Abstract

Abstract Recent evidence has shown that tokamak carbon-based codeposits may become partially or fully depleted of hydrogen through thermo-oxidation, as the hydrogen content of the codeposits is removed more rapidly than the carbon content. In this study we examine the ability of such partially-depleted residual DIII-D divertor codeposits to uptake deuterium upon subsequent exposure to deuterium gas or deuterium plasmas. The partially D-depleted specimens used here were obtained from a previous study where DIII-D codeposits were oxidized for 2 h at 623 K (350 °C) and 267 Pa (2 Torr) O 2 [J.W. Davis et al., Thermo-oxidation of DIII-D codeposits on open surfaces and in simulated tile gaps, J. Nucl. Mater. 415 (2011) S789–S792]. In the present study some of these specimens, having undergone prior oxidation, were exposed to D 2 glow discharge plasmas or D 2 gas at 20 kPa (150 Torr) at 300 or 523 K. In the case of plasma exposure, no uptake of D was observed, while an increase in D content was seen following D 2 gas exposures. When the gas exposure took place at 300 K, heating the specimens in vacuum to 623 K for 15 min led to the release of all of the increased D content. For the gas exposure at 523 K, the increase in D content was found to require longer (8 h) vacuum baking to remove. However, in a reference codeposit specimen (from a closeby location on the tile), which had not been previously oxidized, there was a similar increase in D content following D 2 exposure at 523 K, but it could not be released even following 8 h vacuum baking at 623 K.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fusion materials and technologies · Magnetic confinement fusion research · Nuclear Materials and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (10)

Show source-provided references
1. J.W. Davis, S.L. Allen, B.W.N. Fitzpatrick et al., The effect of thermo-oxidation on plasma performance and in-vessel components in DIII-D, in preparation.
2. Davis · J. Nucl. Mater. · 2011 · 415 · S78910.1016/j.jnucmat.2010.11.019 ↗
3. Wampler · J. Nucl. Mater. · 2007 · 363 · 7210.1016/j.jnucmat.2006.12.038 ↗
4. W.R. Wampler et al., Ion beam analysis of 13C and deuterium deposition in DIII-D and their removal by in situ oxygen bake, in: Proceedings of the 13th International Workshop on Plasma-Facing Materials and Components for Fusion Applications, Rosenheim, Germany 9–13 May 2011, Physica Scripta, submitted for publication.
5. Davis · J. Nucl. Mater. · 2009 · 390 · 53210.1016/j.jnucmat.2009.01.084 ↗
6. Wang · J. Nucl. Mater. · 1997 · 245 · 6610.1016/S0022-3115(96)00745-3 ↗
7. Tsui · Nucl. Fusion · 2008 · 48 · 03500810.1088/0029-5515/48/3/035008 ↗
8. Wampler · J. Nucl. Mater. · 2005 · 337 · 13410.1016/j.jnucmat.2004.10.124 ↗
9. Davis · J. Nucl. Mater. · 1999 · 266 · 47810.1016/S0022-3115(98)00515-7 ↗
10. Haasz · J. Nucl. Mater. · 2009 · 390 · 62610.1016/j.jnucmat.2009.01.303 ↗