Segregation behavior of Fe and Gd in molten corium during solidification progress
Source abstract
Abstract
Abstract For a criticality assessment of the fuel debris generated by the Fukushima–Daiichi Nuclear Power Plant accident, knowing the segregation of neutron absorber materials, i.e., Gd, B, and Fe, in the fuel debris is necessary. Although B may mostly evaporate during melting, Fe and Gd are expected to remain in the molten corium. To understand the redistribution behavior of Gd and Fe during the solidification of the molten corium, solidification experiments with simulated corium (containing UO2, ZrO2, FeO, and Gd2O3 with a small amount of simulated fission products such as MoO3, Nd2O3, SrO, and RuO2) were performed using a cold crucible induction heating method. The simulated corium was slowly cooled from 2500 °C and solidified from the bottom to the top of the melt. An elemental analysis of the solidified material showed that the Fe-concentration in the inner region increased up to approximately 3.4 times that in the bottom region. This suggested that FeO might be concentrated in the residual melt and that, consequently, the concentration of Fe increased in the later solidification region. On the contrary, the Gd concentration in the periphery region was found to be approximately 2.0 times higher than that in the inner region, suggesting the segregation of Gd in the early solidified phase and to remain with the residual, UO2-rich phase even after oxidative losses. No significant segregation was observed for the simulated fission products.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Metallurgical Processes and Thermodynamics · Metallurgy and Material Science
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Raj Sehgal · 2012
2. Fundamental research program for removal of fuel debris
3. Oxidation of boron carbide at high temperatures10.1016/j.jnucmat.2004.09.022 ↗
4. Characterization of solidified melt among materials of UO2 fuel and B4C control blade10.1080/00223131.2014.912567 ↗
5. Phenomenology of BWR fuel assembly degradation10.1016/j.jnucmat.2017.12.004 ↗
6. Lattice contraction and lattice deformation of UO2 and ThO2 doped with Gd2O310.1016/j.jnucmat.2015.09.018 ↗
7. Thermal conductivities of irradiated UO2 and (U,Gd)O210.1016/S0022-3115(00)00578-X ↗
8. Investigations of the melting behaviour of the U–Zr–Fe–O system10.1080/00223131.2015.1023381 ↗
9. Ternary eutectics in the systems FeO-UO2-ZrO2 and Fe2O3-U3O8-ZrO210.1134/S1066362211010024 ↗
10. TEPCO HP
11. Fundamental study on the segregation behavior in U-Zr-Fe-O system during solidification process10.3327/taesj.J18.029 ↗
12. The COMET-L3 experiment on long-term melt–concrete interaction and cooling by surface flooding10.1016/j.nucengdes.2008.12.005 ↗
13. 1981
14. Kinetics of oxidization processes of ruthenium particles10.1111/j.1151-2916.1998.tb02655.x ↗
15. The density of UO2–ZrO2 alloys10.1023/A:1026140627382 ↗
16. Tsurikov · 2007 · vol 15
17. Phase diagram of the UO2–FeO1+x system10.1016/j.jnucmat.2006.11.004 ↗
18. Phase diagram of the ZrO2–FeO system10.1016/j.jnucmat.2005.09.009 ↗
19. Burnable poison-doped fuel10.1016/B978-0-08-056033-5.00037-9 ↗
20. A Numerical simulation method for molten material behavior in nuclear reactors10.1016/j.nucengdes.2017.06.032 ↗