j.jnucmat.2017.01.051 ↗
17. Investigation into the effect of water chemistry on corrosion product formation in areas of accelerated flow10.1016/j.jnucmat.2017.06.030 ↗
18. Effect of dissolved oxygen content on the oxide structure of Alloy 625 in supercritical water environments at 700° C10.1016/j.corsci.2013.11.034 ↗
19. Corrosion behavior of Alloy 625 in supercritical water environments10.1016/j.pnucene.2011.12.015 ↗
20. Corrosion of alumina-forming austenitic steel Fe–20Ni–14Cr–3Al–0.6 Nb–0.1 Ti in supercritical water10.1016/j.jnucmat.2010.01.025 ↗
21. Influence of alloy composition and temperature on corrosion behavior of ODS ferritic steels10.1016/j.jnucmat.2010.12.279 ↗
22. Corrosion behaviour of 16%Cr–4%Al and 16%Cr ODS ferritic steels under different metallurgical conditions in a supercritical water environment10.1016/j.corsci.2010.05.043 ↗
23. Development of Al added high-Cr ODS steels for fuel cladding of next generation nuclear systems10.1016/j.jnucmat.2010.12.300 ↗
24. Barin · 1997
25. Corrosion screening tests of high-performance ceramics in supercritical water containing oxygen and hydrochloric acid10.1016/S0955-2219(96)00072-6 ↗
26. Hara · Mater. Jpn · 2000 · 39 · 32510.2320/materia.39.325 ↗
27. Lai · 1990
28. 1988
29. Opila · Sci. Forum · 2004 · 461–464
30. Pint · Mater. Sci. Forum · 2004 · 461–464 · 81510.4028/www.scientific.net/MSF.461-464.815 ↗
31. High-temperature oxidation performance of a new alumina-forming Ni–Fe–Cr–Al alloy in flowing air10.1016/j.ijhydene.2010.04.099 ↗
32. Oxidation of single crystal PWA 1483 at 950 °C in flowing air10.1016/j.corsci.2008.06.033 ↗
33. Oxidation of nickel-based single-crystal superalloys for industrial gas turbine applications10.1016/j.actamat.2010.09.027 ↗
34. Clark · 1966
35. Differences in growth mechanisms of oxide scales formed on ODS and conventional wrought alloys10.1007/BF00665269 ↗
36. SIMS investigations of the transport phenomena in chromia and alumina scales on ODS alloys
37. 18O Tracer studies of Al2O3 scale formation on NiCrAl alloys10.1007/BF00742122 ↗
38. Anion diffusion in α-Cr2O310.1111/j.1151-2916.1965.tb11802.x ↗
39. Self-diffusion of oxygen in single crystal and polycrystalline aluminum oxide10.1063/1.1731170 ↗
40. Transport phenomena in undoped and chromium or yttrium doped-alumina10.1080/00337578308224712 ↗
41. Diffusion du chrome et du fer dans l'alumine α monocristalline10.1016/0036-9748(80)90222-7 ↗
42. Diffusion of cations in chromia layers grown on iron-base alloys10.1007/BF00665632 ↗
43. Self-diffusion in α-Al2O3 I. Aluminium diffusion in single crystals10.1080/01418619408242929 ↗