Effect of alumina air-abrasion on mechanical bonding between an acrylic resin and casting alloys
Source abstract
Abstract
This study examined the effect of alumina air-abrasion with different pressure on bonding between an acrylic resin and casting alloys. Disk specimens (8 and 10 mm in diameter) were cast from a silver-palladium-copper-gold (Ag-Pd-Cu-Au, Castwell M.C.12) alloy and a titanium-aluminum-niobium alloy (Ti-6Al-7Nb, T-Alloy Tough). The disks were air-abraded with alumina particles (50-70 microm) under different air-pressures (0 unabraded, 0.1, and 0.6 MPa). The disk pairs were bonded together with a tri-n-butylborane (TBB)-initiated acrylic resin, and shear bond strengths were determined both before and after thermocycling. Bond strength varied from a maximum of 37.1 MPa to a minimum of 3.6 MPa for the Ag-Pd-Cu-Au alloy, whereas bond strength to Ti-6Al-7Nb alloy ranged from 34.7 MPa to 0.1 MPa. Specimens abraded with 0.6 MPa pressure recorded the greatest post-thermocycling bond strength (21.7 MPa and 17.9 MPa), and unabraded specimens showed the lowest strength (3.6 MPa and 0.1 MPa) for both alloys. Post-thermocycling bond strength to the Ag-Pd-Cu-Au alloy was higher than that to the Ti-6Al-7Nb alloy under identical air-abrading conditions. It can be concluded that alumina air-abrasion with an air-pressure of 0.6 MPa is effective in enhancing retentive characteristics of the TBB-initiated resin joined to the alloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Additive Manufacturing and 3D Printing Technologies · Engineering Technology and Methodologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. 10.1016/S0022-3913(96)90296-610.1016/S0022-3913(96)90296-6 ↗
2. 2. Pröbster B, Henrich GM (1997) 11-year follow-up study of resin-bonded fixed partial dentures. Int J Prosthodont 10, 259-268.
3. 10.1016/S0022-3913(98)70083-610.1016/S0022-3913(98)70083-6 ↗
4. 10.1067/mpr.2002.12999610.1067/mpr.2002.129996 ↗
5. 10.1046/j.1365-2842.2003.01166.x10.1046/j.1365-2842.2003.01166.x ↗
6. 6. Shimizu H, Takahashi Y (2004) Retainer design for posterior resin-bonded fixed partial dentures: a technical report. Quintessence Int 35, 653-654.
7. 10.1016/0022-3913(92)90233-Z10.1016/0022-3913(92)90233-Z ↗
8. 10.1016/S0300-5712(99)00070-610.1016/S0300-5712(99)00070-6 ↗
9. 9. Yanagida H, Matsumura H, Atsuta M (2001) Bonding of prosthetic composite material to Ti-6Al-7Nb alloy with eight metal conditioners and a surface modification technique. Am J Dent 14, 291-294.
10. 10.4012/dmj.27.5610.4012/dmj.27.56 ↗
11. 10.1016/S0022-3913(05)80178-710.1016/S0022-3913(05)80178-7 ↗
12. 12. Peutzfeldt A, Asmussen E (1996) Distortion of alloy by sandblasting. Am J Dent 9, 65-66.
13. 13. Papadopoulos T, Tsetsekou A, Eliades G (1999) Effect of alumina oxide sandblasting on cast commercially pure titanium surfaces. Eur J Prosthodont Restor Dent 7, 15-21.
14. 10.1016/S0022-3913(99)70035-110.1016/S0022-3913(99)70035-1 ↗
15. 15. Taga Y, Kawai K, Nokubi T (2001) New method for divesting cobalt-chromium alloy castings: sandblasting with a mixed abrasive powder. J Prosthet Dent 85, 357-362.10.1067/mpr.2001.114265 ↗
16. 16. Sugawara H, Yanagida H, Tanoue N, Koishi Y, Nagano K, Atsuta M, Matsumura H (2004) Effect of alumina abrasion for bonding between Ti-6Al-7Nb alloy and an indirect composite. Int Chin J Dent 4, 8-14.
17. 10.1023/A:100890940894810.1023/A:1008909408948 ↗