Effectiveness of a universal adhesive for repair bonding to composite and amalgam
Source abstract
Abstract
The study aimed to compare the repair bond strength of aged composite and amalgam repaired with resin composite after various mechanical and adhesive surface treatments. Specimens were aged by thermal cycling (10,000 cycles, 5-55°C) and randomly subjected to one of three surface treatments: diamond bur abrasion, aluminum oxide air abrasion, or silica coating. Conventional bonding or a universal adhesive with incorporated silane was applied afterward (each n = 16) and resin composite was attached. In the control groups (each n = 16), resin composite was attached using one of the above adhesives without prior mechanical surface conditioning. After further thermal cycling, the shear bond strength (SBS) and failure modes were assessed. Statistical analyses were performed using ANOVA, Weibull statistics, two sample t-tests, and Chi2-test (P < 0.05). The SBS of the repaired amalgam was significantly lower than that of the composite and mechanical pretreatment significantly increased SBS. The universal adhesive significantly improved the SBS of the repaired amalgam compared to the conventional bonding agent and mechanical pretreatment increased the number of cohesive/mixed failures. Amalgam restorations may be repaired using resin composites, but the resulting SBS is lower than that obtained with composite.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Dental materials and restorations · Dental Erosion and Treatment · Dental Implant Techniques and Outcomes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Preventive Dentistry, Periodontology and Cariology, University Medical Center Göttingen
Department of Prosthodontics, University Medical Center Göttingen
References (37)
Show source-provided references
1. 1. Kanzow P, Wiegand A, Schwendicke F (2016) Cost-effectiveness of repairing versus replacing composite or amalgam restorations. J Dent 54, 41-47.10.1016/j.jdent.2016.08.008 ↗
2. 2. Opdam NJ, Bronkhorst EM, Loomans BA, Huysmans M-C (2010) 12-year survival of composite vs. amalgam restorations. J Dent Res 89, 1063-1067.10.1177/0022034510376071 ↗
3. 3. Opdam NJ, Bronkhorst EM, Loomans BA, Huysmans MC (2012) Longevity of repaired restorations: a practice based study. J Dent 40, 829-835.10.1016/j.jdent.2012.06.007 ↗
4. 4. Martin J, Fernandez E, Estay J, Gordan VV, Mjor IA, Moncada G (2013) Minimal invasive treatment for defective restorations: five-year results using sealants. Oper Dent 38, 125-133.10.2341/12-062C ↗
5. 5. Fernández EM, Martín JA, Vildósola P, Oliveira Junior OB, Gordan VV, Mjör IA et al. (2015) Can repair increase the longevity of composite resins? Results of a 10-year clinical trial. J Dent 43, 279-286.10.1016/j.jdent.2014.05.015 ↗
6. 6. Smales RJ, Hawthorne WS (2004) Long-term survival of repaired amalgams, recemented crowns and gold castings. Oper Dent 29, 249-253.
7. 7. Gordan VV, Riley JLr, Blaser PK, Mondragon E, Garvan CW, Mjör IA (2011) Alternative treatments to replacement of defective amalgam restorations: results of a seven-year clinical study. J Am Dent Assoc 142, 842-849.10.14219/jada.archive.2011.0274 ↗
8. 8. Jin XZ, Homaei E, Matinlinna JP, Tsoi JK (2016) A new concept and finite-element study on dental bond strength tests. Dent Mater 32, e238-250.10.1016/j.dental.2016.07.005 ↗
9. 9. Brosh T, Pilo R, Bichacho N, Blutstein R (1997) Effect of combinations of surface treatments and bonding agents on the bond strength of repaired composites. J Prosthet Dent 77, 122-126.10.1016/S0022-3913(97)70224-5 ↗
10. 10. Tezvergil A, Lassila LV, Vallittu PK (2003) Composite-composite repair bond strength: effect of different adhesion primers. J Dent 31, 521-525.10.1016/S0300-5712(03)00093-9 ↗
11. 11. Özcan M, Alander P, Vallittu PK, Huysmans M-C, Kalk W (2005) Effect of three surface conditioning methods to improve bond strength of particulate filler resin composites. J Mater Sci Mater Med 16, 21-27.10.1007/s10856-005-6442-4 ↗
12. 12. Hannig C, Laubach S, Hahn P, Attin T (2006) Shear bond strength of repaired adhesive filling materials using different repair procedures. J Adhes Dent 8, 35-40.
13. 13. Brendeke J, Özcan M (2007) Effect of physicochemical aging conditions on the composite-composite repair bond strength. J Adhes Dent 9, 399-406.
14. 14. Padipatvuthikul P, Mair LH (2007) Bonding of composite to water aged composite with surface treatments. Dent Mater 23, 519-525.10.1016/j.dental.2006.03.010 ↗
15. 15. Özcan M, Cura C, Brendeke J (2010) Effect of aging conditions on the repair bond strength of a microhybrid and a nanohybrid resin composite. J Adhes Dent 12, 451-459.
16. 16. Wiegand A, Stawarczyk B, Buchalla W, Tauböck TT, Özcan M, Attin T (2012) Repair of silorane composite - using the same substrate or a methacrylate-based composite? Dent Mater 28, e19-25.10.1016/j.dental.2011.10.008 ↗
17. 17. Baur V, Ilie N (2013) Repair of dental resin-based composites. Clin Oral Investig 17, 601-608.10.1007/s00784-012-0722-4 ↗
18. 18. Tsujimoto A, Barkmeier WW, Takamizawa T, Wilwerding TM, Latta MA, Miyazaki M (2017) Interfacial characteristics and bond durability of universal adhesive to various substrates. Oper Dent 42, E59-70.10.2341/15-353-L ↗
19. 19. Peterson J, Rizk M, Hoch M, Wiegand A (2018) Bonding performance of self-adhesive flowable composites to enamel, dentin and a nano-hybrid composite. Odontology 106, 171-180.10.1007/s10266-017-0324-3 ↗
20. 20. Özcan M, Vallittu PK, Huysmans M-C, Kalk W, T. V (2006) Bond strength of resin composite to differently conditioned amalgam. J Mater Sci Mater Med 17, 7-13.10.1007/s10856-006-6324-4 ↗
21. 21. Machado C, Sanchez E, Alapati S, Seghi R, Johnston W (2007) Shear bond strength of the amalgam-resin composite interface. Oper Dent 32, 341-346.10.2341/06-100 ↗
22. 22. Özcan M, Koolman C, Aladag A, Dündar M (2011) Effects of different surface conditioning methods on the bond strength of composite resin to amalgam. Oper Dent 36, 318-325.10.2341/10-294-L ↗
23. 23. Jin XZ, Tsoi JKH, Matinlinna JP (2015) A novel silane system for amalgam repair with resin composite: an in vitro study. Silicon, doi: 10.1007/s12633-015-9292-9.10.1007/s12633-015-9292-9 ↗
24. 24. Özcan M, Koc-Dundar B (2014) Composite-composite adhesion in dentistry: a systematic review and meta-analysis. Journal of Adhesion Science and Technology 28, 2209-2229.10.1080/01694243.2014.954659 ↗
25. 25. Hahnel S, Rosentritt M, Handel G, Bürgers R (2008) Influence of saliva substitute films on initial Streptococcus mutans adhesion to enamel and dental substrata. J Dent 36, 977-983.10.1016/j.jdent.2008.08.004 ↗
26. 26. Kielbassa AM, Lynch CD, Wilson NH (2014) Editorial: the Minamata convention: the beginning of the (amalgam-free) future? Quintessence Int 45, 547-548.
27. 27. Kopperud SE, Staxrud F, Espelid I, Tveit AB (2016) The post-amalgam era: norwegian dentists’ experiences with composite resins and repair of defective amalgam restorations. Int J Environ Res Public Health 13, 411.10.3390/ijerph13040441 ↗
28. 28. Tsujimoto A, Barkmeier WW, Takamizawa T, Latta MA, Miyazaki M (2018) Influence of thermal stress on simulated localized and generalized wear of nanofilled resin composites. Oper Dent 43, 380-390.10.2341/16-206-L ↗
29. 29. Gale MS, Darvell BW (1999) Thermal cycling procedures for laboratory testing of dental restorations. J Dent 27, 89-99.10.1016/S0300-5712(98)00037-2 ↗
30. 30. Rodrigues SA, Jr., Ferracane JL, Della Bona A (2009) Influence of surface treatments on the bond strength of repaired resin composite restorative materials. Dent Mater 25, 442-451.10.1016/j.dental.2008.09.009 ↗
31. 31. Hanawa T, Gnade BE, Ferracane JL, Okabe T, Watari F (1993) Compositions of surface layers formed on amalgams in air, water, and saline. Dent Mater J 12, 118-126.10.4012/dmj.12.118 ↗
32. 32. Kanzow P, Dieckmann P, Hausdörfer T, Attin T, Wiegand A, Wegehaupt FJ (2017) Repair restorations: questionnaire survey among dentists in the Canton of Zurich, Switzerland. Swiss Dent J 127, 300-311.10.61872/sdj-2017-04-267 ↗
33. 33. Kanzow P, Hoffmann R, Tschammler C, Kruppa J, Rödig T, Wiegand A (2017) Attitudes, practice and experience of German dentists regarding repair restorations. Clin Oral Invest 21, 1087-1093.10.1007/s00784-016-1859-3 ↗
34. 34. Papacchini F, Dall’Oca S, Chieffi N, Goracci C, Sadek FT, Suh BI et al. (2007) Composite-to-composite microtensile bond strength in the repair of a microfilled hybrid resin: effect of surface treatment and oxygen inhibition. J Adhes Dent 9, 25-31.
35. 35. Parsa RZ, Goldstein GR, Barrack GM, LeGeros RZ (2003) An in vitro comparison of tensile bond strengths of noble and base metal alloys to enamel. J Prosthet Dent 90, 175-183.10.1016/S0022-3913(03)00411-6 ↗
36. 36. Wongsamut W, Satrawaha S, Wayakanon K (2017) Surface modification for bonding between amalgam and orthodontic brackets. J Orthod Sci 6, 129-135.10.4103/jos.JOS_25_17 ↗
37. 37. Scherrer SS, Cesar PF, Swain MV (2010) Direct comparison of the bond strength results of the different test methods: a critical literature review. Dent Mater 26, e78-93.10.1016/j.dental.2009.12.002 ↗