journal article·2008-05

Fatigue testing of metallurgically-bonded EBR-II superheater tubes

T.C. Totemeier, D.M. Wachs, D.L. Porter, N. Kisohara

Journal of Nuclear Materials· Volume 376· Issue 1
Publisher page

Abstract

Fatigue crack growth tests were performed on 2¼Cr-1Mo steel specimens machined from ex-service Experimental Breeder Reactor – II (EBR-II) superheater duplex tubes. The tubes had been metallurgically bonded with a 100 µm thick Ni interlayer; the specimens incorporated this bond layer. Tests were performed at room temperature in air and at 400°C in air and humid Ar; cracks were grown at varied levels of constant ?K. Crack growth tests at a range of ?K were also performed on specimens machined from the shell of the superheater. In all conditions the presence of the Ni interlayer was found to result in a net retardation of growth as the crack passed through the interlayer. The mechanism of retardation was identified as a disruption of crack planarity and uniformity after passing through the porous interlayer. Full crack arrest was only observed in a single test performed at near-threshold ?K level (12 MPa?m) at 400°C. In this case the crack tip was blunted by oxidation of the base steel at the steel-interlayer interface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metallurgical and Alloy Processes · Intermetallics and Advanced Alloy Properties · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. H.W. Buschman, W.H. Penney, M.D. Quilici, W.H. Radke, in: Proceedings of the Joint ASME/IEEE Power Generation Conference, 4–8 October 1981, St. Louis, MO (available from ASME).
2. W.H. Penney, H.W. Buschman, R.A. Washburn, Disassembly and Phase I Examination of EBR-II Superheater SU-712, Argonne National Laboratory Report ANL-82-16, 1982.
3. K.J. Longua, D.L. Porter, R.G. Pahl, J.A. Buzzel, G.D. Hudman, Materials Examinations of the Components of EBR-II Superheater SU-712, Argonne National Laboratory Report ANL-83-103, 1984.
4. J.M. Holt, H. Mindlin, C.Y. Ho (Eds.), Structural Alloys Handbook, 1996 Ed., CINDAS/Purdue University, 1997.
5. Longua · Trans. ANS · 1981 · 38 · 321
6. D.M. Wachs, D.D. Keiser, D.L. Porter, N. Kisohara, Nucl. Technol., submitted for publication.
7. Y. Tomita, T. Kosugi, J. Kubota, K. Nakajima, T. Tsuchiya, Liquid Metal Engineering and Technology, Paper 145, BNES, London, 1984, p. 189.
8. K. Roko, K. Takitani, A. Yoshizaki, M. Shiraha, in: Sixth International Heat Transfer Conference, Toronto, 1978, p. 429.10.1615/IHTC6.830 ↗
9. T.C. Totemeier, Fatigue testing of metallurgically-bonded EBR-II superheater tubes, Idaho National Laboratory Report INL/EXT-06-12011, 2006.10.2172/911861 ↗
10. Suresh · 1991
11. 2004 · 11
12. Uhlig · 1985