Fe-saponite growth on low-carbon and stainless steel in hydrothermal-bentonite experiments
Source abstract
Abstract
Abstract Hydrothermal experiments on engineered barrier system (EBS) materials were conducted to characterize high temperature interactions between bentonite and candidate waste container steels (304SS, 316SS, low-C steel) for deep geological disposition of nuclear spent fuel. Hydrothermal experiments were performed using Dickson reaction cells at temperatures and pressure of up to 300 °C and 15–16 MPa, respectively, for four to six weeks. Wyoming bentonite was saturated with a 1900 ppm K-Ca-Na-Cl solution in combination with stainless and low-C steel coupons. Authigenic Fe-saponite precipitated utilizing steel as a growth substrate with Fe being supplied by steel corrosion. Concurrent with Fe-saponite formation, sulfides precipitated from sulfide-bearing fluids, from pyrite dissolution, near the steel interface. Sulfide mineral formation is dependent on the steel substrate composition: stainless steel produced pentlandite ((Ni, Fe)9S8) and millerite (NiS), whereas low C steel generated pyrrhotite (Fe7S8). The presence of sulfides suggests highly reduced environments at the steel-clay barrier interface potentially influencing overall steel corrosion rates and (re)passivation mechanisms. Results of this research show that nuclear waste steel container material may act as a substrate for mineral growth in response to corrosion during hydrothermal interactions with bentonite barriers.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Groundwater flow and contamination studies · Soil and Unsaturated Flow · Radioactive element chemistry and processing
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (69)
Show source-provided references
1. Hardin · 2013 · 190
2. Greenberg · 2013
3. Multi-purpose container technologies for spent fuel management
4. Pusch · 2008
5. Bryan · 2014
6. Ilgen · 2014 · 26
7. Hydrogen embrittlement of steels10.1146/annurev.ms.08.080178.001551 ↗
8. Results and interpretation of gas-driven radionuclide transport in undisturbed and disturbed Boom Clay
9. The effect of iron on montmorillonite stability. (II) Experimental investigation10.1016/j.gca.2005.09.023 ↗
10. The effect of iron on montmorillonite stability. (I) Background and thermodynamic considerations10.1016/j.gca.2005.10.003 ↗
11. Thermodynamic and fully-coupled reactive transport models of a steel–bentonite interface10.1016/j.apgeochem.2015.05.005 ↗
12. Bentonite evolution at elevated pressures and temperatures: an experimental study for generic nuclear repository designs10.2138/am.2014.4673 ↗
13. Rocking autoclaves for hydrothermal experiments II. The flexible reaction-cell system
14. 5.17 - deep fluids in the continents: II. Crystalline rocks A2 - holland, heinrich D
15. Corrosion behavior of stainless steels in simulated PWR primary water—effect of chromium content in alloys and dissolved hydrogen—10.1080/18811248.2008.9711883 ↗
16. TEM investigations of the oxide layers formed on a 316L alloy in simulated PWR environment10.1007/s10853-012-6975-0 ↗
17. The mechanism of high temperature aqueous corrosion of stainless steels10.1016/0010-938X(91)90125-9 ↗
18. Robertson · 1989 · vol. 1 · 81
19. The mechanism and kinetics of corrosion product release from stainless steel in lithiated high temperature water10.1016/0010-938X(87)90068-0 ↗
20. The composition and morphology of oxide films formed on type 304 stainless steel in lithiated high temperature water10.1016/0010-938X(86)90024-7 ↗
21. The mechanism of oxide film formation on austenitic stainless steels in high temperature water10.1016/S0010-938X(97)00140-6 ↗
22. Analysis of oxide film formed on type 304 stainless steel in 288°C water containing oxygen, hydrogen, and hydrogen peroxide10.5006/1.3283969 ↗
23. Corrosion behavior of 304 stainless steel in high temperature, hydrogenated water10.1016/S0010-938X(02)00004-5 ↗
24. Nanostructure and local properties of oxide layers grown on stainless steel in simulated pressurized water reactor environment10.1016/j.corsci.2014.03.030 ↗
25. Multilayered surface oxides within crevices of type 316L stainless steels in high-temperature pure water10.5006/1106 ↗
26. Jiao · 2015 · 42
27. Oxidation behavior of 304 stainless steel during crevice corrosion in high-temperature pure water10.5006/1705 ↗
28. Calculation of the relative metastabilities of proteins using the CHNOSZ software package10.1186/1467-4866-9-10 ↗
29. Thermodynamics of Cr2O3, FeCr2O4, ZnCr2O4, and CoCr2O410.1016/j.jct.2007.03.001 ↗
30. Thermodynamic Properties of Minerals and Related Substances at 298.15 K and 1 Bar (10ˆ5 Pascals) Pressure and at Higher Temperatures
31. Wolery · 2003
32. Iron-rich saponite (ferrous and ferric forms)10.1346/CCMN.1973.0210405 ↗
33. Duane · 1997
34. Kinetics of pyrite to pyrrhotite reduction by hydrogen in calcite buffered solutions between 90 and 180°C: implications for nuclear waste disposal10.1016/j.gca.2010.02.027 ↗
35. Evidence of montmorillonite/Fe-rich smectite transformation in the Morrón de Mateo bentonite deposit (Spain): implications for the clayey barrier behaviour10.1016/j.clay.2015.12.033 ↗
36. Clay minerals in the miocene low-grade metamorphic rocks, tanzawa mountains, kanagawa prefecture, central Japan10.2465/ganko1941.68.311 ↗
37. Conversion of trioctahedral smectite to interstratified chlorite/smectite in Plioscene acidic pyroclastic sediments of the Ohyu District, Akita Prefecture, Japan
38. Compositions and parageneses of secondary minerals in the Onikobe geothermal system, Japan10.1016/0009-2541(85)90143-3 ↗
39. Smectite-to-chlorite transformation in thermally metamorphosed volcanoclastic rocks in the Kamikita area, northern Honshu, Japan
40. Thermodynamic modeling of Fe–Ni pentlandite10.1016/j.jpcs.2007.10.011 ↗
41. Experimental reduction of aqueous sulphate by hydrogen under hydrothermal conditions: implication for the nuclear waste storage10.1016/j.gca.2009.05.043 ↗
42. Sulphide mineral reactions in clay-rich rock induced by high hydrogen pressure. Application to disturbed or natural settings up to 250°C and 30bar10.1016/j.chemgeo.2013.05.025 ↗
43. Mineralogical evolution of A claystone after reaction with iron under thermal gradient10.1346/CCMN.2012.0600501 ↗
44. Experimental synthesis of chlorite from smectite at 300°C in the presence of metallic Fe10.1180/0009855033830096 ↗
45. Experimental study of the transformation of smectite at 80 and 300°C in the presence of Fe oxides10.1180/0009855043910117 ↗
46. Effects of temperature, pH, and iron/clay and liquid/clay ratios on experimental conversion of dioctahedral smectite to berthierine, chlorite, vermiculite, or saponite10.1346/CCMN.2010.0580212 ↗
47. Experimental investigation of smectite interaction with metal iron at 80 °C: structural characterization of newly formed Fe-rich phyllosilicates10.2138/am.2012.4062 ↗
48. Experimental study of smectite interaction with metal Fe at low temperature: 1. Smectite destabilization10.1346/CCMN.2005.0530606 ↗
49. Bentonite–iron interactions under alkaline condition: an experimental approach10.1016/j.clay.2006.01.006 ↗
50. Evidence of a critical content in Fe(0) on FoCa7 bentonite reactivity at 80 °C10.1016/j.clay.2007.03.002 ↗
51. Towards a link between the energetic heterogeneities of the edge faces of smectites and their stability in the context of metallic corrosion10.1016/j.gca.2006.12.011 ↗
52. The effect of smectite on the corrosion of iron metal10.1346/CCMN.2012.0600204 ↗
53. Iron–clay interactions under hydrothermal conditions: impact of specific surface area of metallic iron on reaction pathway10.1016/j.chemgeo.2014.05.013 ↗
54. Carbon steel corrosion in clay-rich environment10.1016/j.corsci.2014.07.020 ↗
55. Iron–clay interactions: detailed study of the mineralogical transformation of claystone with emphasis on the formation of iron-rich T–O phyllosilicates in a step-by-step cooling experiment from 90°C to 40°C10.1016/j.chemgeo.2014.08.010 ↗
56. Reaction of smectites with iron in a nitrogen atmosphere at 75°C10.1016/j.clay.2010.08.004 ↗
57. Metal corrosion and argillite transformation at the water-saturated, high-temperature iron–clay interface: a microscopic-scale study10.1016/j.apgeochem.2008.05.019 ↗
58. Anodic activation of iron corrosion in clay media under water-saturated conditions at 90 °C: characterization of the corrosion interface
59. Corrosion of metal iron in contact with anoxic clay at 90°C: characterization of the corrosion products after two years of interaction10.1016/j.apgeochem.2014.09.002 ↗
60. Iron corrosion in Callovo–Oxfordian argilite: from experiments to thermodynamic/kinetic modelling10.1016/j.pce.2006.04.019 ↗
61. Synthesis of smectite clay minerals; a critical review10.1346/CCMN.1999.0470501 ↗
62. Synthesis and characterization of saponite clays: Part 2. Thermal stability10.2138/am.2005.1617 ↗
63. Contribution of long-term hydrothermal experiments for understanding the smectite-to-chlorite conversion in geological environments10.1007/s00410-016-1307-z ↗
64. Corrosion of iron in gaseous environments and in gas-saturated aqueous environments10.5006/1.3585068 ↗
65. Vedage · 1993
66. Smith · 2006
67. Corrosion of iron in an H2S-CO2-H2O system mechanism of sulfide film formation and kinetics of corrosion reaction10.5006/0010-9312-21.8.245 ↗
68. Interaction of Eu-isotopes with saponite as a component of the engineered barrier10.1016/j.clay.2011.02.027 ↗
69. Quantification and comparison of the reaction properties of FEBEX and MX-80 clays with saponite: europium immobilisers under subcritical conditions10.1016/j.clay.2014.08.012 ↗