journal article·2002-12

Properties of copper–stainless steel HIP joints before and after neutron irradiation

S. Tähtinen, A. Laukkanen, B.N. Singh, P. Toft

Publisher page

Abstract

Abstract The tensile and fracture behaviour of CuCrZr and CuAl25 IG0 alloys joint to 316L(N) stainless steel by hot isostatic pressing (HIP) have been determined in unirradiated and neutron-irradiated conditions. The tensile and fracture behaviour of copper alloy HIP joint specimens are dominated by the properties of the copper alloys, and particularly, by the strength mismatch and mismatch in strain hardening capacities between copper alloys and stainless steel. The test temperature, neutron irradiation and thermal cycles primarily affect the copper alloy HIP joint properties through changing the strength mismatch between the base alloys. Changes in the loading conditions i.e. tensile, bend ( J I ) and mixed-mode bend ( J I / J II ) lead to different fracture modes in the copper alloy HIP joint specimens.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Tähtinen · Fus. Eng. Des. · 2001
2. Tähtinen · 2000 · vol. 3 · 1080
3. Ivanov · J. Nucl. Mater. · 2000 · 283–287 · 3510.1016/S0022-3115(00)00329-9 ↗
4. L. Briottet, P. Bucci, H. Burlet, I. Chu, Note Technique DEM No. 99/26, CEA-CEREM, Crenoble, 1999, p. 32
5. Tähtinen · 2000 · 1241
6. A. Laukkanen, S. Tähtinen, Research report BVAL64-011132, VTT Manufacturing Technology, Espoo, 2001, p. 26
7. S. Tähtinen, M. Pyykkönen, B.N. Singh, P. Toft, Research report VALB-282, VTT Manufacturing Technology, Espoo, 1998, p. 22
8. Pyykkönen · 1998 · 173
9. S. Tähtinen, B.N. Singh, Researh report BVAL62-001030, VTT Manufacturing Technology, Espoo, 2000, p. 14
10. S. Tähtinen, B.N. Singh, Research report BVAL62-001062, VTT Manufacturing Technology, Espoo, 2000, p. 12
11. Tähtinen · J. Nucl. Mater. · 1998 · 258–263 · 101010.1016/S0022-3115(98)00075-0 ↗
12. Tähtinen · J. Nucl. Mater. · 2000 · 283–287 · 123810.1016/S0022-3115(00)00177-X ↗
13. Fabritsiev · J. Nucl. Mater. · 2000 · 283–287 · 52310.1016/S0022-3115(00)00372-X ↗
14. Laukkanen · 2000 · vol. 1 · 103
15. Xu · J. Nucl. Mater. · 2000 · 283–287 · 122910.1016/S0022-3115(00)00175-6 ↗
16. S. Revol, C. Labonne, T. Portra, E. Rigal, Note Technique D.E.M. No. 74/98, CEA-CEREM, Grenoble, 1998, p. 17
17. Hatano · J. Nucl. Mater. · 1998 · 258–263 · 95010.1016/S0022-3115(98)00122-6 ↗