Synergistic effect of nickel and oxygen on 316L stainless steel corrosion in liquid lead
Source abstract
Abstract
Austenitic 316L suffers dissolution corrosion in liquid lead (Pb) as the selective leaching of nickel (Ni) results in a destabilized microstructure. We demonstrate a chemistry-based corrosion control approach in which sub-saturated Ni together with controlled oxygen additions co-inhibit dissolution and promote oxide formation. Tests at 500 °C for 500 h spanned a 2 × 3 matrix (Oxygen: 5 · 10 –8 and 5 · 10 –7 wt.%; Ni: 0, 0.05, 0.1 wt.%). In-situ oxygen concentration and oxygen consumption monitoring, corrosion depth measurements, and microstructure measured by SEM/EDX were assessed. In Ni-free lead, uniform selective leaching of Ni from the stainless steel is observed. At 0.05 wt.% dissolved Ni the depth of dissolution is localized and reduced by a factor of 10. And with 0.1 wt.% Ni, oxidation of the steel dominated at both oxygen concentrations. Oxygen consumption at 5 · 10 –7 wt.% was ∼3 times that at 5 · 10 –8 wt.%, consistent with ∼3 times thicker oxide. This work indicates a coupled effect of dissolved Ni and O that reduces dissolution corrosion observed on stainless steel in high temperature lead.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Thermodynamic and Structural Properties of Metals and Alloys · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Properties of austenitic steels for nuclear reactor applications, (2012) 267–283. https://doi.org/10.1016/B978-0-08-056033-5.00019-7.10.1016/B978-0-08-056033-5.00019-7 ↗
2. Review on sodium corrosion evolution of nuclear-grade 316 stainless steel for sodium-cooled fast reactor applications
3. Investigation of the effect of lead–bismuth eutectic on the fracture properties of T91 and 316L10.1016/j.jnucmat.2009.10.021 ↗
4. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
5. Dissolution mechanism of 316L in lead–bismuth eutectic at 500 °C10.1016/j.corsci.2011.05.031 ↗
6. Selective leaching of nickel and chromium from type 316 austenitic steel in oxygen-containing lead–bismuth eutectic (LBE)10.1016/j.corsci.2014.03.016 ↗
7. Corrosion behavior of austenitic steels 1.4970, 316L and 1.4571 in flowing LBE at 450 and 550 °C with 10−7mass% dissolved oxygen10.1016/j.jnucmat.2014.08.024 ↗
8. Corrosion behavior of 316 stainless steel arc parts in liquid lead at 650 °C under high oxygen concentrations10.1039/D2RA05165F ↗
9. Corrosion behavior of AISI 316L steel in static lead melt at 450 oС and 650 °C10.1016/j.prostr.2024.04.031 ↗
10. Oxygen-enhanced dissolution corrosion of austenitic stainless steel 316 L in static lead-bismuth eutectic at 500 °C10.1016/j.corsci.2024.112224 ↗
11. Oxidation mechanism of a Fe–9Cr–1Mo steel by liquid Pb–Bi eutectic alloy (Part I)10.1016/j.corsci.2008.06.050 ↗
12. Early stages of liquid-metal corrosion on pre-oxidized surfaces of austenitic stainless steel 316L exposed to static Pb-Bi eutectic at 400 °C10.1016/j.corsci.2023.111680 ↗
13. Oxidation of steels in liquid lead bismuth: oxygen control to achieve efficient corrosion protection10.1016/j.nucengdes.2010.07.039 ↗
14. Aspects of minimizing steel corrosion in liquid lead-alloys by addition of oxygen10.1016/j.nucengdes.2011.09.002 ↗
15. A review of the surface modifications for corrosion mitigation of steels in lead and LBE10.3390/coatings11010053 ↗
16. Research progress on LBE corrosion-resistant coatings: a review10.1016/j.pnucene.2024.105358 ↗
17. Corrosion of austenitic stainless steels in liquid Pb with 2E-7 wt% oxygen at 600 and 700 °C10.1016/j.corsci.2024.112651 ↗
18. Oxide scale formation on 316L and FeCrAl steels exposed to oxygen controlled static LBE at temperatures up to 800 °C10.1016/j.solmat.2015.09.007 ↗
19. Long term corrosion on T91 and AISI1 316L steel in flowing lead alloy and corrosion protection barrier development: experiments and models10.1016/j.jnucmat.2011.04.028 ↗
20. Improved LBE corrosion resistance of the FeCrAl coating by the addition of trace Si element10.1016/j.intermet.2024.108197 ↗
21. Advanced Al2O3 coatings for high temperature operation of steels in heavy liquid metals: a preliminary study10.1016/j.corsci.2013.07.039 ↗
22. Effect of Y2O3 content on microstructure and corrosion behavior of ZrO2 coatings in liquid lead-bismuth eutectic
23. Lead-bismuth eutectic corrosion resistance of TiAlN coating after N5+ ion irradiation10.1016/j.tsf.2024.140224 ↗
24. Early stages of dissolution corrosion in 316L and DIN 1.4970 austenitic stainless steels with and without anticorrosion coatings in static liquid lead-bismuth eutectic (LBE) at 500 °C
25. Long term corrosion resistance of alumina forming austenitic stainless steels in liquid lead10.1016/j.jnucmat.2015.03.011 ↗
26. Corrosion behaviour of Al-added high Mn austenitic steels in molten lead bismuth eutectic with saturated and low oxygen concentrations at 450 °C10.1016/j.corsci.2020.108864 ↗
27. Corrosion prevention of type 316L stainless steel in Pb-17Li through nickel addition10.13182/FST13-661 ↗
28. 2024
29. Solubility of oxygen and metastable limit for PbO nucleation in liquid Pb10.1007/s11837-021-04909-2 ↗
30. Control of dissolved oxygen in liquid LBE by electrochemical oxygen pumping10.1016/j.snb.2014.07.117 ↗
31. Solubility of nickel and chromium in molten lead
32. Corrosion of T91 and pure iron in flowing and static Pb-Bi alloy between 450 °C and 540 °C: experiments, modelling and mechanism10.1016/j.corsci.2020.108897 ↗
33. Orientation relationship of the austenite-to-ferrite transformation in austenitic stainless steels due to dissolution corrosion in contact with liquid Pb-Bi eutectic10.1016/j.scriptamat.2019.03.035 ↗