journal article·2026-04

Corrosion behavior of alloy matrix and welded joint of Inconel 693 alloy in high-alkalinity supercritical water oxidation environment containing phosphate

Ziyi An, Shengdong Zhang, Yidan Han, Yingju Li, Cheng Zhu, Zongyao Ge, Xiaohui Feng, Yuansheng Yang

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Subcritical and Supercritical Water Processes · High-Temperature Coating Behaviors · High Entropy Alloys Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (61)

Show source-provided references
1. Review on treatment technologies of radioactive waste organic phase (TBP/OK) [J]
2. Treatment of spent radioactive organic solvents from nuclear fuel reprocessing plant: advances and perspectives [J]10.1016/j.nucengdes.2024.113138 ↗
3. Treatment of spent radioactive organic solvents from nuclear fuel reprocessing plant: advances and perspectives [J]10.1016/j.nucengdes.2024.113138 ↗
4. Study on radioactive TBP/kerosene treatment by super critical water oxidation [J]
5. An assessment of supercritical water oxidation (SCWO) - existing problems, possible solutions and new reactor concepts [J]10.1016/S1385-8947(00)00255-2 ↗
6. Corrosion in high-temperature and supercritical water and aqueous solutions: a review [J]10.1016/S0896-8446(03)00031-7 ↗
7. The corrosion of nickel-base alloy 625 in sub- and supercritical aqueous solutions of oxygen: a long time study [J]10.1023/A:1006607608189 ↗
8. Corrosion of alloy 625 in aqueous solutions containing chloride and oxygen [J]10.5006/1.3284802 ↗
9. Multiscale insights into temperature effects on the sliding wear of a martensitic stainless steel [J]10.1016/j.jmrt.2025.06.102 ↗
10. Oxidation of alloy 600 and alloy 690: experimentally accelerated study in hydrogenated supercritical water [J]10.1007/s11661-016-3897-5 ↗
11. Characteristics of oxidation and oxygen penetration of alloy 690 in 600 °C aerated supercritical water [J]10.1016/j.jmst.2016.11.001 ↗
12. Intergranular corrosion of Ni-30Cr in high-temperature hydrogenated water after removing surface passivating film [J]10.1038/s41529-024-00442-0 ↗
13. Corrosion of Inconel 690 and Inconel 693 in an iron phosphate glass melt [J]10.1016/j.corsci.2013.05.027 ↗
14. R. Halder, P. Sengupta, G. Abraham, C.P. Kaushik, G.K. Dey. Interaction of Alloy 693 with Borosilicate Glass at High Temperature; proceedings of the Conference on Advances in Refractory and Reactive Metals and Alloys (ARRMA), Mumbai, INDIA, F Jan 27-29, 2016 [C]. 2016.10.1016/j.matpr.2016.09.017 ↗
15. Mitigating grain boundary gd segregation to enhance high-temperature oxidation resistance in Mg-6Gd-1Al alloy: a comparative microstructural study [J]10.1016/j.corsci.2025.113256 ↗
16. Corrosion of alloy 625 in high-temperature, high-pressure sulfate solutions [J]10.5006/1.3284888 ↗
17. Effect of dissolved precursors on corrosion characteristics of Ni-based alloy Inconel 625, stainless steel 316L and titanium alloy TA2 in acidic and neutral supercritical water: a comparative study [J]10.1016/j.supflu.2024.106249 ↗
18. Transpassive dissolution of alloy 625, chromium, nickel, and molybdenum in high-temperature solutions containing hydrochloric acid and oxygen [J]10.5006/1.3287652 ↗
19. Comparative study of the corrosion behavior of Inconel 625 in supercritical water containing dissolved and molten phosphates [J]10.1016/j.supflu.2024.106495 ↗
20. Sulfate corrosion and phosphate passivation of Ni-based alloy in supercritical water [J]10.1016/j.supflu.2022.105564 ↗
21. The effect of molten phosphate on corrosion of 316 stainless steel, alloy 625, and titanium TA8 in supercritical water oxidation conditions [J]10.3390/ma16010395 ↗
22. The corrosion of alloy 625 (NiCr22Mo9Nb; 2.4856) in high-temperature, high-pressure aqueous solutions of phosphoric acid and oxygen. Corrosion at sub- and supercritical temperatures [J]10.1002/(SICI)1521-4176(199811)49:11<831::AID-MACO831>3.0.CO;2-V ↗
23. General corrosion and stress corrosion cracking behaviors of Alloy 825 in high-temperature supercritical water [J]10.1016/j.corsci.2025.112895 ↗
24. Corrosion behavior and slow strain rate tensile testing of Inconel 718 alloy in deaerated supercritical water at 650 °C [J]10.1016/j.jmrt.2025.02.254 ↗
25. Effect of post weld heat treatment on microstructural and mechanical properties of martensitic heat-resistant steel weldments [J]10.1016/j.ijpvp.2024.105323 ↗
26. Carbide behavior and micro-void of inconel 690 according to Nb content and aging temperature [J]10.1007/s12540-021-01028-0 ↗
27. Investigation on early formation and evolution of oxide scales on ferritic-martensitic steels in supercritical water [J]10.1016/j.corsci.2018.02.036 ↗
28. A precipitation hardened austenitic stainless steel with excellent stress corrosion cracking resistance against high-temperature water [J]10.1016/j.corsci.2025.113352 ↗
29. Enhancing high-temperature corrosion and cracking resistance of a dual-phase high entropy alloy through surface grinding [J]10.1016/j.corsci.2025.113227 ↗
30. Anomalous oxidation behavior and enhanced corrosion resistance of a lean-Cr FeCrAl alloy in the oxygenated PWR primary water [J]10.1016/j.corsci.2025.113452 ↗
31. Investigation on the component prediction and supercritical water oxidation of Ni-Cr-Mo alloy based on machine learning [J]10.1016/j.jnucmat.2024.155566 ↗
32. Exploring the influence of alloying elements (Zr, Si, and V) on the corrosion behavior of FeCoNiCr-based high entropy alloys in supercritical water environment [J]10.1016/j.jnucmat.2024.155605 ↗
33. Surface chemistry and corrosion behavior of Inconel 625 and 718 in subcritical, supercritical, and ultrasupercritical water [J]10.1016/j.apsusc.2017.01.119 ↗
34. X-ray pjotoelectron studies on some oxides and hydroxides of cobalt, nickel, and copper [J]10.1021/ac60363a034 ↗
35. Characterization of β-Ni(OH)2 by XPS [J]10.1116/1.1247752 ↗
36. Raman-spectroscopy of aqueous phosphate solutions At temperatures up to 450-degrees-C - 2 liquid-phases, supercritical fluids, and pyro-phosphate to ortho-phosphate conversions [J]10.1039/F29898501963 ↗
37. A novel phosphorus segregation-driven chromium depletion mechanism for intergranular corrosion of inconel 625 in SCWO-HyMoS environments [J]
38. Thermodynamic analysis of electroless plating nickel for 5383 aluminum alloy [J]
39. Defects and cation diffusion In magnetite (Iii) tracer diffusion of foreign tracer cations As A function of temperature and oxygen potential [J]10.1002/bbpc.19780820803 ↗
40. Corrosion behavior of Alloy 690 in aerated supercritical water [J]10.1016/j.corsci.2012.10.001 ↗
41. The mechanism of oxide film formation on austenitic stainless steels in high temperature water [J]10.1016/S0010-938X(97)00140-6 ↗
42. The mechanism of high temperature aqueous corrosion of stainless steels [J]10.1016/0010-938X(91)90125-9 ↗
43. An XPS study of the electronic structure of the ZnxCd1−xCr2(X = S, Se) spinel system [J]10.1016/0022-3697(89)90487-3 ↗
44. X-ray photoelectron studies on some oxides and hydroxides of cobalt, nickel, and copper [J]10.1021/ac60363a034 ↗
45. XPS and auger spectroscopy studies on mixtures of the oxides SiO2, Al2O3, Fe2O3 and Cr2O3 [J]10.1016/0368-2048(87)80022-1 ↗
46. X-ray photoelectron spectra of hexavalent iron [J]10.1016/0368-2048(80)80021-1 ↗
47. Corrosion mechanism of 5083 aluminum alloy in seawater containing phosphate [J]10.1007/s11802-021-4545-2 ↗
48. An investigation on microstructure and pitting corrosion behavior of 316L stainless steel weld joint [J]10.1557/jmr.2017.316 ↗
49. Corrosion resistance of welded joints of X5CrNi18-10 stainless steel [J]10.1016/j.jmatprotec.2018.11.029 ↗
50. Microstructural and local electrochemical characterisation of Gr. 91 steel welded joints as function of post-weld heat treatments [J]10.1016/j.corsci.2018.12.042 ↗
51. Corrosion characteristics of Fe, Ni and Ti based alloys near the critical point of water and during supercritical water gasification and oxidation of municipal sludge [J]10.1016/j.supflu.2024.106337 ↗
52. Nickel monochromated Al Kα XPS spectra from the Physical electronics model 5400 spectrometer [J]10.1116/1.1247750 ↗
53. X-ray photoelectron-spectroscopy of nickel boride catalysts - correlation of surface-states with reaction-products In the hydrogenation of acrylonitrile [J]10.1016/0021-9517(80)90294-8 ↗
54. A study of a number of maxed transition-metal oxide spinels using X-ray photoelectron-spectroscopy [J]10.1016/0169-4332(89)90977-X ↗
55. Curve fitting of Cr 2p photoelectron spectra of Cr2O3 and CrF3 [J]10.1002/sia.740231306 ↗
56. On the determination of atomic charge via ESCA including application to organometallics [J]10.1016/0368-2048(95)02392-5 ↗
57. An X-ray photoelectron spectroscopic study of some chromium oxygen systems [J]10.1002/sia.740130210 ↗
58. Noncrystalline chromium, molybdenum and tungsten phosphate films prepared by metal organic-chemical vapor-deposition [J]10.1016/0040-6090(91)90122-E ↗
59. On the oxide formation on stainless steels AISI 304 and incoloy 800H investigated with XPS [J]10.1016/0169-4332(87)90062-6 ↗
60. On the oxide formation on stainless-steels AISI-304 and INCOLOY-800H investigated with XPS [J]10.1016/0169-4332(87)90062-6 ↗
61. Oxidation evolutions in different regions of 9Cr3W3Co martensitic steel welded joints exposed to oxygenated supercritical water at 650 °C [J]10.1016/j.ijpvp.2025.105530 ↗