journal article·2008-02

Evaluation of self-welding susceptibility of an austenitic stainless steel (alloy D9) in sodium

Hemant Kumar, S.K. Albert, V. Ramakrishnan, C. Meikandamurthy, G. Amarendra, A.K. Bhaduri

Journal of Nuclear Materials· Volume 374· Issue 1-2
Publisher page

Abstract

Abstract Self-welding susceptibility of a 15Cr–15Ni–2Mo titanium-modified austenitic stainless steel (alloy D9), in both annealed and 20% cold-worked conditions, have been evaluated in flowing sodium at 823 K for 2160 and 4320 h under contact stress of 9.4 MPa. Tests were performed on flat-on-flat geometry of hollow cylindrical specimens under compression. One pair of 20% cold-worked alloy D9 vs. 20% cold-worked alloy D9 specimens tested for 4320 h was self-welded for which the breakaway shear force was measured. Scanning electron micrographs of the self-welded region showed that portions of the original interface no longer existed. The paper discusses the experimental set-up installed in the sodium loop test facility and the results of self-welding susceptibility studies on this material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (4)

Show source-provided references
1. Chander · Wear · 1993 · 162–164 · 45810.1016/0043-1648(93)90530-Y ↗
2. Yukota · Nucl. Technol. · 1988 · 81 · 40710.13182/NT88-A16061 ↗
3. Agostini · Liquid Metals Technol. Energy Prod. · 1988 · 501 · 1
4. Huber · 1976