Abstract

This study compared the wear characteristics of a heat-pressed lithium disilicate ceramic material opposed to feldspathic porcelain, a lithium disilicate glass ceramic, and zirconia materials. Ceramic plate specimens were prepared from feldspathic porcelain (EX-3 nA1B), lithium disilicate glass ceramics (e.max CAD MO1/C14), and zirconia (Katana KT 10) and then ground or polished. Rounded rod specimens were fabricated from heat-pressed lithium disilicate glass ceramic (e.max press LT A3) and then glazed or polished. A sliding wear testing apparatus was used for wear testing. Wear of glazed rods was greater than that of polished rods when they were abraded with ground zirconia, ground porcelain, polished porcelain, or polished lithium disilicate ceramics. For both glazed and polished rods, wear was greater when the rods were abraded with ground plates. The findings indicate that application of a polished surface rather than a glazed surface is recommended for single restorations made of heat-pressed lithium disilicate material. In addition, care must be taken when polishing opposing materials, especially those used in occlusal contact areas. (J Oral Sci 58, 117-123, 2016).
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Implant Techniques and Outcomes · Temporomandibular Joint Disorders

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Fixed Prosthodontics, Nihon University School of Dentistry

Division of Advanced Dental Treatment, Dental Research Center, Nihon University School of Dentistry

Division of Applied Oral Sciences, Nihon University Graduate School of Dentistry

References (20)

Show source-provided references
1. 1. Christensen RP, Ploeger BJ (2010) A clinical comparison of zirconia, metal and alumina fixed-prosthesis frameworks veneered with layered or pressed ceramic: a three-year report. J Am Dent Assoc 141, 1317-1329.10.14219/jada.archive.2010.0076 ↗
2. 2. Mundhe K, Jain V, Pruthi G, Shah N (2015) Clinical study to evaluate the wear of natural enamel antagonist to zirconia and metal ceramic crowns. J Prosthet Dent 114, 358-363.10.1016/j.prosdent.2015.03.001 ↗
3. 3. Conrad HJ, Seong WJ, Pesun IJ (2007) Current ceramic materials and systems with clinical recommendations: a systematic review. J Prosthet Dent 98, 389-404.10.1016/S0022-3913(07)60124-3 ↗
4. 4. al-Wahadni A, Martin DM (1998) Glazing and finishing dental porcelain: a literature review. J Can Dent Assoc 64, 580-583.
5. 5. Sarac D, Sarac YS, Yuzbasioglu E, Bal S (2006) The effects of porcelain polishing systems on the color and surface texture of feldspathic porcelain. J Prosthet Dent 96, 122-128.10.1016/j.prosdent.2006.05.009 ↗
6. 6. Sarikaya I, Güler AU (2010) Effects of different polishing techniques on the surface roughness of dental porcelains. J Appl Oral Sci 18, 10-16.10.1590/S1678-77572010000100004 ↗
7. 7. Jagger DC, Harrison A (1994) An in vitro investigation into the wear effects of unglazed, glazed, and polished porcelain on human enamel. J Prosthet Dent 72, 320-323.10.1016/0022-3913(94)90347-6 ↗
8. 8. Oh WS, Delong R, Anusavice KJ (2002) Factors affecting enamel and ceramic wear: a literature review. J Prosthet Dent 87, 451-459.10.1067/mpr.2002.123851 ↗
9. 9. Preis V, Behr M, Handel G, Schneider-Feyrer S, Hahnel S, Rosentritt M (2012) Wear performance of dental ceramics after grinding and polishing treatments. J Mech Behav Biomed Mater 10, 13-22.10.1016/j.jmbbm.2012.03.002 ↗
10. 10. Luangruangrong P, Cook NB, Sabrah AH, Hara AT, Bottino MC (2014) Influence of full-contour zirconia surface roughness on wear of glass-ceramics. J Prosthodont 23, 198-205.10.1111/jopr.12088 ↗
11. 11. Saiki O, Koizumi H, Nogawa H, Hiraba H, Akazawa N, Matsumura H (2014) Influence of ceramic surface texture on the wear of gold alloy and heat-pressed ceramics. Dent Mater J 33, 865-873.10.4012/dmj.2014-129 ↗
12. 12. Preis V, Behr M, Kolbeck C, Hahnel S, Handel G, Rosentritt M (2011) Wear performance of substructure ceramics and veneering porcelains. Dent Mater 27, 796-804.10.1016/j.dental.2011.04.001 ↗
13. 13. Burgess JO, Janyavula S, Lawson NC, Lucas TJ, Cakir D (2014) Enamel wear opposing polished and aged zirconia. Oper Dent 39, 189-194.10.2341/12-345-L ↗
14. 14. Janyavula S, Lawson N, Cakir D, Beck P, Ramp LC, Burgess JO (2013) The wear of polished and glazed zirconia against enamel. J Prosthet Dent 109, 22-29.10.1016/S0022-3913(13)60005-0 ↗
15. 15. Lawson NC, Janyavula S, Syklawer S, McLaren EA, Burgess JO (2014) Wear of enamel opposing zirconia and lithium disilicate after adjustment, polishing and glazing. J Dent 42, 1586-1591.10.1016/j.jdent.2014.09.008 ↗
16. 16. Lee A, Swain M, He L, Lyons K (2014) Wear behavior of human enamel against lithium disilicate glass ceramic and type III gold. J Prosthet Dent 112, 1399-1405.10.1016/j.prosdent.2014.08.002 ↗
17. 17. Miyazaki T, Nakamura T, Matsumura H, Ban S, Kobayashi T (2013) Current status of zirconia restoration. J Prosthodont Res 57, 236-261.10.1016/j.jpor.2013.09.001 ↗
18. 18. Ogino T, Koizumi H, Furuchi M, Murakami M, Matsumura H, Tanoue N (2007) Effect of a metal priming agent on wear resistance of gold alloy-indirect composite joint. Dent Mater J 26, 201-208.10.4012/dmj.26.201 ↗
19. 19. Hirata M, Koizumi H, Tanoue N, Ogino T, Murakami M, Matsumura H (2011) Influence of laboratory light sources on the wear characteristics of indirect composites. Dent Mater J 30, 127-135.10.4012/dmj.2010-043 ↗
20. 20. Lien W, Roberts HW, Platt JA, Vandewalle KS, Hill TJ, Chu TM (2015) Microstructural evolution and physical behavior of a lithium disilicate glass-ceramic. Dent Mater 31, 928-940.10.1016/j.dental.2015.05.003 ↗