journal article·2013-06

Strength loss in MA-MOX green pellets from radiation damage to binders

Paul A. Lessing, W. Roger Cannon, Gerald W. Egeland, Larry D. Zuck, James K. Jewell, Douglas W. Akers, Gary S. Groenewold

Journal of Nuclear Materials· Volume 437· Issue 1-3
Publisher page

Abstract

Abstract The fracture strength of green Minor Actinides (MA)-MOX pellets containing 75 wt.% DUO2, 20 wt.% PuO2, 3 wt.% AmO2 and 2 wt.% NpO2 was studied as a function of storage time, after mixing with the binder and before sintering, to test the effect of radiation damage on binders. Fracture strength degraded continuously over the 10 days of the study for all three binders studied: PEG binder (Carbowax 8000), microcrystalline wax (Mobilcer X) and styrene–acrylic copolymer (Duramax B1022) but the fracture strength of Duramax B1022 degraded the least. For instance, for several hours after mixing Carbowax 8000 with MA-MOX, the fracture strength of a pellet was reasonably high and pellets were easily handled without breaking but the pellets were too weak to handle after 10 days. Strength measured using diametral compression test showed that strength degradation was more rapid in pellets containing 1.0 wt.% Carbowax PEG 8000 compared to those containing only 0.2 wt.%, suggesting that irradiation not only left the binder less effective but also reduced the pellet strength. In contrast the strength of pellets containing Duramax B1022 degraded very little over the 10 days period. It was suggested that the styrene portion present in the Duramax B1022 copolymer provided the radiation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Nuclear Materials and Properties · Fusion materials and technologies · Orthopaedic implants and arthroplasty

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Warin · J. Nucl. Sci. Technol. · 2007 · 44 · 41010.1080/18811248.2007.9711302 ↗
2. Warin · Trans. Am. Nucl. Soc. · 2010 · 103 · 155
3. Magill · Nucl. Energy · 2003 · 42 · 263
4. Borell · Eur. Nucl. Soc. · 2006 · 2006 · 100
5. Neuman · J. Nucl. Mater. · 2009 · 385 · 16810.1016/j.jnucmat.2008.10.021 ↗
6. Egeland · J. Nucl. Mater. · 2010 · 406 · 20510.1016/j.jnucmat.2010.08.022 ↗
7. Nayak · J. Mater. Sci.: Mater. Med. · 2008 · 19 · 2437
8. Wachtman · 2008
9. Fink · 2004
10. Ziegler · 2008
11. Wu · Am. Ceram. Soc. Bull. · 1997 · 76 · 49
12. Cannon · J. Am. Ceram. Soc. · 2012 · 95 · 295710.1111/j.1551-2916.2012.05369.x ↗
13. Groenewold · Nucl. Instrum. Meth. B · 2013 · 296 · 4110.1016/j.nimb.2012.11.017 ↗
14. Technical Data Sheet, Crystal Inc.-PMC.
15. Kazanjian · 1976
16. Reed · 1988
17. Radiation resistance of polymers and composites