A study on the reaction of Zircaloy-4 tube with hydrogen/steam mixture
Source abstract
Abstract
Abstract In order to fundamentally understand the secondary hydriding mechanism of zirconium alloy cladding, the reaction of commercial Zircaloy-4 tubes with hydrogen and steam mixture was studied using a thermo-gravimetric analyser with two variables, H2/H2O ratio and temperature. Phenomenological analysis revealed that in the steam starvation condition, i.e., when the H2/H2O ratio is greater than 104, hydriding is the dominant reaction and the weight gain increases linearly after a short incubation time. On the other hand, when the gas ratio is 5 × 102 or 103, both hydriding and oxidation reactions take place simultaneously, leading to three distinct regimes: primary hydriding, enhanced oxidation, and massive hydriding. Microstructural changes of oxide demonstrate that when the weight gain exceeds a certain critical value, massive hydriding takes place due to the significant localized crack development within the oxide, which possibly simulates the secondary hydriding failure in a defective fuel operation. This study reveals that the steam starvation condition above the critical H2/H2O ratio is only a necessary condition for the secondary hydriding failure and, as a sufficient condition, oxide needs to grow sufficiently to reach the critical thickness that produces substantial crack development. In other words, in a real defective fuel operation incident, the secondary failure is initiated only when both steam starvation and oxide degradation conditions are simultaneously met. Therefore, it is concluded that the indispensable time for the critical oxide growth primarily determines the triggering time of massive hydriding failure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Nuclear Engineering Thermal-Hydraulics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. The main causes of fuel element failure in water-cooled power reactors
2. Failure of a barrier rod in Oskarshamn 3
3. Post-defect behavior of barrier fuel
4. Olander · 1993
5. Kinetic studies on massive hydriding of commercial zirconium alloy tubing10.1016/S0022-3115(98)00902-7 ↗
6. Evdokimov · 2009 · 193
7. Lewis · 1993 · 79
8. The behaviour of defective reactor fuel10.1016/0029-5493(72)90080-5 ↗
9. Clayton · 1989 · 266
10. Performance of failed BWR fuel
11. Investigation on the post-defect deterioration of nonbarrier BWR failed rods
12. Secondary defect behaviour in ABB BWR fuel
13. Markowitz · 1963
14. High pressure hydriding of sponge-Zr in steam-hydrogen mixtures10.1016/S0022-3115(97)00066-4 ↗
15. Secondary hydriding criteria under irradiation conditions10.1016/j.nucengdes.2011.01.043 ↗
16. Measurements of delayed hydride cracking propagation rate in the radial direction of Zircaloy-2 cladding tubes10.1016/j.jnucmat.2012.04.012 ↗
17. Efsing · 1996 · 394
18. Boyle · 1958
19. Shannon · 1963
20. Gibby · 1965
21. Kinetics of reaction of zirconium alloy with hydrogen10.1016/0022-5088(78)90165-0 ↗
22. Defected zircaloy fuel
23. Hillner · 1977 · 211
24. Bouineau · 2009 · 405
25. Some thoughts on the mechanisms of in-reactor corrosion of zirconium alloys10.1016/j.jnucmat.2004.09.029 ↗
26. The origin of the cubic rate law in zirconium alloy oxidation10.1149/1.2134204 ↗
27. Billot · 1991 · 539
28. ABB-CE experience with high burnup fuel PWR performance
29. Garde · 1991 · 566
30. Cheng · 1996 · 137
31. Blat · 2000 · 563
32. Harada · 2009 · 384
33. Autoclave study of zirconium alloys with and without hydride rim10.1179/1743278212Y.0000000055 ↗
34. Blat · 1996 · 319
35. PWR Zircaloy cladding corrosion behavior: quantitative analyses10.1016/S0022-3115(97)00125-6 ↗
36. The effect of heat treatment on the microstructure and the corrosion resistance of zircaloy-4 in 450°C steam10.1016/0022-3115(85)90027-3 ↗
37. Oxidation kinetics of low-Sn zircaloy-4 at the temperature range from 773 to 1,573K10.1080/18811248.2003.9715351 ↗
38. Measurements of hydrogen permeation and absorption in zirconium oxide scales10.1016/S0022-3115(02)01556-8 ↗
39. A mechanism for the hydrogen uptake process in zirconium alloys10.1016/S0022-3115(98)00492-9 ↗
40. A hydrogen uptake micro-mechanism for Zr alloys10.1016/S0022-3115(98)00898-8 ↗
41. Hydriding of zirconium alloys in hydrogen gas10.1016/0921-5093(93)90519-K ↗
42. Multiple rate transitions in the aqueous corrosion of zircaloy10.1149/1.2425526 ↗
43. Transmission electron microscopy examination of oxide layers formed on Zr alloys10.1016/j.jnucmat.2005.10.012 ↗
44. Zircaloy-4 and M5® high temperature oxidation and nitriding in air10.1016/j.jnucmat.2008.07.002 ↗
45. Preuss · 2011 · 649
46. Detection of breakaway oxidation with acoustic emission during zirconium oxide scale growth10.1007/s11085-012-9355-x ↗
47. Residual stresses and tetragonal phase fraction characterisation of corrosion tested zircaloy-4 using energy dispersive synchrotron X-ray diffraction10.1016/j.jnucmat.2012.07.025 ↗
48. In situ high temperature oxidation analysis of zircaloy-4 using acoustic emission coupled with thermogravimetry10.1016/j.jnucmat.2015.03.014 ↗