Reaction between molten 316 L stainless steel and Zircaloy–4 at 1450 ℃ during a core melt accident of LWR
Source abstract
Abstract
• Oxide layers on Zircaloy suppress Zr dissolution into molten stainless steel. • Secondary oxides form at the interface due to oxygen enrichment in Zr. • A product layer with Laves phase grows between oxide layers over time. • Zr dissolution rate is modeled by time and oxide thickness. • Secondary oxide layers form rapidly and remain stable during reaction. Regarding the interaction between Zircaloy and stainless steel in the accidental conditions of light water reactors, the detailed mechanism of the eutectic liquefaction has been widely studied. However, there are seldom data on the interaction between the surface-oxidized Zircaloy and molten stainless steel, which could happen in several potential accident scenarios. The dissolution reaction rate of Zr from the surface-oxidized Zircaloy into the molten SS316L was experimentally evaluated at 1450 °C. The amount of Zr transferred externally by the Zircaloy–SS316L reaction can be formulated as m ( x , t ) A = ( − 0.0002 x + 0.115 ) · { ln ( t + 0.759 ) + 0.275 } [ g / cm 2 ] , where m ( x,t ), A, x , and t represent the amount of transferred Zr [g], reaction area [cm 2 ], thickness of oxide film on Zircaloy surface [µm], and reaction time [min], respectively.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Nuclear Materials and Properties · Iron and Steelmaking Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. TEPCO, Fukushima Daiichi Decommissioning, https://www.tepco.co.jp/decommission/index-j.html, (accessed 2025 May 14).
2. The results of the CLADS-MADE-03 BWR bundle degradation test in steam under 1F Unit 1 postulated conditions10.1016/j.nucengdes.2023.112729 ↗
3. Reactor core materials interactions at very high temperatures10.13182/NT-TMI2-146 ↗
4. Overview of the facility and experiments performed in Phébus FP10.1016/j.anucene.2013.03.040 ↗
5. Study of boron behaviour in the primary circuit of water reactors under severe accident conditions: a comparison of Phebus FPT3 results with other recent integral and separate-effects data10.1016/j.nucengdes.2011.08.031 ↗
6. BWR lower head penetration failure test focusing on eutectic melting10.1016/j.anucene.2022.109129 ↗
7. A BWR control blade degradation observed in situ during a CLADS-MADE-02 test under Fukushima Dai-Ichi Unit 3 postulated conditions10.1080/00223131.2021.1906777 ↗
8. Modelling of the interactions between B4C and stainless steel at high temperatures10.1016/0022-3115(95)00094-1 ↗
9. Reaction between B4C and austenitic stainless steel in oxidizing atmosphere at temperatures below 1673 K10.1016/j.jnucmat.2015.07.015 ↗
10. Solidification and re-melting mechanisms of SUS-B4C eutectic mixture10.1016/j.jnucmat.2020.152527 ↗
11. Reaction behavior of molten 316L stainless steel with B4C at 1450°C during a core melt accident of BWR10.1016/j.jnucmat.2025.155705 ↗
12. Interaction between B4C, 304 stainless steel, and Zircaloy-4 in H2O/H2 atmosphere at 1473 K10.1080/00223131.2017.1403388 ↗
13. High temperature reaction of multiple eutectic-component system: The case of solid metallic Zr and molten stainless steel-B4C
14. Oxidation of solidified SS304-B4C melt under high-temperature steam10.1016/j.anucene.2023.109724 ↗
15. Dissolution behavior of solid stainless steel by its molten eutectic mixture with B4C under dynamic condition10.1016/j.pnucene.2019.103094 ↗
16. Reaction behavior between B4C, 304 grade of stainless steel and Zircaloy at 1473 K10.1016/j.jnucmat.2016.04.049 ↗
17. Chemical interactions between pre-oxidized Zircaloy-4 and 304 stainless steel-B4C melt at 1300 °C10.1016/j.jnucmat.2018.05.057 ↗
18. The release behavior of boron and silicon from degraded absorber rods on core degradation during BWR severe accident10.1016/j.jnucmat.2018.11.001 ↗
19. Effect of B4C addition on the solidus and liquidus temperatures, density and surface tension of type 316 austenitic stainless steel in the liquid state10.1016/j.jnucmat.2021.153100 ↗
20. Oxidation of solidified SS304-B4C melt under high-temperature steam10.1016/j.anucene.2023.109724 ↗
21. Experimental investigation of nonisothermal interaction between Fe-Zr melt and stainless steel forming “metallic debris” in Fukushima Daiichi Nuclear Power Station10.1016/j.anucene.2025.111333 ↗
22. Summary of TMI-2 core sample examinations10.1016/0029-5493(90)90045-Y ↗
23. Olsen
24. TEPCO, Progress of the accident at each reactor unit during the Fukushima Daiichi Nuclear Power Station accident, and the status of the reactor, containment vessel, and fuel debris, https://www.aec.go.jp/kaigi/teirei/2024/siryo11/1_haifu.pdf, (accessed 2025 August 10).
25. Oxidation behaviour of Zr-1.7Sn-2.3Hf alloy in nitrogen-containing steam at 1200 °C10.1016/j.corsci.2018.05.029 ↗
26. Oxidation kinetics and related phenomena of zircaloy-4 fuel cladding exposed to high temperature steam and hydrogen-steam mixtures under PWR accident conditions10.1016/0029-5493(87)90286-X ↗
27. The Kinetics of Oxidation of Zircaloy-4 in Steam at High Temperatures10.1149/1.2129227 ↗
28. Oxidation reaction kinetics of Zircaloy-4 in an unlimited steam environment10.1016/0022-3115(76)90017-9 ↗
29. FactSage thermochemical software and databases, 2010–201610.1016/j.calphad.2016.05.002 ↗
30. Hino · 2010
31. The O−Zr (Oxygen-Zirconium) system10.1007/BF02881546 ↗