journal article·2018-11

Grout durability within miniaturised Intermediate Level Waste drums at early stages of interior volume expansion induced by encapsulated metallic corrosion

C. Paraskevoulakos, K.R. Hallam, T.B. Scott

Publisher page

Abstract

Abstract In the UK, the typical route being followed to handle metallic Intermediate Level Waste (ILW) derived from decladding of irradiated nuclear fuel is to primarily deposit it within stainless steel drums/boxes and subsequently encapsulate it into grout. Thus, a monolithic bond between the waste and the encapsulants can be achieved. However, recent inspections have revealed bulges around the circumference in a considerable proportion of the inspected packages. This distortion has been ascribed to the interior metallic corrosion–induced volume expansion, occurring throughout the waste packages storage period. Throughout this period, the volume expansion taking place in the core of the ILW drums has imposed continuously growing levels of strain on the surrounding encapsulants, i.e. grout and steel confinement. As a result, the encapsulants may exhibit considerable damage, in the form of cracks in the grout or/and steel distortion, threatening the integrity of the packages and, consequently, raising safety concerns within the nuclear community. Herein, experimental work performed on ILW drum–simulant packages is described, attempting to evaluate the performance of the packages under an internal corrosion–induced volume expansion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Concrete Corrosion and Durability · Nuclear Materials and Properties · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. Wilson · 1996
2. ILW Treatment and Storage | Sellafield Ltd. http://www.sellafieldsites.com/solution/waste-management/ilw-treatment-and-storage/(Accessed 13 May 2017).
3. Properties of cement systems containing intermediate level wastes10.1016/0008-8846(92)90072-4 ↗
4. Stitt · 2015
5. Ojovan · 2014
6. The preparation of Mg-based hydro-reactive materials and their reactive properties in seawater10.1016/j.ijhydene.2011.02.108 ↗
7. Susceptibility to corrosion of aluminium alloy components in ethanol adsorption chiller10.1016/j.renene.2016.08.042 ↗
8. Nuclear waste viewed in a new light; a synchrotron study of uranium encapsulated in grout10.1016/j.jhazmat.2014.11.035 ↗
9. Pyrophoric behaviour of uranium hydride and uranium powders10.1016/j.jnucmat.2009.11.007 ↗
10. Characterization of uranium corrosion products involved in a uranium hydride pyrophoric event10.1016/S0022-3115(99)00245-7 ↗
11. Cronin · 2011
12. Factors controlling cracking of concrete affected by reinforcement corrosion10.1007/BF02480466 ↗
13. Effect of corrosion on reinforcement bond strength
14. Bond characteristics of corroding reinforcement in concrete beams10.1007/BF02479434 ↗
15. On the penetration of corrosion products from reinforcing steel into concrete due to chloride-induced corrosion10.1016/j.corsci.2010.03.025 ↗
16. Critical thickness of rust layer at inner and out surface cracking of concrete cover in reinforced concrete structures10.1016/j.corsci.2012.03.018 ↗
17. Cover cracking as a function of bar corrosion: Part I-Experimental test10.1007/BF02472805 ↗
18. Corrosion reinforcement and service life of concrete structures
19. Distribution of millscale on corroded steel bars and penetration of steel corrosion products in concrete10.1016/j.corsci.2012.09.014 ↗
20. Modeling of corrosion-induced concrete cover cracking: a critical analysis10.1016/j.conbuildmat.2013.01.019 ↗
21. Gonnerman · 1928
22. The kinetics of the hydriding of uranium metal10.1016/0022-5088(91)90439-B ↗
23. Real time, in-situ deuteriding of uranium encapsulated in grout; effects of temperature on the uranium-deuterium reaction10.1016/j.corsci.2017.08.016 ↗
24. Effects of gas phaseimpurities on the topochemical-kinetic behaviour of uranium hydride development10.1016/0022-5088(88)90019-7 ↗
25. An investigation on the persistence of uranium hydride during storage of simulant nuclear waste packages10.1371/journal.pone.0132284 ↗
26. Properties of concrete containing ground granulated blast furnace slag (GGBFS) at elevated temperatures10.1016/j.jare.2011.03.004 ↗
27. Effect of ground granulate blast-furnace slag on corrosion performance of steel embedded in concrete10.1016/j.matdes.2010.01.057 ↗
28. Dodds · 2012
29. The nature of C-S-H in hardened cements10.1016/S0008-8846(99)00168-4 ↗
30. A model for prediction of time from corrosion initiation to corrosion cracking10.1016/j.cemconcomp.2006.11.004 ↗
31. Modeling the time-to-corrosion cracking in chloride contaminated reinforced concrete structures
32. Prediction of corrosion-induced cover cracking in reinforced concrete structures10.1016/j.conbuildmat.2010.11.074 ↗