Protective Al-rich oxide scale formation in low-Cr alumina-forming martensitic steels under liquid lead corrosion
Source abstract
Abstract
Two alumina-forming martensitic (AFM) steels containing less than 8 wt.% Cr were exposed for over 1000 h at 550°C and 650°C in static liquid Pb with controlled oxygen concentration to evaluate the formation of an alumina oxide scale and its protective capacity against corrosion. The AFM-1 steel (3.6 wt.% Al, 7.8 wt.% Cr) formed a continuous, protective oxide scale that effectively resisted Pb penetration under all conditions, particularly at 650°C, where performance improved due to the dissolution of B2-NiAl precipitates during prolonged exposure, releasing Al that migrated to the surface and enabled the formation of an Al-rich oxide layer, ensuring sustained protection and mitigating the localized nodular oxidation observed at 550 °C. In contrast, the AFM-2 steel (2.9 wt.% Al, 7.5 wt.% Cr) failed to develop a complete protective oxide layer, allowing molten Pb to penetrate and react with the substrate even at 650 °C, causing severe oxidation. These results demonstrate that, beyond a high Ni content (12 wt.%), achieving excellent corrosion resistance in liquid Pb requires a synergistic combination of an optimal Al/Cr balance, dissolution of B2-NiAl precipitates as an Al source, and enhanced atomic diffusion facilitated by the high density of subgrain boundaries in the martensitic microstructure.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · High-Temperature Coating Behaviors · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (60)
Show source-provided references
1. Ferritic/martensitic steels for next-generation reactors10.1016/j.jnucmat.2007.05.005 ↗
2. Overview of reactor systems and operational environments for structural materials in gen-iv fission reactors
3. Materials for high temperature liquid lead storage for concentrated solar power (Csp) air tower systems10.3390/ma14123261 ↗
4. Worldwide status of advanced reactors (GEN IV) research and technology development
5. Materials compatibility for the next generation of concentrated Solar Power plants10.1016/j.ensm.2018.02.023 ↗
6. K.H. Mayer, F. Masuyama, The development of creep-resistant steels, in: Creep-Resistant Steels, Elsevier Ltd., 2008: pp. 15–77. https://doi.org/10.1533/9781845694012.1.15.10.1533/9781845694012.1.15 ↗
7. A-USC programs in the European union, in: materials for ultra-supercritical and advanced ultra-supercritical power plants
8. A review: ferritic-martensitic steels – treatment
9. Advances in physical metallurgy and processing of steels. strengthening mechanisms of creep resistant tempered martensitic steel10.2355/isijinternational.41.641 ↗
10. Structural materials for Gen-IV nuclear reactors: Challenges and opportunities10.1016/j.jnucmat.2008.08.044 ↗
11. Sodium fast reactor evaluation: Core materials10.1016/j.jnucmat.2009.03.021 ↗
12. Analysis of creep crack growth behavior of P92 steel welded joint by experiment and numerical simulation10.1016/j.msea.2012.07.094 ↗
13. Advances in physical metallurgy and processing of steels. history of power plants and progress in heat resistant steels10.2355/isijinternational.41.612 ↗
14. Void swelling in ferritic-martensitic steels under high dose ion irradiation: Exploring possible contributions to swelling resistance10.1016/j.scriptamat.2015.08.032 ↗
15. Comparison of swelling and irradiation creep behavior of fcc-austenitic and bcc-ferritic/martensitic alloys at high neutron exposure10.1016/S0022-3115(99)00225-1 ↗
16. Improved oxidation resistance of ferritic - martensitic steels in water vapour containing environments via diffusion coatings10.3184/096034012X13315446390033 ↗
17. Ferritic-martensitic steels: Improvement of the oxidation behavior in steam environments via diffusion coatings10.1016/j.surfcoat.2013.09.018 ↗
18. Influence of surface state on the corrosion behavior of si-reinforced f/m steels under solid-phase oxygen-controlled static liquid LBE environment
19. New insights into oxidation mechanism and kinetics of 9Cr–1Mo ferritic-martensitic steel in oxygen-saturated liquid lead-bismuth eutectic10.1016/j.jallcom.2024.174825 ↗
20. Corrosion of ferritic and ferritic-martensitic steels in NaCl-KCl-VCl 2 melts10.1149/05011.0699ecst ↗
21. Investigation on oxygen controlled liquid lead corrosion of surface treated steels10.1016/S0022-3115(99)00211-1 ↗
22. Control of oxygen concentration in liquid lead and lead-bismuth10.1016/S0022-3115(03)00250-2 ↗
23. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
24. C. Fazio, V.P. Sobolev, A. Aerts, S. Gavrilov, K. Lambrinou, P. Schuurmans, A. Gessi, P. Agostini, A. Ciampichetti, L. Martinelli, S. Gosse, F. Balbaud-Celerier, J.L. Courouau, A. Terlain, N. Li, H. Glasbrenner, J. Neuhausen, S. Heinitz, L. Zanini, Y. Dai, M. Jolkkonen, Y. Kurata, T. Obara, N. Thiolliere, F.J. Martin-Munoz, A. Heinzel, A. Weisenburger, G. Mueller, G. Schumacher, A. Jianu, J. Pacio, L. Marocco, R. Stieglitz, T. Wetzel, M. Daubner, K. Litfin, J.B. Vogt, I. Proriol-Serre, D. Gorse, S. Eckert, F. Stefani, D. Buchenau, T. Wondrak, I.S. Hwang, NEA (2024), Handbook on lead-bismuth eutectic alloy and lead properties, Materials Compatibility, Thermal-hydraulics and Technologies, 2015 Edition, OECD Publishing, Paris, 2015. www.oecd.org/publishing/corrigenda.
25. Y. Yamamoto, M.P. Brady, Z.P. Lu, P.J. Maziasz, C.T. Liu, B.A. Pint, K.L. More, H.M. Meyer, E.A. Payzant, Creep-resistant, Al 2 O 3 -forming austenitic stainless steels, Science (1979) 316 (2007) 433–436. https://doi.org/10.1126/science.1137711.10.1126/science.1137711 ↗
26. Alumina-forming austenitic alloys for advanced recuperators
27. L. Liu, C. Fan, H. Sun, F. Chen, J. Guo, T. Huang, Research progress of alumina-forming austenitic stainless steels: a review, Materials 15 (2022). https://doi.org/10.3390/ma15103515.10.3390/ma15103515 ↗
28. Evaluating candidate materials for balance of plant components in SOFC: Oxidation and Cr evaporation properties10.1016/j.corsci.2021.109671 ↗
29. T.S. Chester, S.S. Norman, C.H. William, Superalloys II, High Temperature Materials for Aerospace and Industrial Power (1987).
30. Diffusion studies in oxides scales grown on alumina-and chromia-forming alloys10.1016/S1359-6462(97)00167-X ↗
31. Self-diffusion in α-Al2O3 and growth rate of alumina scales formed by oxidation: effect of Y2O3 doping10.1007/BF00352151 ↗
32. Composition, microstructure, and water vapor effects on internal/external oxidation of alumina-forming austenitic stainless steels10.1007/s11085-009-9161-2 ↗
33. Y. Yamamoto, Q.Q. Ren, M.P. Brady, Role of Cr Content in Microstructure, Creep, and Oxidation Resistance of Alumina-Forming Austenitic Alloys at 850–900°C, Metals 12 (2022). https://doi.org/10.3390/met12050717.10.3390/met12050717 ↗
34. The effect of water vapor on the initial stages of oxidation of the FeCrAl alloy kanthal AF at 900°C10.1007/s11085-007-9055-0 ↗
35. Effect of water vapor on the oxide growth in FeCrAl-based oxide dispersion-strengthened fuel cladding material at 1100 °C and 1200 °C
36. K. Lindgren, P. Dömstedt, P. Szakalos, M. Thuvander, The Nanostructure of the Oxide Formed on Fe–10Cr–4Al Exposed in Liquid Pb, Microsc. Microanal. 28 (2022) 1321–1334. https://doi.org/10.1017/S1431927621000337.10.1017/S1431927621000337 ↗
37. Design of alumina forming FeCrAl steels for lead or lead-bismuth cooled fast reactors10.1016/j.jnucmat.2012.04.006 ↗
38. Oxidation studies of Fe10CrAl-RE alloys exposed to Pb at 550 C for 10,000 h10.1016/j.jnucmat.2013.07.023 ↗
39. Optimizing the oxidation properties of FeCrAl alloys at low temperatures10.1007/s11085-017-9718-4 ↗
40. Factors affecting the high temperature performance of creep strength enhanced ferritic steels
41. The influence of alloying elements on the development and maintenance of protective scales10.1007/BF01046725 ↗
42. The oxidation of high-purity iron-chromium-aluminum alloys at 800°C10.1007/BF00662042 ↗
43. The Effect of the Third Element Cr on Oxidation Behavior of Fe-xCr-10Al (at.%) Alloys at 900°C10.2174/1876503300902010037 ↗
44. The nature of the third-element effect in the oxidation of Fe–xCr–3 at.% Al alloys in 1 atm O2 at 1000°C10.1016/j.corsci.2007.06.019 ↗
45. The effect of water vapor on the initial stages of oxidation of the FeCrAl alloy kanthal AF at 900°C10.1007/s11085-007-9055-0 ↗
46. The formation of aluminum oxide scales on high-temperature alloys10.1007/BF00666913 ↗
47. The criteria for the transitions between the various oxidation modes of binary solid-solution alloys forming immiscible oxides at high oxidant pressures10.1023/A:1018847116670 ↗
48. The internal oxidation of ternary alloys. VI: the transition from internal to external oxidation of the most-reactive component under intermediate oxidant pressures10.1007/s11085-004-0920-9 ↗
49. An assessment of the Fe-O system10.1007/BF02645709 ↗
50. High-resolution characterization reveals the role of Al content in the evolution of oxide scales formed on alumina-forming alloy exposed to supercritical water10.1016/j.corsci.2024.111968 ↗
51. Increasing the upper temperature oxidation limit of alumina forming austenitic stainless steels in air with water vapor10.1007/s11085-011-9237-7 ↗
52. New insights into the initial oxidation behavior of an ultra-corrosion resistant alumina-forming austenitic steel in supercritical carbon dioxide: the effects of precipitated intragranular intermetallic compounds10.1016/j.corsci.2023.111260 ↗
53. Tecnalia Research & Innovation, (n.d.). https://www.tecnalia.com/(accessed August 19, 2025).
54. P. Villars, K. Cenzual, W.B. Pearson, Pearson’s crystal data : crystal structure database for inorganic compounds, in: 2007.
55. Corrosion behavior of T91 steel in liquid lead-bismuth eutectic at 550°C: Effects of exposure time and dissolved oxygen concentration10.1016/j.corsci.2022.110405 ↗
56. Anomalous oxidation rate-temperature dependence of alumina-forming austenitic stainless steels exposed to 500–600°C supercritical water10.1016/j.corsci.2024.111936 ↗
57. Corrosion and mechanical behavior of novel alumina forming steels in molten lead
58. High-temperature oxidation resistance of alumina-forming ferritic alloys in a steam-containing atmosphere10.1016/j.corsci.2025.113363 ↗
59. Transient alumina transformations on Ni–Cr–Al alloys: nanocrystallization and Cr concentration impacts10.1016/j.jmrt.2025.07.002 ↗
60. Effect of phase difference on growth kinetic of alloy layer in aluminized and diffusion-treated 12% Cr heating resistant steels10.1016/j.surfcoat.2013.12.061 ↗