journal article·2008Open access

Effects of ceramic thickness and curing unit on light transmission through leucite-reinforced material and polymerization of dual-cured luting agent

Milena C. Pazin, Rafael R. Moraes, Luciano S. Gonçalves, Gilberto A. Borges, Mário A. C. Sinhoreti, Lourenço Correr-Sobrinho

Journal of Oral Science· Volume 50· Issue 2

Abstract

This study investigated the influence of ceramic thickness and curing unit on light transmission through leucite-reinforced material and polymerization of a dual-cured resin luting agent. Discs of Empress Esthetic (Ivoclar Vivadent) of 0.7-, 1.4- and 2-mm thickness were prepared. Variolink II (Ivoclar Vivadent) was placed in a 1-mm-thick cylindrical mold, and light-activated through ceramic for 40 s, using QTH or LED units. The samples were divided into dual, light, and chemically-polymerized control groups. Knoop hardness indentations were made on the top and bottom surfaces. Data were subjected to split-plot design three-way ANOVA and Tukey's test (P < 0.05). The light spectrum transmitted through ceramic was obtained using a spectrometer. Samples activated through 1.4-and 2-mm-thick discs showed lower hardness than all others groups, except for the chemical control group. Dual and light-polymerized control samples showed similar hardness to those activated through the 0.7-mm ceramic, whereas chemically polymerized control samples showed similar hardness to those activated through 1.4- and 2-mm ceramics. No significant differences in hardness were detected between the curing units or between the top and bottom layers. No significant alteration in the light spectrum profile was observed for both units, irrespective of the ceramic thickness.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Photopolymerization techniques and applications · Dental materials and restorations · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (16)

Show source-provided references
1. 1. Malament KA, Socransky SS (2001) Survival of Dicor glass-ceramic dental restorations over 16 years. Part III: effect of luting agent and tooth or tooth-substitute core structure. J Prosthet Dent 86, 511-51910.1067/mpr.2001.119415 ↗
2. 2. Groten M, Probster L (1997) The influence of different cementation modes on the fracture resistance of feldspathic ceramic crowns. Int J Prosthodont 10, 169-177
3. 3. Rosenstiel SF, Land MF, Crispin BJ (1998) Dental luting agents: a review of the current literature. J Prosthet Dent 80, 280-30110.1016/S0022-3913(98)70128-3 ↗
4. 10.1002/jbm.b.3092810.1002/jbm.b.30928 ↗
5. 10.1016/j.jdent.2004.03.00310.1016/j.jdent.2004.03.003 ↗
6. 10.1016/S0109-5641(01)00069-010.1016/S0109-5641(01)00069-0 ↗
7. 7. el-Mowafy OM, Rubo MH, el-Badrawy WA (1999) Hardening of new resin cements cured through a ceramic inlay. Oper Dent 24, 38-44
8. 8. Jung H, Friedl KH, Hiller KA, Furch H, Bernhart S, Schmalz G (2006) Polymerization efficiency of different photocuring units through ceramic discs. Oper Dent 31, 68-7710.2341/04-188 ↗
9. 9. Jung H, Friedl KH, Hiller KA, Haller A, Schmalz G (2001) Curing efficiency of different polymerization methods through ceramic restorations. Clin Oral Investig 5, 156-16110.1007/s007840100118 ↗
10. 10. Soares CJ, da Silva NR, Fonseca RB (2006) Influence of the feldspathic ceramic thickness and shade on the microhardness of dual resin cement. Oper Dent 31, 384-38910.2341/05-51 ↗
11. 11. Rasetto FH, Driscoll CF, Prestipino V, Masri R, von Fraunhofer JA (2004) Light transmission through all-ceramic dental materials: a pilot study. J Prosthet Dent 91, 441-44610.1016/j.prosdent.2004.02.019 ↗
12. 10.1016/j.polymertesting.2006.10.01010.1016/j.polymertesting.2006.10.010 ↗
13. 13. Brodbelt RH, O'Brien WJ, Fan PL (1980) Translucency of dental porcelains. J Dent Res 59, 70-7510.1177/00220345800590011101 ↗
14. 14. Ozturk N, Usumez A, Usumez S, Ozturk B (2005) Degree of conversion and surface hardness of resin cement cured with different curing units. Quintessence Int 36, 771-777
15. 15. Schneider LF, Moraes RR, Cavalcante LM, Sinhoreti MA, Correr-Sobrinho L, Consani S (2008) Cross-link density evaluation through softening tests: effect of ethanol concentration. Dent Mater 24, 199-20310.1016/j.dental.2007.03.010 ↗
16. 16. Bühler-Zemp P (2004) IPS Empress Esthetic scientific documentation. Ivoclar Vivadent AG, Schaan, 3-5