Vicker's microhardness and energy dispersive x-ray analysis of fluorapatite-leucite and fluorapatite ceramics cyclically immersed in acidic agents
Source abstract
Abstract
This study evaluated the microhardness and elemental composition of various ceramics immersed in acidic agents. One hundred and five discs of fluorapatite-leucite (IPS d.SIGN) and fluorapatite ceramics (IPS e.max Ceram) were randomly divided into 7 groups of 15 each. Five groups were alternately immersed in acidic agents (citrate buffer solution, pineapple juice, green mango juice, cola soft drink and 4% acetic acid) for 30 min and deionized water for 5 min in 7 cycles at 37 degrees C. Two groups were continuously immersed in 4% acetic acid at 80 degrees C for 16 h and deionized water at 37 degrees C for 245 min. Vicker's microhardness and elemental composition were recorded before and after immersion. Data were analyzed using two-way repeated ANOVA and t-test at a significance level 0.05. For IPS d.SIGN, there was statistically significant difference in microhardness values between before and after immersion in the green mango, cola soft drink and 4% acetic acid for 16 h (P < 0.05). However, for IPS e.max Ceram, there was no significant difference between before and after immersion in any of the groups (P > 0.05). EDX results of both ceramics found that the elemental percentage of Na, K, Zr, Al and Si decreased after being immersed in acidic agents.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Health and Care Utilization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. 1. Raptis NV, Michalakis KX, Hirayama H (2006) Optical behavior of current ceramic systems. Int J Periodontics Restorative Dent 26, 31-41.
2. 10.1007/s10856-006-0441-y10.1007/s10856-006-0441-y ↗
3. 10.1016/j.dental.2005.08.00710.1016/j.dental.2005.08.007 ↗
4. 4. Höland W, Rheinberger V, Schweiger M (2003) Control of nucleation in glass ceramics. Phil Trans R Soc Lond A 361, 575-589.10.1098/rsta.2002.1152 ↗
5. 10.1016/S0022-3913(00)70033-310.1016/S0022-3913(00)70033-3 ↗
6. 6. Kelly JR, Giordano R, Pober R, Cima MJ (1990) Fracture surface analysis of dental ceramics: clinically failed restorations. Int J Prosthodont 3, 430-440.
7. 10.1016/S0109-5641(00)00030-010.1016/S0109-5641(00)00030-0 ↗
8. 10.1177/15440591030820120710.1177/154405910308201207 ↗
9. 10.1016/S0022-3913(03)00214-210.1016/S0022-3913(03)00214-2 ↗
10. 10.1002/jbm.1010910.1002/jbm.10109 ↗
11. 11. Anusavice KJ (1992) Degradability of dental ceramics. Adv Dent Res 6, 82-89.10.1177/08959374920060012201 ↗
12. 10.1016/j.jeurceramsoc.2005.03.24210.1016/j.jeurceramsoc.2005.03.242 ↗
13. 13. Jakovac M, Zivko-Babic J, Curkovic L, Carek A (2006) Chemical durability of dental ceramic material in acid medium. Acta Stomatol Croat 40, 65-71.
14. 10.1016/S0142-9612(98)00223-310.1016/S0142-9612(98)00223-3 ↗
15. 15. Demirhanoglu ST, Sahin E (1992) Effect of topical fluorides and citric acid on overglazed and autoglazed porcelain surfaces. Int J Prosthodont 5, 434-440.
16. 16. Clayton JA, Green E (1970) Roughness of pontic materials and dental plaque. J Prosthet Dent 23, 407-411.10.1016/0022-3913(70)90007-7 ↗
17. 17. Jaeggi T, Lussi A (2006) Prevalence, incidence and distribution of erosion. Monogr Oral Sci 20, 44-65.10.1159/000093350 ↗
18. 18. Khan F, Young WG, Law V, Priest J, Daley TJ (2001) Cupped lesions of early onset dental erosion in young southeast Queensland adults. Aust Dent J 46, 100-107.10.1111/j.1834-7819.2001.tb00564.x ↗
19. 19. Imfeld T (1996) Dental erosion. Definition, classification and links. Eur J Oral Sci 104, 151-155.10.1111/j.1600-0722.1996.tb00063.x ↗
20. 20. Kontonasaki E, Kantiranis N, Papadopoulou L, Chatzistavrou X, Kavouras P, Zorba T, Sivropoulou A, Chrissafis K, Paraskevopoulos KM, Koidis PT (2008) Microstructural characterization and comparative evaluation of physical, mechanical and biological properties of three ceramics for metal-ceramic restorations. Dent Mater 24, 1362-1373.10.1016/j.dental.2008.03.002 ↗
21. 21. International Organization for Standardization (1995) Dental ceramic. ISO 6872, Geneve.
22. 22. Milleding P, Karlsson S, Nyborg L (2003) On the surface elemental composition of non-corroded and corroded dental ceramic materials in vitro. J Mater Sci Mater Med 14, 557-566.10.1023/A:1023416232222 ↗
23. 23. Seghi RR, Sorensen JA (1995) Relative flexural strength of six new ceramics materials. Int J Prosthodont 8, 239-246.
24. 24. Denry IL (1996) Recent advances in ceramics for dentistry. Crit Rev Oral Biol Med 7, 134-143.10.1177/10454411960070020201 ↗
25. 10.1016/S0109-5641(98)00033-510.1016/S0109-5641(98)00033-5 ↗
26. LEE H-H · 1997 · 16 · 13410.4012/dmj.16.134 ↗
27. 10.1007/BF0075791010.1007/BF00757910 ↗
28. 28. Ahmed AA, El-Batal HA, Ghoneim NA, Khalifa FA (1982) Leaching of some lithium-silicate glasses and glass-ceramic. J Non-Cryst Solids 41, 57-70.10.1016/0022-3093(80)90191-X ↗
29. 29. Fairhurst CW, Anusavice KJ, Hashinger DT, Ringle RD, Twiggs SW (1980) Thermal expansion of dental alloys and porcelains. J Biomed Mater Res 14, 435-446.10.1002/jbm.820140410 ↗
30. 30. Mackert JR Jr, Evans AL (1991) Effect of cooling rate on leucite volume fraction in dental porcelains. J Dent Res 70, 137-139.10.1177/00220345910700020801 ↗
31. 31. Mackert JR Jr, Rueggeberg FA, Lockwood PE, Evans AL, Thompson WO (1994) Isothermal anneal effect on microcrack density around leucite particles in dental porcelain. J Dent Res 73, 1221-1227.10.1177/00220345940730061401 ↗
32. 10.1016/0109-5641(92)90106-M10.1016/0109-5641(92)90106-M ↗
33. 33. Forss H, Seppä L, Lappalainen R (1991) In vitro abrasion resistance and hardness of glass-ionomer cements. Dent Mater 7, 36-39.10.1016/0109-5641(91)90024-S ↗
34. 34. Pinto MM, Cesar PF, Rosa V, Yoshimura HN (2008) Influence of pH on slow crack growth of dental porcelains. Dent Mater 24, 814-823.10.1016/j.dental.2007.10.001 ↗
35. 10.1016/S0010-938X(99)00143-210.1016/S0010-938X(99)00143-2 ↗