journal article·2025-11Open access

Mechanical behaviors of Cr coating on Zircaloy tubes prepared by pulsed laser deposition

Ziqi Wei, Bo Li, Lijuan Cui, John Andrew Kane Jovellana, Zideng Wang, Zongda Yang, Huilong Yang, Sho Kano, Toshiyasu O, Hiroaki Abe

Abstract

Chromium-coated Zircaloy cladding is one promising candidate for accident-tolerant fuel (ATF), yet its mechanical reliability under loading remains insufficiently understood. This study aims to investigate the cracking behavior and fracture resistance of a thin nanocrystalline/amorphous chromium (Cr) coating fabricated by pulsed laser deposition (PLD) under hoop tensile strain. A 350-nm-thick Cr bilayer coating was deposited onto Zircaloy-4 substrates, and its hoop tensile response was evaluated using the advanced expansion due to compression (A-EDC) test. Key mechanical properties, including Young’s modulus (227 GPa), hardness (13.3 GPa), and residual stress (-1450 MPa), were measured by nanoindentation and X-ray diffraction (XRD). Detailed analyses by scanning electron microscopy (SEM) revealed the evolution of transverse and slanted cracks under increasing strain, with a superior first cracking strain of 3.2 %. A crack density-strain relationship was established and used to estimate the fracture strength (5.8 GPa) and interfacial shear strength (980 MPa) via a shear-lag model. The findings highlight the mechanical advantages of the nanocrystalline/amorphous structure, including grain refinement strengthening and the ductile-buffering effect of the amorphous layer. This study provides a new mechanical perspective for advancing the Cr-coated Zircaloy claddings for ATF applications.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (73)

Show source-provided references
1. Accident tolerant fuel cladding development: promise, status, and challenges10.1016/j.jnucmat.2017.12.043 ↗
2. Tensile properties and microstructure of Zr–1.8Nb alloy subjected to 140-MeV C4+ ion irradiation10.1016/j.jnucmat.2017.07.068 ↗
3. Pasamehmetoglu · 2018
4. Reactivity of Zircaloy-4 with Ti3SiC2 and Ti2AlC in the 1100–1300 °C temperature range10.1016/j.jnucmat.2015.02.006 ↗
5. Protective coatings on zirconium-based alloys as accident-tolerant fuel (ATF) claddings10.1515/corrrev-2017-0010 ↗
6. Behavior of an improved Zr fuel cladding with oxidation resistant coating under loss-of-coolant accident conditions10.1016/j.jnucmat.2016.10.021 ↗
7. Characterization of as-deposited cold sprayed Cr-coating on Optimized ZIRLO™ claddings10.1016/j.jnucmat.2021.152892 ↗
8. Development and property evaluation of nuclear grade wrought FeCrAl fuel cladding for light water reactors10.1016/j.jnucmat.2015.10.019 ↗
9. An investigation of FeCrAl cladding behavior under normal operating and loss of coolant conditions10.1016/j.jnucmat.2017.04.039 ↗
10. Chemical compatibility between UO2 fuel and SiC cladding for LWRs
11. Characterization of SiC–SiC composites for accident tolerant fuel cladding10.1016/j.jnucmat.2015.08.020 ↗
12. Recent advances in protective coatings for accident tolerant Zr-Based fuel claddings10.3390/coatings11050557 ↗
13. Early studies on Cr-Coated Zircaloy-4 as enhanced accident tolerant nuclear fuel claddings for light water reactors10.1016/j.jnucmat.2019.02.018 ↗
14. Residual stress and cracking in thin PVD coatings10.1016/S0042-207X(01)00327-X ↗
15. Review on chromium coated zirconium alloy accident tolerant fuel cladding10.1016/j.jallcom.2021.162450 ↗
16. Nested loops explain low irradiation-induced swelling rate10.1016/j.actamat.2024.119700 ↗
17. Improved irradiation resistance of Cr-Fe alloy for Cr-coated Zircaloy application in accident tolerant fuel10.1016/j.scriptamat.2023.115344 ↗
18. TEM characterization of irradiation-induced dislocation loops and voids in ion-irradiated pure chromium10.1016/j.jnucmat.2022.153920 ↗
19. The issue of stress state during mechanical tests to assess cladding performance during a reactivity-initiated accident (RIA)10.1016/j.jnucmat.2011.03.015 ↗
20. W. Beck, P. Blanpain, T. Fuketa, A. Gorzel, Z. Hozer, K. Kamimura, Y.-H. Koo, D. Maertens, O. Nechaeva, M. Petit, Nuclear fuel safety criteria technical review, (2012).
21. Assessment at CEA of coated nuclear fuel cladding for LWRs with increased margins in LOCA and beyond LOCA conditions
22. Adhesion property and high-temperature oxidation behavior of Cr-coated Zircaloy-4 cladding tube prepared by 3D laser coating10.1016/j.jnucmat.2015.06.030 ↗
23. Mechanical testing of neutron irradiated E-ATF chromium-coated Zr-Based claddings
24. Development of advanced expansion due to compression (A-EDC) test method for safety evaluation of degraded nuclear fuel cladding materials10.1080/00223131.2015.1056560 ↗
25. Mechanical properties of zircaloy-4 cladding tube by advanced expansion due to compression (A-EDC) test10.2320/matertrans.ML201601 ↗
26. A comparative study of hydride-induced embrittlement of Zircaloy-4 fuel cladding tubes in the longitudinal and hoop directions10.1080/00223131.2017.1287603 ↗
27. Expansion deformation behavior of zirconium alloy claddings with different hydrogen concentrations10.1016/j.jnucmat.2021.153082 ↗
28. Chromium coatings deposited by cooled and hot target magnetron sputtering for accident tolerant nuclear fuel claddings10.1016/j.surfcoat.2020.125618 ↗
29. Measurement of local mechanical properties for Cr-coated accident tolerant fuel cladding10.1016/j.jnucmat.2023.154407 ↗
30. High temperature Cr-Zr interaction of two types of Cr-coated Zr alloys in inert gas environment10.1016/j.jnucmat.2021.152806 ↗
31. Influences of arc current on microstructure of Cr coating for Zr-4 alloy prepared by multi-arc ion plating via EBSD10.1016/j.matchar.2021.111211 ↗
32. Effect of gas pressure and bias potential on oxidation resistance of Cr coatings10.1016/j.anucene.2019.04.038 ↗
33. Development of Cr cold spray–coated fuel cladding with enhanced accident tolerance10.1016/j.net.2017.12.011 ↗
34. A systematic study of the oxidation behavior of Cr coatings on Zry4 substrates in high temperature steam environment10.1016/j.corsci.2020.108826 ↗
35. Atomic-scale interface structure of a Cr-coated Zircaloy-4 material10.1007/s10853-018-2333-1 ↗
36. Quantifying cracking and strain localisation in a cold spray chromium coating on a zirconium alloy substrate under tensile loading at room temperature10.1016/j.jnucmat.2024.154899 ↗
37. Hall–Petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
38. Grain-boundary strengthening in nanocrystalline chromium and the Hall–Petch coefficient of body-centered cubic metals10.1016/j.scriptamat.2012.09.025 ↗
39. Tuning the microstructure and mechanical properties in nanocrystalline Cr coatings by sputtering power10.1016/j.msea.2022.143204 ↗
40. On the crack propagation and fracture properties of Cr-coated Zr-4 alloys for accident-tolerant fuel cladding: in situ three-point bending test and cohesive zone modeling10.1016/j.surfcoat.2021.127810 ↗
41. Temperature-dependent deformation and cracking behavior in Cr coating for accident tolerant fuel cladding: an in situ SEM study10.1016/j.surfcoat.2021.127815 ↗
42. Mechanical behavior of a chromium coating on a zirconium alloy substrate at room temperature10.1016/j.jnucmat.2021.153332 ↗
43. Thermal stability of the Cr-coated zirconium alloy microstructure prepared by pulsed laser deposition
44. Low-temperature bonding between F82H and Cr assisted by metastable Cr interlayers applied by pulsed laser deposition10.1016/j.fusengdes.2023.113974 ↗
45. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
46. 2007
47. Accurate measurement of thin film mechanical properties using nanoindentation10.1557/s43578-022-00541-1 ↗
48. Modeling of Young's modulus, hardness and stiffness of chromium zigzag multilayers sputter deposited10.1016/j.tsf.2005.12.157 ↗
49. Fitzpatrick · 2005
50. The determination of dislocation densities in thin films10.1080/14786436108239679 ↗
51. Evolution of the F82H/Cr interface after solid-state diffusion bonding below Ac1 temperature: examination of microstructures and hardness10.1016/j.jnucmat.2023.154627 ↗
52. On the microstructures and cracking modes of Cr-coated Zr-4 alloys oxidized and vacuum-annealed at 1000 °C10.1016/j.jallcom.2022.164610 ↗
53. Young's modulus and internal friction in metallic glass alloys from 1.5 to 300 K10.1103/PhysRevB.9.4073 ↗
54. An investigation on synthesis and characterization of superhard Cr-Zr-O coatings10.1016/j.surfcoat.2019.06.102 ↗
55. P.S. Prevéy, X-ray diffraction residual stress techniques, 1986. https://doi.org/10.31399/asm.hb.v10.a0001761.10.31399/asm.hb.v10.a0001761 ↗
56. Evans · 2014 · 187
57. Thermal treatment effect on structural and mechanical properties of Cr–C coatings10.1080/00202967.2018.1424403 ↗
58. Mechanical and thermomechanical properties of commercially pure chromium and chromium alloys10.1016/S0022-3115(01)00745-0 ↗
59. Temperature-dependent nanoindentation and activation volume in high-purity body-centered cubic chromium10.1016/j.msea.2022.143629 ↗
60. Comparative study on the tensile cracking behavior of CrN and Cr coatings for accident-tolerant fuel claddings10.1016/j.surfcoat.2020.126812 ↗
61. An elastic–plastic shear lag model for fracture of layered coatings10.1016/S0040-6090(02)01124-0 ↗
62. In-situ study on the tensile behavior of Cr-coated zircaloy for accident tolerant fuel claddings10.1016/j.surfcoat.2020.125747 ↗
63. Shear band multiplication induced strong strain delocalization and high tensile ductility in amorphous thin films by metallic substrates10.1016/j.ijsolstr.2020.03.011 ↗
64. Molecular dynamics simulation of deformation and failure of nanocrystals of bcc metals10.1016/j.tafmec.2006.02.002 ↗
65. Effect of initial coating crack on the mechanical performance of surface-coated zircaloy cladding10.1016/j.net.2020.09.029 ↗
66. Cracking of thin bonded films in residual tension10.1016/0020-7683(92)90015-L ↗
67. Mechanical behaviour of hard chromium deposited from a trivalent chromium bath10.3390/coatings12030354 ↗
68. Nanomechanics of Hall–Petch relationship in nanocrystalline materials10.1016/j.pmatsci.2009.03.008 ↗
69. Review on superior strength and enhanced ductility of metallic nanomaterials10.1016/j.pmatsci.2018.02.002 ↗
70. Plastic deformation in metallic glasses10.1016/0001-6160(79)90055-5 ↗
71. A practical guide to pulsed laser deposition10.1039/D2CS00938B ↗
72. Eason · 2006
73. Intrinsic stress evolution in laser deposited thin films10.1063/1.1602565 ↗