journal article·2023-01Open access

Reply to S. Wang's comments (Journal of Nuclear Materials 570 (2022) 153952) on short communication of G.A. McRae and C.E. Coleman published in Journal of Nuclear Materials 568 (2022) 153889

G.A. McRae, C.E. Coleman

Abstract

Helium (He) isotope exchange in tungsten (W) during sequential irradiation by 3 keV 4He and 3He ions at room (RT) and elevated temperatures (700-1200 K) was investigated. The total He fluence was in the range of 5 × 1021–1.8 × 1022 He/m2 to provide a saturation of the surface layer. The amount of He retained in W after irradiation was measured using in-situ (up to 1500 K) and ex-situ (up to 2500 K) thermal desorption spectroscopy (TDS). Air exposure influenced TDS spectra, but clear were no noticeable differences between 3He and 4He TDS spectra after single irradiation. Subsequent irradiation with different He isotopes demonstrated a very efficient isotope exchange already at room temperature. The substitution of He atoms goes even faster with increasing irradiation temperature. Mechanisms of observed processes are discussed on the base of a simple model.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Nuclear Physics and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (5)

Show source-provided references
1. On the origin of the hydride precipitation-dissolution hysteresis in zirconium: Comments on Short Communication of G.A. McRae and C.E. Coleman published in Journal of Nuclear Materials 568 (2022) 15388910.1016/j.jnucmat.2022.153952 ↗
2. Rival interpretations of hydride precipitation-dissolution hysteresis in zirconium: rebuttal to critical comments to the letter to the editor of G.A. McRae and C.E. Coleman published in Journal of Nuclear Materials 556 (2021) 15316910.1016/j.jnucmat.2022.153889 ↗
3. The influence of alloying elements on the terminal solubility of hydrogen in α-zirconium”10.1016/0022-3115(64)90046-7 ↗
4. The Zr α-phase/(α-phase + hydride) transformation should obey the Phase Rule10.1016/j.jnucmat.2021.153169 ↗
5. Cottrell · 1953