journal article·2020-10Open access

Plasma and X-ray radiation-induced damage mechanisms in a tungsten heavy alloy

Qi An, Ahmed Elshafiey, Lujun Huang, David A. Hammer, Mostafa Hassani

Abstract

Abstract Tungsten-based materials are among the main candidate plasma-facing materials for future fusion reactors where extreme conditions of thermomechanical stresses, radiation, and energetic particles must be withstood. Here a hybrid X-pinch platform combined with a pulsed power machine was used to study damage mechanisms in 90W–4Cu–6Ni tungsten heavy alloy as a result of exposure to high energy density plasma, X-ray radiation, and the resulting thermal shock. It was found that the plasma-facing surface of the material undergoes severe melting and ablation with the extent of ablation being higher in the Cu–Ni phase than the W particles. Rapid melting and solidification transform the W particles into fine dendrite morphologies embedded in the Cu–Ni solid solution. Cracking was also observed in the subsurface layers at the interfaces between the W particles and the Cu-rich phase of the Cu–Ni matrix. X-ray radiation, on the other hand, cause slight melting on the surface without significant ablation and no cracking.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Advanced materials and composites · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (46)

Show source-provided references
1. Structure and phase composition of tungsten alloys modified by compression plasma flows and high-intense pulsed ion beam impacts10.1016/j.apsusc.2019.06.113 ↗
2. Plasma-wall interaction of advanced materials10.1016/j.nme.2016.10.008 ↗
3. Damages on pure tungsten irradiated by compression plasma flows10.1016/j.nimb.2018.12.050 ↗
4. A review of ELMs in divertor tokamaks10.1016/S0022-3115(96)00504-1 ↗
5. A comparative study on the in situ helium irradiation behavior of tungsten: coarse grain vs. nanocrystalline grain10.1016/j.actamat.2018.01.015 ↗
6. Helium-implantation-induced lattice strains and defects in tungsten probed by X-ray micro-diffraction10.1016/j.matdes.2018.11.001 ↗
7. Temperature dependence of helium-implantation-induced lattice swelling in polycrystalline tungsten: X-ray micro-diffraction and Eigenstrain modelling10.1016/j.scriptamat.2015.05.029 ↗
8. Saturation of deuterium retention in self-damaged tungsten exposed to high-flux plasmas10.1088/0029-5515/52/2/023008 ↗
9. Ion-irradiation induced clustering in W-Re-Ta, W-Re and W-Ta alloys: an atom probe tomography and nanoindentation study10.1016/j.actamat.2016.10.050 ↗
10. Competing kinetics and he bubble morphology in W10.1103/PhysRevLett.114.105502 ↗
11. Nanostructured fuzz growth on tungsten under low-energy and high-flux He irradiation10.1038/srep10959 ↗
12. Measures to overcome deep cracks of tungsten tiles in the ASDEX Upgrade divertor10.1016/j.fusengdes.2019.04.011 ↗
13. Surface damage characteristics of CFC and tungsten with repetitive ELM-like pulsed plasma irradiation10.1016/j.jnucmat.2010.12.019 ↗
14. Fabrication of ODS austenitic steels and CoCrFeNi high-entropy alloys by spark plasma sintering for nuclear energy applications
15. Effect of Re-deposition layers in plasma-facing wall on tritium retention and tritium depth profile10.1585/pfr.14.1405125 ↗
16. Refractory metals as structural materials for fusion high heat flux components10.1016/j.jnucmat.2018.09.052 ↗
17. Thermal shock of tungsten carbide in plasma-facing conditions10.1016/j.jnucmat.2019.06.041 ↗
18. Fluence dependence of helium ion irradiation effects on the microstructure and mechanical properties of tungsten10.1016/j.nimb.2017.09.002 ↗
19. Combined effect of laser thermal shock and helium ion irradiation on W-Y2O3 composites10.1016/j.fusengdes.2019.01.134 ↗
20. On the effects of different regimes of plasma pulses affecting the material due to their succession10.1016/j.nme.2019.01.012 ↗
21. Plasma facing and high heat flux materials – needs for ITER and beyond10.1016/S0022-3115(02)01175-3 ↗
22. Μicro-structured tungsten: an advanced plasma-facing material10.1016/j.nme.2019.02.007 ↗
23. Influence of dual beam ion irradiation and transient heat loading on tungsten surface morphology and erosion10.1016/j.jnucmat.2018.12.004 ↗
24. Investigations on tungsten heavy alloys for use as plasma facing material10.1016/j.fusengdes.2017.01.043 ↗
25. Elevated temperature tensile behavior and microstructure evolution of liquid phase sintered 90W-7Ni-3Fe alloy10.1016/j.jallcom.2019.06.222 ↗
26. Tensile and impact properties of microwave sintered tungsten heavy alloys10.1016/j.msea.2014.03.130 ↗
27. Recent progress in processing of tungsten heavy alloys10.1155/2014/764306 ↗
28. Results on the use of tungsten heavy alloys in the divertor of ASDEX Upgrade10.1016/j.jnucmat.2018.05.066 ↗
29. Radiographic and spectroscopic studies of X-pinch plasma implosion dynamics and x-ray burst emission characteristics10.1063/1.1351553 ↗
30. Hybrid X-pinches10.1134/S1063780X1204006X ↗
31. Hybrid X-pinch with conical electrodes10.1063/1.3504226 ↗
32. Evolution of the structure of the dense plasma near the cross point in exploding wire X pinches10.1063/1.873241 ↗
33. Electron kinetics inferred from observations of microwave bursts during edge localized modes in the mega-amp spherical tokamak10.1103/PhysRevLett.114.125004 ↗
34. X-pinch X-ray emission on a portable low-current, fast rise-time generator10.1063/1.5032112 ↗
35. Dynamics of hybrid X-pinches10.1134/S1063780X15010031 ↗
36. Deuterium-Fiber-initiated Z-pinches: simulation compared to experiment
37. Enhanced stability and neutron production in a dense Z-pinch plasma formed from a frozen deuterium fiber10.1103/PhysRevLett.59.892 ↗
38. High-gain magnetized inertial fusion10.1103/PhysRevLett.108.025003 ↗
39. Selective laser melting of W-Ni-Cu composite powder: densification, microstructure evolution and nano-crystalline formation10.1016/j.ijrmhm.2017.09.004 ↗
40. Effect of two-time spark plasma sintering on microstructure and mechanical properties of W-6Ni-4Mn alloy10.1016/j.msea.2018.12.109 ↗
41. Murdoch · 2013
42. Mechanical properties and microstructures after abnormal grain growth in electrodeposited Ni-W alloys10.1016/j.mtla.2019.100481 ↗
43. Radiation tolerance of Cu/W multilayered nanocomposites10.1016/j.jnucmat.2011.03.030 ↗
44. Surface modifications of fusion reactor relevant materials on exposure to fusion grade plasma in plasma focus device10.1016/j.apsusc.2015.07.192 ↗
45. Plasma focus assisted damage studies on tungsten10.1016/j.apsusc.2012.10.093 ↗
46. Brandes · 2013