Insights into crevice corrosion in high temperature molten salt system: nickel-based GH3535 alloy exposed to static FLiNaK salt at 700 °C
Bibliographic record
Abstract
No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.
Source: Not provided · Quality: missing
Research context
OpenAlex topics: Nuclear reactor physics and engineering · Nuclear Materials and Properties · Molten salt chemistry and electrochemical processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Generation IV International Forum (GIF)
2. DOE nuclear energy research advisory committee and the generation iv international forum
3. Thorium molten salt reactor nuclear energy system (TMSR)
4. Assessing the benefit of thorium fuel in a once through molten salt reactor10.1016/j.pnucene.2024.105369 ↗
5. Oak Ridge National Laboratory, The development status of Molten-salt breeder reactors, 1972, 416.
6. Understanding of the stress assisted cracking behavior of Ni-based alloy GH3535 in molten LiF-NaF-KF salt10.1016/j.corsci.2025.113038 ↗
7. Crevice corrosion characteristics and impact on the shear performance of screw connections10.1016/j.istruc.2025.109809 ↗
8. Comparison of crevice corrosion of P110S and HP-13Cr in extremely aggressive environment containing CO2 and H2S
9. Crevice chemistry and corrosion in high temperature water: a review10.1016/j.net.2024.03.010 ↗
10. R.C. Briant, J.H. Buck, A.J. Miller, ORNL-1375 aircraft nuclear propulsion program quarterly progress report for period ending september 10, 1952, 109.
11. Corrosion behavior of GH3535 alloy in molten LiF–BeF2 salt10.1016/j.corsci.2022.110168 ↗
12. Materials corrosion in molten LiF-NaF-KF salt10.1016/j.jfluchem.2008.05.008 ↗
13. Intergranular corrosion of high temperature alloys in molten fluoride salts10.3184/096034010X12743509428336 ↗
14. Aggregation and data analysis of corrosion studies in molten chloride and fluoride salts10.1016/j.jnucmat.2018.07.036 ↗
15. Corrosion performance of Ni-based structural alloys for applications in molten-salt based energy systems: experiment & numerical validation10.1016/j.corsci.2021.109607 ↗
16. On the possibility of severe corrosion of a Ni-W-Cr alloy in fluoride molten salts at high temperature10.1016/j.corsci.2019.01.012 ↗
17. Effect of moisture on corrosion of Ni-based alloys in molten alkali fluoride FLiNaK salt environments10.1016/j.jnucmat.2013.02.021 ↗
18. Non-uniform corrosion of UNS N10003 alloy induced by trace SO42- in molten FLiNaK salt10.1016/j.corsci.2021.109802 ↗
19. Effect of O2- additive on the corrosion behavior of Hastelloy N alloy in molten FLiNaK10.1016/j.corsci.2023.111001 ↗
20. Corrosion behavior of UNS N10003 alloy in molten LiF-BeF2-ZrF4 with phosphide impurity10.1016/j.corsci.2023.111635 ↗
21. Dissolved valence state of iron fluorides and their effect on Ni-based alloy in FLiNaK salt10.1016/j.corsci.2021.109794 ↗
22. Effect of CrF3 on the corrosion behaviour of Hastelloy-N and 316L stainless steel alloys in FLiNaK molten salt10.1016/j.corsci.2017.12.008 ↗
23. Interaction mechanisms of a Hastelloy N-316L stainless steel couple in molten LiF-NaF-KF salt10.1016/j.corsci.2019.108317 ↗
24. Effect of graphite particles in molten LiF-NaF-KF eutectic salt on corrosion behaviour of GH3535 alloy10.1016/j.corsci.2020.108581 ↗
25. He bubbles inhibition and abnormal hardening in GH3535 alloy by niobium element addition10.1016/j.jnucmat.2023.154841 ↗
26. Microstructural evolution and hardening of GH3535 alloy under energetic Xe ion irradiation at room temperature and 650 °C10.1016/j.jnucmat.2017.12.006 ↗
27. Effect of irradiation damage defects on the impurity containing molten salt corrosion behavior in GH3535 alloy10.1016/j.corsci.2023.111475 ↗
28. Helium ion irradiation-induced damage of powder metallurgy-hot isostatic pressed Ni-based alloy GH3535 for molten salt reactor applications10.1016/j.jnucmat.2023.154871 ↗
29. Synergistic effect of irradiation and molten salt corrosion: acceleration or deceleration?10.1016/j.corsci.2021.109434 ↗
30. 2020
31. Characteristics of the initiation and propagation of crevice corrosion in stainless steel10.1016/j.corsci.2025.113063 ↗
32. Electroactive Shewanella algae accelerates the crevice corrosion of X70 pipeline steel in marine environment10.1016/j.corsci.2024.112226 ↗
33. Corrosion and Te embrittlement behaviors of Ni-Mo-Cr-Nb alloy in Te-containing molten salts10.1016/j.jnucmat.2024.155450 ↗
34. Corrosion behavior of Incoloy 800H/HT in the fluoride molten salt FLiNaK + MFx (MFx = CrF3, FeF2, FeF3 and NiF2)10.1039/C5NJ01839K ↗
35. D.H. Suo, G.Y. Ran, X.Z. Yuan, M.T. Li, Y.Y. Liu, Y.M. Jiang, J. Li, Y.T. Sun, Multi-scale evaluation of crevice corrosion behavior in two lean duplex stainless steels: from initiation to propagation, Corros. Commun.. In press, https://doi.org/10.1016/j.corcom.2024.09.003<2026/bib>.10.1016/j.corcom.2024.09.003 ↗
36. Effect of molybdate on crevice corrosion initiation of hydrogen-charged duplex stainless steel10.1016/j.jmrt.2023.02.159 ↗
37. Long-term corrosion behaviors of Hastelloy-N and Hastelloy-B3 in moisture-containing molten FLiNaK salt environments10.1016/j.jnucmat.2013.11.045 ↗
38. Effect of long-term thermal exposure on microstructure and stress rupture properties of GH3535 superalloy10.1016/j.jmst.2014.07.021 ↗
39. The high-temperature corrosion of Hastelloy N alloy (UNS N10003) in molten fluoride salts analysed by STXM, XAS, XRD, SEM, EPMA, TEM/EDS10.1016/j.corsci.2016.02.010 ↗
40. The effect of silicon on precipitation and decomposition behaviors of M6C carbide in a Ni–Mo–Cr superalloy10.1016/j.jallcom.2014.09.112 ↗
41. C. Eveleigh, Research internship report in Shanghai Institute of Applied Physics, 2018, pp. 24.
42. Effect of high temperature molten salt corrosion on the microstructure of a Co-Mo-Cr-Si wear resistant alloy10.1016/j.matchar.2021.111377 ↗
43. Pankratz · 1984
44. The solubilities of hydrogen fluoride and deuterium fluoride in molten fluorides10.1021/j100869a013 ↗
45. Validating modern methods for impurity analysis in fluoride salts10.1016/j.jnucmat.2021.152972 ↗
46. Metallic impurities induced corrosion of a Ni-26W-6Cr alloy in molten fluoride salts at 850 °C10.1016/j.corsci.2020.109079 ↗
47. Accelerated corrosion testing in molten fluoride salts: effect of additives and the crucible material10.1016/j.corsci.2021.110011 ↗