journal article·2012-08

D retention in C- and O-contaminated tungsten during D+ irradiation

J.P. Roszell, A.J. Labelle, P. Brodersen, J.W. Davis, A.A. Haasz

Journal of Nuclear Materials· Volume 427· Issue 1-3
Publisher page

Abstract

Abstract Deuterium retention during 10 eV and 500 eV/D + irradiations at 300 and 500 K was compared for 99.96% pure polycrystalline tungsten (PCW) foils and similar PCW foils contaminated with carbon and oxygen impurities. The contaminated foils showed reduced deuterium retention at 500 K compared with pure foil specimens while there was no difference for 300 K irradiations. X-ray photoelectron spectroscopy (XPS) and secondary ion mass spectroscopy (SIMS) of the unirradiated specimens showed regions of highly localised, non-homogeneous C and O contamination as well as a broader region of low level contamination of about 1–10% areal coverage. It is hypothesised that the C/O contamination creates a diffusion barrier in the PCW foil preventing deuterium from diffusing from the near surface into the bulk, thus reducing overall D retention at 500 K. This finding has implications for tritium retention in ITER; if carbon contamination even at low levels can impede T diffusion into the bulk it would mean reduced T loading in W plasma-facing components.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Nuclear Materials and Properties · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Skinner · Fusion Sci. Technol. · 2008 · 54 · 89110.13182/FST54-891 ↗
2. ITER Plant Description Document, Safety; Document No. G A0 FDR 1 01-07-13 545 R1.0, 2001 (Chapter 5).
3. Ueda · Nucl. Fusion · 2004 · 44 · 6210.1088/0029-5515/44/1/007 ↗
4. Kawakami · Jpn. J. Appl. Phys. · 2003 · 42 · 752910.1143/JJAP.42.7529 ↗
5. Bizyukov · J. Nucl. Mater. · 2010 · 400 · 24510.1016/j.jnucmat.2010.03.010 ↗
6. Wang · J. Nucl. Mater. · 1997 · 241 · 108710.1016/S0022-3115(97)80199-7 ↗
7. Kobayashi · Phys. Scr. · 2009 · T138 · 01405010.1088/0031-8949/2009/T138/014050 ↗
8. Alimov · J. Nucl. Mater. · 2008 · 375 · 19210.1016/j.jnucmat.2008.01.008 ↗
9. Anderl · J. Nucl. Mater. · 2001 · 290–293 · 3810.1016/S0022-3115(00)00622-X ↗
10. Poon · J. Nucl. Mater. · 2000 · 283 · 106210.1016/S0022-3115(00)00167-7 ↗
11. Alimov · Phys. Scr. · 2004 · T108 · 4610.1238/Physica.Topical.108a00046 ↗
12. Matsunami · J. Nucl. Mater. · 2009 · 390–91 · 69310.1016/j.jnucmat.2009.01.191 ↗
13. Alimov · J. Nucl. Mater. · 2011 · 409 · 2710.1016/j.jnucmat.2010.12.028 ↗
14. A.J.R.R. Labelle, The Effects of Helium on Deuterium Retention in Tungsten Under Simultaneous Irradiation, MSc thesis, University of Toronto, 2011.
15. J.P. Roszell, The Effect of Ion Energy and Substrate Temperature on Deuterium Trapping in Tungsten, PhD thesis, University of Toronto, 2012.
16. Haasz · Nucl. Instrum. Methods Phys. Res., Sect. B · 1993 · 83 · 11710.1016/0168-583X(93)95915-R ↗
17. Mech · J. Nucl. Mater. · 1997 · 241 · 114710.1016/S0022-3115(96)00689-7 ↗
18. Http://Srdata.Nist.Gov/Xps/ElmSpectralSrch.Aspx?selEnergy=PE (2000).
19. Haasz · J. Nucl. Mater. · 1998 · 258–263 · 88910.1016/S0022-3115(98)00072-5 ↗
20. Lee · J. Nucl. Mater. · 2007 · 363–365 · 89810.1016/j.jnucmat.2007.01.111 ↗
21. Lee · J. Nucl. Mater. · 2007 · 360 · 19610.1016/j.jnucmat.2006.09.013 ↗
22. Roszell · J. Nucl. Mater. · 2011 · 415 · S64110.1016/j.jnucmat.2010.12.013 ↗
23. Enomoto · J. Nucl. Mater. · 2009 · 385 · 60610.1016/j.jnucmat.2009.01.298 ↗