Oxidation and embrittlement behavior of FeCrAl-ODS cladding tube under loss-of-coolant accident conditions
Source abstract
Abstract
To evaluate the oxidation and embrittlement behavior of an oxide-dispersion-strengthened FeCrAl (FeCrAl-ODS) cladding tube under loss-of-coolant accident (LOCA) conditions, we conducted isothermal oxidation and ring-compression tests on unirradiated, stress-relieved FeCrAl-ODS cladding tube specimens. Further, we discussed the loss of coolable geometry of the reactor core loaded with the FeCrAl-ODS cladding tubes under LOCA conditions, using data from the ring-compression tests in this study and the integral thermal shock tests from our previous study. The results reveal that oxidation kinetics of the FeCrAl-ODS cladding tube at is four orders of magnitude lower than that of a conventional Zircaloy cladding tube, which highlights the exceptional oxidation resistance of the FeCrAl-ODS cladding tube. The breakaway oxidation of the FeCrAl-ODS cladding tube was observed at for durations equal to or exceeding , and melting was observed at . The ring-compression and the integral thermal shock tests indicate that, depending on the oxidation time, the ductile to brittle transition threshold — as determined by the ring-compression test — exists between and . Meanwhile, the fracture threshold — established through the integral thermal shock test — falls between and . Therefore, taking a conservative approach based on available data, the fracture and non-fracture results from the integral thermal shock tests can define the lower and upper boundaries of the threshold for the loss of coolable geometry of the reactor core during a LOCA.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Accident tolerant fuels for LWRs: a perspective10.1016/j.jnucmat.2013.12.005 ↗
2. S. Yamashita, I. Ioka, Y. Nemoto, T. Kawanishi, M. Kurata, Y. Kaji, T. Fukahori, T. Nozawa, D. Sato, N. Murakami, H. Sato, T. Kondo, K. Sakamoto, K. Kusagaya, S. Ukai, A. Kimura, A. Yamaji, Overview of accident-tolerant fuel R&D program in Japan, in: Proc. TopFuel 2019, 2019 Sep. 22–27, Seattle (USA).
3. Development of accident tolerant FeCrAl-ODS fuel cladding for BWRs in Japan10.1016/j.jnucmat.2021.153276 ↗
4. Alloy design and characterization of a recrystallized FeCrAl-ODS cladding for accident-tolerant BWR fuels: an overview of research activity in Japan10.1016/j.jnucmat.2023.154508 ↗
5. Fuel behavior under loss-of-coolant accident situations
6. Meyer · 2014
7. Nagase · 2020
8. Behavior of fuel with zirconium alloy cladding in reactivity-initiated accident and loss-of-coolant accident
9. Overview of Japanese development of accident tolerant FeCrAl-ODS fuel claddings for BWRs
10. K. Sakamoto, Y. Miura, S. Ukai, A. Kimura, A. Yamaji, K. Kusagaya, T. Kondo, S. Yamashita, Progress on Japanese development of accident tolerant FeCrAl-ODS fuel claddings for BWRs, in: Proc. TopFuel 2018, 2018 Sep. 30—Oct. 4, Prague (Czech Republic).
11. K. Sakamoto, Y. Miura, S. Ukai, A. Kimura, A. Yamaji, K. Kusagaya, S. Yamashita, Recent progress in development of accident tolerant FeCrAl-ODS fuel claddings for BWRs in Japan, in: Proc. TopFuel 2019, 2019 Sep. 22–27, Seattle USA,.
12. A study of the oxidation behaviour of FeCrAl-ODS in air and steam environments up to Image 36
13. OECD/NEA · 2011
14. Behavior of FeCrAl-ODS cladding tube under loss-of-coolant accident conditions10.1016/j.jnucmat.2023.154467 ↗
15. 2.07 - zirconium alloys: properties and characteristics
16. Microstructure and texture evolution and ring-tensile properties of recrystallized FeCrAl ODS cladding tubes10.1016/j.msea.2019.138636 ↗
17. Kinetics of low-Sn Zircaloy-4 at the temperature range from 773 to 1,573K10.1080/18811248.2003.9715351 ↗
18. Oxidation mechanism and kinetics of nuclear-grade FeCrAl alloys in the temperature range of 500–Image 37 in steam10.1016/j.jnucmat.2022.153696 ↗
19. Oxidation of Zircaloy-4 under high temperature steam atmosphere and its effect on ductility of cladding10.1080/18811248.1978.9735555 ↗
20. Uetsuka · 1984
21. Oxidation of Zircaloy-4 under limited steam supply from 1,000 to Image 3910.1080/18811248.1986.9735077 ↗
22. Oxidation kinetics and related phenomena of Zircaloy-4 fuel cladding exposed to high temperature steam and hydrogen-steam mixtures under PWR accident conditions10.1016/0029-5493(87)90286-X ↗
23. Nissley · 2005
24. The effect of oxidation-and-quenching process during a LOCA on the behavior of the oxidation and embrittlement of Zircaloy-4 cladding under reheating transients10.1080/00223131.2016.1198730 ↗
25. Influence of composition and heating schedules on compatibility of FeCrAl alloys with high-temperature steam10.1016/j.jnucmat.2018.09.026 ↗
26. High temperature oxidation of fuel cladding candidate materials in steam–hydrogen environments10.1016/j.jnucmat.2013.05.047 ↗
27. The kinetics of oxidation of Zircaloy-4 in steam at high temperatures10.1149/1.2129227 ↗
28. Microstructure and environmental resistance of low Cr ODS FeCrAl10.1179/0960340914Z.00000000088 ↗