Effect of thermal cycling on bond strengths of single-step self-etch adhesives to bovine dentin

Yohei Asaka, Kanako Yamaguchi, Hirohiko Inage, Toshiki Takamizawa, Hiroyasu Kurokawa, Akitomo Rikuta, Takashi Kuroda, Masashi Miyazaki

Journal of Oral Science· Volume 48· Issue 2

Abstract

The purpose of this study was to clarify the effect of thermal cycling on dentin bond strengths of single-step self-etch adhesives. Five commercially available single-step self-etch systems were used. The adhesives were applied to the dentin surfaces of bovine incisors, and then light-irradiated. Resin composites were condensed into a mold and light-irradiated. Bonded specimens were divided into two groups and stored in water at 37 degrees C for 24 h without thermal cycling, or in water at 37 degrees C for 24 h followed by 10,000 thermal cycles between 5 degrees C and 60 degrees C. Ten samples per group were tested for shear strength at a crosshead speed of 1.0 mm/min. The data were analyzed by Student's t test and Tukey HSD test at a probability level of 0.05. After 24 h of storage in water, the mean dentin bond strengths ranged from 9.3 MPa to 14.0 MPa. After 10,000 thermal cycles, the mean bond strengths remained unchanged. Failure after the test was commonly due to adhesive breakdown associated with partial cohesive failure of the resin. The present results suggest that the benefit of using single-step self-etch systems, in terms of simplifying the clinical procedure, might be acceptable even after thermal stresses.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Dental materials and restorations · Dental Research and COVID-19 · Dental Erosion and Treatment

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. 1. Van Meerbeek B, De Munck J, Yoshida Y, Inoue S, Vargas M, Vijay P, Van Landuyt K, Lambrechts P, Vanherle G (2003) Buonocore memorial lecture. Adhesion to enamel and dentin: current status and future challenges. Oper Dent 28, 215-235
2. 2. Chiba Y, Yamaguchi K, Miyazaki M, Tsubota K, Takamizawa T, Moore BK (2006) Effect of air-drying time of single-application self-etch adhesives on dentin bond strength. Oper Dent (in press)10.2341/05-19 ↗
3. 3. Asaka Y, Miyazaki M, Takamizawa T, Tsubota K, Moore BK (2006) Influence of delayed placement of composites over cured adhesives on dentin bond strength of single-application self-etch systems. Oper Dent 31, 18-2410.2341/04-157 ↗
4. 4. De Munck J, Van Meerbeek B, Satoshi I, Vargas M, Yoshida Y, Armstrong S, Lambrechts P, Vanherle G (2003) Microtensile bond strengths of one- and two-step self-etch adhesives to bur-cut enamel and dentin. Am J Dent 16, 414-420
5. 5. Hashimoto M, Ohno H, Yoshida E, Hori M, Sano H, Kaga M, Oguchi H (2003) Resin-enamel bonds made with self-etching primers on ground enamel. Eur J Oral Sci 111, 447-45310.1034/j.1600-0722.2003.00060.x ↗
6. MEERBEEK BART VAN · 2005 · 24 · 110.4012/dmj.24.1 ↗
7. 7. Cotert HS, Sen BH, Balkan M (2001) In vitro comparison of cuspal fracture resistances of posterior teeth restored with various adhesive restorations. Int J Prosthodont 14, 374-378
8. 8. De Munck J, Van Landuyt K, Peumans M, Poitevin A, Lambrechts P, Braem M, Van Meerbeek B (2005) A critical review of the durability of adhesion to tooth tissue, methods and results. J Dent Res 84, 118-13210.1177/154405910508400204 ↗
9. 10.1016/S0300-5712(98)00037-210.1016/S0300-5712(98)00037-2 ↗
10. 10. Kubo S, Yokota H, Sata Y, Hayashi Y (2001) Microleakage of self-etching primers after thermal and flexural load cycling. Am J Dent 14, 163-169
11. 11. Cardoso PE, Placido E, Moura SK (2002) Microleakage of four simplified adhesive systems under thermal and mechanical stresses. Am J Dent 15, 164-168
12. 12. Helvatjoglu-Antoniades M, Koliniotou-Kubia E, Dionyssopoulos P (2004) The effect of thermal cycling on the bovine dentine shear bond strength of current adhesive systems. J Oral Rehabil 31, 911-91710.1111/j.1365-2842.2004.01318.x ↗
13. 10.1016/0109-5641(92)90097-V10.1016/0109-5641(92)90097-V ↗
14. 14. Schilke R, Bauβ O, Lisson JA, Schuckar M, Geurtsen W (1999) Bovine dentin as a substitute for human dentin in shear bond strength measurements. Am J Dent 12, 92-96
15. 15. Yamada M, Miyazaki M, Onose H, Moore BK (2005) Influence of interchanging self-etching primers and bonding agents on bond strengths to bovine dentin. Am J Dent 18, 155-159
16. 16. Miyazaki M, Sato M, Onose H, Moore BK (1998) Influence of thermal cycling on dentin bond strength of two-step bonding systems. Am J Dent 11, 118-122
17. 17. Sato M, Miyazaki M (2005) Comparison of depth of dentin etching and resin infiltration with single-step adhesive systems. J Dent 33, 475-48410.1016/j.jdent.2004.10.024 ↗
18. 10.1016/j.dental.2005.01.01310.1016/j.dental.2005.01.013 ↗
19. 19. Armstrong SR, Vargas MA, Chung I, Pashley DH, Campbell JA, Laffoon JE, Qian F (2004) Resin-dentin interfacial ultrastructure and microtensile dentin bond strength after five-year water storage. Oper Dent 29, 705-712
20. 1996 · 12 · 302
21. 10.1016/S0300-5712(02)00064-710.1016/S0300-5712(02)00064-7 ↗
22. 22. Tay FR, Frankenberger R, Krejci I, Bouillaguet S, Pashley DH, Carvalho RM, Lai CN (2004) Single-bottle adhesives behave as permeable membranes after polymerization. I. In vivo evidence. J Dent 32, 611-62110.1016/j.jdent.2004.04.006 ↗
23. 23. Söderholm KJ (1991) Correlation of in vivo and in vitro performance of adhesive restorative materials: a report of the ASC MD156 task group on test methods for the adhesion of restorative materials. Dent Mater 7, 74-8310.1016/0109-5641(91)90049-5 ↗
24. 10.1002/jbm.1020810.1002/jbm.10208 ↗
25. 25. Yoshida Y, Nagakane K, Fukuda R, Nakayama Y, Okazaki M, Shintani H, Inoue S, Tagawa Y, Suzuki K, De Munck J, Van Meerbeek B (2004) Comparative study on adhesive performance of functional monomers. J Dent Res 83, 454-45810.1177/154405910408300604 ↗
26. 10.1002/jbm.121610.1002/jbm.1216 ↗