Negative effect of bismuth in lead on liquid metal embrittlement of a ferritic steel

Christopher Petersson, Peter Szakalos, Rachel Pettersson, Daniel Dietrich Stein

Abstract

Liquid metal embrittlement (LME) of a Fe-10Cr-4Al ferritic steel was studied at 375°C in liquid Pb-Bi alloys. Slow strain rate testing (SSRT) in low oxygen conditions was used to evaluate the ductility as a function of Bi concentration. It was found that susceptibility to LME increased strongly with the Bi concentration. The steel showed a reduction in its total strain to failure, which started at 3-5 wt.% Bi. The alloying elements (Fe, Cr, and Al) have a higher solubility in Bi than pure lead (Pb), so they are expected to dissolve more readily when Bi is added to the Pb. This is believed to be part of the explanation for the observed increase of LME. Lead with up to 3 wt.% Bi induced no LME in the studied corrosion resistance FeCrAl alloy.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear reactor physics and engineering

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. S. Bortot, "Generation-IV reactors-coolants", 2018.
2. S. Bortot, "Generation-IV Reactors", 2018.
3. "Generation IV Nuclear Reactors". 2020. https://world-nuclear.org/information-library/nuclear-fuel-cycle/nuclear-power-reactors/generation-iv-nuclear-reactors.aspx (accessed 211203, 2021).
4. International Seminar on Liquid Metal Systems: material Behavior Physical Chemistry in Liquid Metal Systems", Liquid metal systems
5. David G. Kolman, "Liquid Metal Induced Embrittlement", 2003. [Online]. Available: https://meridian.allenpress.com/corrosion/article-abstract/75/1/42/199240/A-Review-of-Recent-Advances-in-the-Understanding.10.5006/2904 ↗
6. Environmental degradation of structural materials in liquid lead- and lead-bismuth eutectic-cooled reactors10.1016/j.pmatsci.2022.100920 ↗
7. Corrosion of structural materials by liquid metals used in fusion, fission, and spallation
8. Liquid Metal Embrittlement
9. A review of recent advances in the understanding of liquid metal embrittlement10.5006/2904 ↗
10. Review Liquid metal embrittlement
11. A review of steel corrosion by liquid lead and lead–bismuth10.1016/j.corsci.2009.03.013 ↗
12. Liquid metal embrittlement susceptibility of an oxide-dispersion strengthened FeCrAl alloy in contact with liquid lead-bismuth eutectic at 350 °C
13. Dömstedt · 2021
14. Oxidation studies of Fe10CrAl–RE alloys exposed to Pb at 550 °C for 10,000 h10.1016/j.jnucmat.2013.07.023 ↗
15. Long term corrosion resistance of alumina forming austenitic stainless steels in liquid lead10.1016/j.jnucmat.2015.03.011 ↗
16. J.R.C. European Commission, Hojna, A., Nilsson, K., "Overview of mechanisms & models for liquid metal embrittlement and future directions, Publications Office", 2018. [Online]. Available: https://op.europa.eu/en/publication-detail/-/publication/f640b823-072d-11e9-81b4-01aa75ed71a1/language-en.
17. Influence of liquid lead and lead–bismuth eutectic on tensile, fatigue and creep properties of ferritic/martensitic and austenitic steels for transmutation systems10.1016/j.jnucmat.2011.04.047 ↗
18. Liquid metal embrittlement susceptibility of ferritic–martensitic steel in liquid lead alloys10.1016/j.jnucmat.2008.02.008 ↗
19. T91 cladding tubes with and without modified FeCrAlY coatings exposed in LBE at different flow, stress and temperature conditions10.1016/j.jnucmat.2008.02.026 ↗
20. The role of oxide films in preventing liquid metal embrittlement of T91 steel exposed to liquid lead-bismuth eutectic10.1016/j.jnucmat.2018.07.018 ↗
21. Liquid metal embrittlement sensitivity of the T91 steel in lead, in bismuth and in lead-bismuth eutectic10.1016/j.jnucmat.2020.152021 ↗
22. Liquid metal embrittlement of T91 and 316 L steels by heavy liquid metals: a fracture mechanics assessment10.1016/j.jnucmat.2008.02.043 ↗
23. Temperature effect in the maximum propagation rate of a liquid metal filled crack: the T91 martensitic steel/Lead–Bismuth Eutectic system10.1016/j.corsci.2009.06.049 ↗
24. New alumina-forming steels for future energy production with focus on solar power. [ALSTEr]
25. A comparative study on liquid metal embrittlement susceptibility of three FeCrAl ferritic alloys in contact with liquid lead-bismuth eutectic at 350 °C10.1016/j.corsci.2021.109346 ↗
26. Design of alumina forming FeCrAl steels for lead or lead–bismuth cooled fast reactors10.1016/j.jnucmat.2012.04.006 ↗
27. Development of low-Cr ODS FeCrAl alloys for accident-tolerant fuel cladding10.1016/j.jnucmat.2017.12.035 ↗
28. Effect of temperature on liquid metal embrittlement susceptibility of an Fe10Cr4Al ferritic alloy in contact with stagnant lead-bismuth eutectic10.1016/j.jnucmat.2020.152196 ↗
29. Slow strain rate testing of Fe-10Cr-4Al ferritic steel in liquid lead and lead–bismuth eutectic
30. Z. SGM5. "Oxygen Analyzer SGM5". https://www.zirox.de/en/products/analyzers/oxygen-analyzer-sgm5/ (accessed 2022).
31. Handbook on lead–bismuth eutectic alloy and lead properties, materials compatibility, thermal hydraulics and technologies
32. "Philips XL 30 SEM". https://cmm.centre.uq.edu.au/philips-xl30-sem (accessed 2023, 10-10).
33. "Zeiss 1540XB Crossbeam SEM". https://www.fkf.mpg.de/5670354/Zeiss_CrossBeam (accessed 2023, 10-10).
34. Corrosion of structural materials by liquid metals used fusion, fission and spallation
35. Aluminum- low melting metal alloys
36. Obenchain · Electrochemistry Technology · 1965 · 3 · 221
37. T.R.A. Davey, "Determination of Solubilities in Light Metals", presented at the AIME Met. Soc. Conf., Physical Chemistry of Process Metallurgy, New York, 1961.
38. The Pb-Al Diagram