Shear bond strength between an indirect composite veneering material and zirconia ceramics after thermocycling

Futoshi Komine, Kazuhisa Kobayashi, Ayako Saito, Ryosuke Fushiki, Hiroyasu Koizumi, Hideo Matsumura

Journal of Oral Science· Volume 51· Issue 4

Abstract

The present study evaluated the shear bond strength between an indirect composite material and zirconium dioxide (zirconia) ceramics after thermocycling. A total of 80 zirconia (Katana) discs were divided into five groups and primed with one of following agents: All Bond 2 Primer B (ABB), Alloy Primer (ALP), AZ Primer (AZP), Estenia Opaque Primer (EOP), and Porcelain Liner M Liquid A (PLA). An indirect composite material (Estenia C&B) was then bonded to the primed zirconia. One-half of the specimens (n = 8) in each group were stored in distilled water at 37 degrees C for 24 h, and the remaining eight specimens were thermocycled 5,000 times before shear bond strength testing. Mean bond strengths before thermocycling varied from 10.1 to 15.6 MPa; bond strengths after thermocycling ranged from 4.3 to 17.6 MPa. The ALP group had the highest strengths after thermocycling; there were no significant differences among the PLA, AZP, and EOP groups. The bond strength values for PLA, AZP, EOP, and ALP did not decrease with thermocycling. The application of an acidic functional monomer containing carboxylic anhydride (4-META), phosphonic acid (6-MHPA), or phosphate monomer (MDP) provided durable bond strength between Estenia C&B indirect composite and Katana zirconia.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Dental Implant Techniques and Outcomes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (11)

Show source-provided references
1. 10.1111/j.1365-2842.2004.01437.x10.1111/j.1365-2842.2004.01437.x ↗
2. 10.1016/j.prosdent.2006.08.01010.1016/j.prosdent.2006.08.010 ↗
3. 3. Sailer I, Féher A, Filser F, Gauckler LJ, Lüthy H, Hämmerle CH (2007) Five-year clinical results of zirconia frameworks for posterior fixed partial dentures. Int J Prosthodont 20, 383-388.
4. 4. Tinschert J, Schulze KA, Natt G, Latzke P, Heussen N, Spiekermann H (2008) Clinical behavior of zirconia-based fixed partial dentures made of DC-Zirkon: 3-year results. Int J Prosthodont 21, 217-222.
5. 5. Edelhoff D, Florian B, Florian W, Johnen C (2008) HIP zirconia fixed partial dentures – clinical results after 3 years of clinical service. Quintessence Int 39, 459-471.
6. 6. Molin MK, Karlsson SL (2008) Five-year clinical prospective evaluation of zirconia-based Denzir 3-unit FPDs. Int J Prosthodont 21, 223-227.
7. 7. Ciftçi Y, Canay S (2000) The effect of veneering materials on stress distribution in implant-supported fixed prosthetic restorations. Int J Oral Maxillofac Implants 15, 571-582.
8. 8. Takahashi Y, Hisama K, Sato H, Chai J, Shimizu H, Kido H, Ukon S (2002) Probability of failure of highly filled indirect resin-veneered implant-supported restorations: an in vitro study. Int J Prosthodont 15, 179-182.
9. 9. Kobayashi K, Komine F, Blatz MB, Saito A, Koizumi H, Matsumura H (2009) Influence of priming agents on the short-term bond strength of an indirect composite veneering material to zirconium dioxide ceramic. Quintessence Int 40, 545-551.
10. 10. Blatz MB, Chiche G, Holst S, Sadan A (2007) Influence of surface treatment and simulated aging on bond strengths of luting agents to zirconia. Quintessence Int 38, 745-753.
11. 10.1016/0022-3913(92)90239-710.1016/0022-3913(92)90239-7 ↗